Effect of slab flexural reinforcement and depth on punching strength

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of slab flexural reinforcement and depth on punching strength

Author(s): Neil M. Hawkins, Carlos E. Ospina

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s): 117-140

Keywords: Concrete design codes, depth effect, flat slabs, moment transfer, punching shear, reinforcement ratio, size effect, slab-column connections

DOI:

Date: 4/1/2017

Abstract:
Recommendations are presented for proposed revisions to the punching shear provisions of ACI 318-14 in order to recognize the limitations imposed on punching shear capacity by low amounts of slab flexural reinforcement and by slab depth effects. The influence of those two factors is investigated by examining relevant experimental results from tests on slab-column assemblages and slab systems.