Lightweight Aggregates and Shrinkage-Reducing Admixtures for Low-Cracking Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lightweight Aggregates and Shrinkage-Reducing Admixtures for Low-Cracking Concrete

Author(s): Harikrishnan Nair and H. Celik Ozyildirim

Publication: Materials Journal

Volume: 116

Issue: 5

Appears on pages(s): 91-98

Keywords: durability; lightweight concrete; low cracking; permeability; shrinkage; shrinkage-reducing admixture

DOI: 10.14359/51716830

Date: 9/1/2019

Abstract:
Cracks in bridge decks facilitate the penetration of chlorides that induce corrosion of reinforcing steel. Formation of cracks is related to the shrinkage and properties of the concrete and the restraints to movement. Lightweight concrete with a low modulus of elasticity, high creep, and water in the aggregate pores for internal curing has a reduced cracking potential. To control cracking, shrinkage of concrete can be reduced by using a shrinkage-reducing admixture (SRA). A recent study at the Virginia Department of Transportation (VDOT) investigated the performance of both lightweight concretes and concretes with SRA containing normal-weight aggregates in the field and found that these concretes had no cracks or fewer cracks than were typical of decks constructed with normal-weight aggregates over the past 20 years. VDOT developed a new specification that included lightweight concretes or concretes with normal-weight aggregates and SRA and this specification is being used successfully to reduce cracking in bridge decks. This paper summarizes the work conducted to develop the new specification and includes information on field applications.

Related References:

1. Darwin, D., and Browning, J., “Construction of Low Cracking High Performance Concrete (LC-HPC) Bridge Decks: Field Experience,” Proceedings of the Concrete Bridge Conference, National Concrete Bridge Council, Skokie, IL, 2008.

2. Ozyildirim, C., “Durable Concrete for Bridges,” Aspire: The Concrete Bridge Magazine, Summer 2007, pp. 15-29.

3. Holm, T. A., and Ries, J., “Lightweight Concrete and Aggregates,” Significance of Tests and Properties of Concrete and Concrete Making Materials, STP 169D, ASTM International, West Conshohocken, PA, 2006, pp. 548-560.

4. Byard, B. E.; Schindler, A. K.; and Barnes, R. W., “Cracking Tendency of Lightweight Aggregate Bridge Deck Concrete,” ACI Materials Journal, V. 109, No. 2, Mar-Apr. 2012, pp. 179-188.

5. Byard, B. E.; Schindler, A. K.; and Barnes, R. W., “Early-Age Cracking Tendency and Ultimate Degree of Hydration of Internally Cured Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 8, 2012, pp. 1025-1033. doi: 10.1061/(ASCE)MT.1943-5533.0000469

6. Weiss, W. J., “Prediction of Early-Age Shrinkage Cracking in Concrete Elements,” doctoral dissertation, Northwestern University, Evanston, IL, 1999.

7. Ozyildirim, C., and Gomez, J. P., “First Bridge Structure with Lightweight High-Performance Concrete Beams and Decks in Virginia,” VTRC 06-R12, Virginia Transportation Research Council, Charlottesville, VA, 2005.

8. Ozyildirim, C., “Durability of Structural Lightweight Concrete,” ESCSI Special Workshop on Lightweight Aggregate Concrete Bridges, Concrete Bridge Conference, St. Louis, MO, 2008.

9. ACI Committee 231, “Report on Early-Age Cracking: Causes, Measurement, and Mitigation (ACI 231R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 46 pp.

10. Weiss, W. J., and Berke, N. S., “Admixtures for Reduction of Shrinkage and Cracking,” Early Age Cracking in Cementitious Systems, A. Bentur, ed., RILEM, Bagneux, France, 2003, pp. 323-338.

11. Shah, S. P.; Weiss, W. J.; and Yang, W., “Shrinkage Cracking: Can It Be Prevented?” Concrete International, V. 20, No. 4, Apr. 1998, pp. 51-55.

12. Shah, S. P.; Karaguler, M. E.; and Sarigaphuti, M., “Effects of Shrinkage Reducing Admixture on Restrained Shrinkage Cracking of Concrete,” ACI Materials Journal, V. 89, No. 3, May-June 1992, pp. 88-90.

