222R-19: Guide to Protection of Metals in Concrete Against Corrosion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 222R-19: Guide to Protection of Metals in Concrete Against Corrosion

Author(s): ACI Committee 222

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 60

Keywords: allowable chloride; carbonation; chloride; chloride threshold; corrosion; corrosion-resistant reinforcement; durability; prestressed concrete; reinforced concrete; reinforcing steels.

DOI:

Date: 4/1/2019

Abstract:
This guide reviews the most recent developments of metal corrosion, specifically reinforcing steel, in concrete. Individual chapters are devoted to corrosion of metals in concrete, protective measures for new concrete construction, procedures for identifying corrosive environments, active corrosion in concrete, and remedial measures.