Effect of Admixed and External Chlorides on Transport of Chlorides in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Admixed and External Chlorides on Transport of Chlorides in Concrete

Author(s): Mahmoud Shakouri, Naga Pavan Vaddey, and David Trejo

Publication: Materials Journal

Volume: 116

Issue: 5

Appears on pages(s): 119-128

Keywords: admixed chlorides; chloride binding capacity; external chlorides; finite elemental analysis

DOI: 10.14359/51716833

Date: 9/1/2019

Abstract:
The binding of chlorides by the hydration products of cement in concrete is one of the factors that affects the rate of chloride ingress, which in turn can influence the time to corrosion initiation of reinforcing steel in concrete. Theoretical assessments of the influence of chloride binding on the chloride ingress and service life estimates are often based on empirically developed chloride binding isotherms to account for the interaction between the concrete matrix and external chlorides. While being useful, these assessments disregard the binding influence of admixed chlorides that may be present in the concrete from the early stages of hydration. It is suspected that the presence of free admixed chlorides can influence the diffusivity of chlorides in concrete. This work focuses on determining the binding behavior of admixed chlorides and proposes a modified diffusion model that takes chloride binding from admixed and external chlorides into consideration.

Related References:

1. Thompson, N. G.; Yunovich, M.; and Dunmire, D., “Cost of Corrosion and Corrosion Maintenance Strategies,” Corrosion Reviews, V. 25, No. 3-4, 2007, pp. 247-262. doi: 10.1515/CORRREV.2007.25.3-4.247

2. Jacobson, G. A., “NACE International’s IMPACT Study Breaks New Ground in Corrosion Management Research and Practice,” The Bridge, V. 46, No. 2, 2016, pp. 30-38.

3. Angst, U. M., “Challenges and Opportunities in Corrosion of Steel in Concrete,” Materials and Structures, V. 51, No. 1, 2018, p. 4 doi: 10.1617/s11527-017-1131-6

4. Shakouri, M., and Trejo, D., “A Time-Variant Model of Surface Chloride Build-Up for Improved Service Life Predictions,” Cement and Concrete Composites, V. 84, 2017, pp. 99-110. doi: 10.1016/j.cemconcomp.2017.08.008

5. Shakouri, M., and Trejo, D., “A Study of the Factors Affecting the Surface Chloride Maximum Phenomenon in Submerged Concrete Samples,” Cement and Concrete Composites, V. 94, 2018, pp. 181-190. doi: 10.1016/j.cemconcomp.2018.09.006

6. Shakouri, M., and Trejo, D., “Estimating the Critical Chloride Threshold of Reinforcing Steel in Concrete Using a Hierarchical Bayesian Model,” Sustainable and Resilient Infrastructure, V. 2017, 2017, pp. 1-21. doi: 10.1080/23789689.2017.1405655

7. ACI Committee 222, “Protection of Metals in Concrete Against Corrosion (ACI 222R-01),” American Concrete Institute, Farmington Hills, MI, 2001, 41 pp.

8. Pruckner, F., and Gjørv, O., “Effect of CaCl2 and NaCl Additions on Concrete Corrosivity,” Cement and Concrete Research, V. 34, No. 7, 2004, pp. 1209-1217. doi: 10.1016/j.cemconres.2003.12.015

9. Juenger, M.; Monteiro, P.; Gartner, E.; and Denbeaux, G., “A Soft X-Ray Microscope Investigation into the Effects of Calcium Chloride on Tricalcium Silicate Hydration,” Cement and Concrete Research, V. 35, No. 1, 2005, pp. 19-25. doi: 10.1016/j.cemconres.2004.05.016

10. Abalaka, A., and Babalaga, A., “Effects of Sodium Chloride Solutions on Compressive Strength Development of Concrete Containing Rice Husk Ash,” ATBU Journal of Environmental Technology, V. 4, No. 1, 2011, pp. 33-40.

11. Ramachandran, V. S., “Possible States of Chloride in the Hydration of Tricalcium Silicate in the Presence of Calcium Chloride,” Materiales de Construcción, V. 4, No. 1, 1971, pp. 3-12. doi: 10.1007/BF02473926

12. Henocq, P., Modélisation des interactions ioniques à la surface des silicates de calcium hydratés, Cergy-Pontoise, 2005.

13. Henocq, P.; Marchand, J.; Samson, E.; and Lavoie, J.-A., “Modeling of Ionic Interactions at the C–S–H Surface—Application to CsCl and LiCl Solutions in Comparison with NaCl Solutions,” Second International Symposium on Advances in Concrete through Science and Engineering (RILEM Proceedings), 2006.

14. Elakneswaran, Y.; Nawa, T.; and Kurumisawa, K., “Electrokinetic Potential of Hydrated Cement in Relation to Adsorption of Chlorides,” Cement and Concrete Research, V. 39, No. 4, 2009, pp. 340-344. doi: 10.1016/j.cemconres.2009.01.006

15. Ramachandran, V.; Paroli, M. R.; Beaudoin, J. J.; and Delgado, A. H., “Gypsum and Gypsum Products,” Handbook of Thermal Analysis of Construction Materials, Chapter 11, 2002, pp. 449-490.