13. Weiss, W. J.; Yang, W.; and Shah, S. P., “Shrinkage Cracking of Restrained Concrete Slabs,” Journal of Engineering Mechanics, ASCE, V. 124, No. 7, 1998, pp. 765-774. doi: 10.1061/(ASCE)0733-9399(1998)124:7(765)

14. Cope, B. L., and Ramey, G. E., “Reducing Drying Shrinkage of Bridge Deck Concrete,” Concrete International, V. 23, No. 8, Aug. 2001, pp. 76-82.

15. Chaunsali, P.; Lim, S.; Mondal, P.; Foutch, D.; Richardson, D.; Tung, Y.; and Hindi, R., “Bridge Decks: Mitigation of Cracking and Increased Durability,” FHWA-ICT-13-023, Illinois Department of Transportation, Springfield, IL, 2013.

16. Weiss, W.; Yang, W.; and Shah, S., “Factors Influencing Durability and Early-Age Cracking in High Strength Concrete Structures,” High Performance Concrete: Research to Practice, SP-189, American Concrete Institute, Farmington Hills, MI, 1999, pp. 387-409.

17. Bentz, D. P.; Geiker, M. R.; and Hansen, K. K., “Shrinkage-Reducing Admixtures and Early Age Desiccation in Cement Pastes and Mortars,” Cement and Concrete Research, V. 31, No. 7, 2001, pp. 1075-1085. doi: 10.1016/S0008-8846(01)00519-1

18. Lindquist, W.; Darwin, D.; and Browning, J., “Development and Construction of Low-Cracking High-Performance Concrete (LC-HPC) Bridge Decks: Free-Shrinkage, Mixture Optimization, and Concrete Production,” SM Report No. 92, University of Kansas Center for Research, Inc., Lawrence, KS, 2008, 540 pp.

19. Ozyildirim, C., “Performance of First Structure Built with High-Performance Concrete in Virginia,” Transportation Research Record: Journal of the Transportation Research Board, V. 1798, No. 1, 2002, pp. 43-50. doi: 10.3141/1798-07

20. Lane, D. S., and Ozyildirim, C., “Combinations of Pozzolans and Ground, Granulated, Blast-Furnace Slag for Durable Hydraulic Cement Concrete,” VTRC 00-R1, Virginia Transportation Research Council, Charlottesville, VA, 2000.

21. Sharp, R. S.; Lundy, J. L.; Nair, H.; Moen, D. C.; Johnson, B. J.; and Sarver, B., “Quality Control Procedures for New Types of Corrosion Resistant Reinforcing Steel,” VCTIR 11-R21, Virginia Center for Transportation Innovation and Research, Charlottesville, VA, 2011.

22. Babaei, K., and Fouladgar, A., “Solutions to Concrete Bridge Deck Cracking,” Concrete International, V. 19, No. 7, July 1997, pp. 34-37.

23. Virginia Department of Transportation, Guide Manual for Causes and Repair of Cracks in Bridge Decks, Sept. 2009. http://www.virginiadot.org/business/resources/const/guidemancrackrepair.pdf. (last accessed June 2018)

24. Darwin, D., “Low-Cracking High-Performance Concrete Bridge Decks,” Concrete Bridge Views, No. 78, 2014.

25. Darwin, D., and Browning, J., “Construction of Low Cracking High Performance Concrete (LC-HPC) Bridge Decks: Field Experience,” Proceedings of the Concrete Bridge Conference, National Concrete Bridge Council, Skokie, IL, 2008.

26. Maggenti, R.; Knapp, C.; and Fereira, S., “Controlling Shrinkage Cracking,” Concrete International, V. 35, No. 7, July 2013, pp. 36-41.

27. Gaines, M., and Sheikhizadeh, M., “ How to Specify and Construct Durable Crack Free Bridge Decks: Washington State Experience,” Concrete Bridge Views, No. 72, Sept.-Oct. 2013.

28. Virginia Department of Transportation, “Road and Bridge Specifications,” Richmond, VA, 2016.


ALSO AVAILABLE IN:

Electronic Materials Journal