16. Suryavanshi, A. K.; Scantlebury, J. D.; and Lyon, S. B., “Mechanism of Friedel’s Salt Formation in Cements Rich in Tri-calcium Aluminate,” Cement and Concrete Research, V. 26, No. 5, 1996, pp. 717-727. doi: 10.1016/S0008-8846(96)85009-5

17. Vaddey, N. P., and Trejo, D., “Influence of Concrete Mixture Parameters on Chloride Test Measurements,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 8, 2018, p. 04018188 doi: 10.1061/(ASCE)MT.1943-5533.0002364

18. Trejo, D.; Vaddey, N. P.; and Shakouri, M., “Factors Influencing Chloride Test Results of Cementitious Systems,” ACI Materials Journal, V. 116, No. 1, Jan. 2019, doi: 10.14359/51712240

19. Florea, M., and Brouwers, H., “Chloride Binding Related to Hydration Products: Part I: Ordinary Portland Cement,” Cement and Concrete Research, V. 42, No. 2, 2012, pp. 282-290. doi: 10.1016/j.cemconres.2011.09.016

20. Trejo, D.; Shakouri, M.; Vaddey, N. P.; and Isgor, O. B., “Development of Empirical Models for Chloride Binding in Cementitious Systems Containing Admixed Chlorides,” Construction and Building Materials, V. 189, 2018, pp. 157-169. doi: 10.1016/j.conbuildmat.2018.08.197

21. Hirao, H.; Yamada, K.; Takahashi, H.; and Zibara, H., “Chloride Binding of Cement Estimated by Binding Isotherms of Hydrates,” Journal of Advanced Concrete Technology, V. 3, No. 1, 2005, pp. 77-84. doi: 10.3151/jact.3.77

22. Ekolu, S.; Thomas, M.; and Hooton, R., “Pessimum Effect of Externally Applied Chlorides on Expansion due to Delayed Ettringite Formation: Proposed Mechanism,” Cement and Concrete Research, V. 36, No. 4, 2006, pp. 688-696. doi: 10.1016/j.cemconres.2005.11.020

23. Yuan, Q.; Shi, C.; De Schutter, G.; Audenaert, K.; and Deng, D., “Chloride Binding of Cement-Based Materials Subjected to External Chloride Environment—A Review,” Construction and Building Materials, V. 23, No. 1, 2009, pp. 1-13. doi: 10.1016/j.conbuildmat.2008.02.004

24. Brunauer, S.; Skalny, J.; and Bodor, E., “Adsorption on Nonporous Solids,” Journal of Colloid and Interface Science, V. 30, No. 4, 1969, pp. 546-552. doi: 10.1016/0021-9797(69)90423-8

25. Shakouri, M.; Trejo, D.; and Gardoni, P., “A Probabilistic Framework to Justify Allowable Admixed Chloride Limits In Concrete,” Construction and Building Materials, V. 139, 2017, pp. 490-500. doi: 10.1016/j.conbuildmat.2017.02.053

26. ASTM C305-13, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 2013, 3 pp.

27. Adams, M. P., “Factors Influencing Conversion and Volume Stability in Calcium Aluminate Cement Systems,” doctoral dissertation, Oregon State University, Corvallis, OR, 2015, 301 pp.

28. Arya, C.; Buenfeld, N.; and Newman, J., “Assessment of Simple Methods of Determining the Free Chloride Ion Content of Cement Paste,” Cement and Concrete Research, V. 17, No. 6, 1987, pp. 907-918. doi: 10.1016/0008-8846(87)90079-2

29. Glass, G.; Wang, Y.; and Buenfeld, N., “An Investigation of Experimental Methods Used to Determine Free and Total Chloride Contents,” Cement and Concrete Research, V. 26, No. 9, 1996, pp. 1443-1449. doi: 10.1016/0008-8846(96)00115-9

30. Vollpracht, A.; Lothenbach, B.; Snellings, R.; and Haufe, J., “The Pore Solution of Blended Cements: A Review,” Materials and Structures, V. 49, No. 8, 2016, pp. 3341-3367. doi: 10.1617/s11527-015-0724-1

31. ASTM C1152/C1152M-04, “Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2004, 4 pp.

32. Hranice, C., “The Effect of Water Ratio on Microstructre and Composition of the Hydration Products of Portland Cement Pastes,” Ceramics-Silikáty, V. 46, No. 4, 2002, pp. 152-158.

33. Bentz, D. P., “Influence of Water-to-Cement Ratio on Hydration Kinetics: Simple Models Based on Spatial Considerations,” Cement and Concrete Research, V. 36, No. 2, 2006, pp. 238-244. doi: 10.1016/j.cemconres.2005.04.014

34. Pane, I., and Hansen, W., “Investigation of Blended Cement Hydration by Isothermal Calorimetry and Thermal Analysis,” Cement and Concrete Research, V. 35, No. 6, 2005, pp. 1155-1164. doi: 10.1016/j.cemconres.2004.10.027

35. Lothenbach, B.; Scrivener, K.; and Hooton, R., “Supplementary Cementitious Materials,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1244-1256. doi: 10.1016/j.cemconres.2010.12.001


ALSO AVAILABLE IN:

Electronic Materials Journal