Cores at Early Ages for In-Place Concrete Acceptance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cores at Early Ages for In-Place Concrete Acceptance

Author(s): Adam A. Felinczak, Marc C. Johnson, Rania Al-Hammoud, and Carolyn M. Hansson

Publication: Materials Journal

Volume: 116

Issue: 5

Appears on pages(s): 49-56

Keywords: core test; coring; durability; early ages; electrical resistivity; rapid chloride permeability test

DOI: 10.14359/51716826

Date: 9/1/2019

Abstract:
Practitioners often question the correlation between the performance of a structure and the results of standard 28-day cylinder testing. Testing cores extracted from the structure is one approach to evaluate in-place concrete but is frequently performed at ages greater than 28 days. Due to increasing demands for faster construction timelines, the feasibility of extracting and testing cores at an earlier age to satisfy acceptance criteria was considered. In this study, cores from laboratory-constructed structures were tested on days 3, 7, and 28 using acceptance criteria for compressive strength, rapid chloride permeability (RCP), and electrical resistivity. This research has shown that extracting and testing cores—as early as day 3 from high-strength concretes and day 7 for other concretes—is feasible. Results of 28-day testing were not affected by coring day and duration of conditioning. Electrical resistivity was found to be a feasible alternative for the RCP test.

Related References:

1. Ariöz, Ö.; Tuncan, M.; Ramyar, K.; and Tuncan, A., “A Comparative Study on the Interpretation of Concrete Core Strength Results,” Magazine of Concrete Research, V. 58, No. 2, 2006, pp. 117-122. doi: 10.1680/macr.2006.58.2.117

2. Szypula, A., and Grossman, J. S., “Cylinder versus Core Strength,” Concrete International, V. 12, No. 2, Feb. 1990, pp. 55-61.

3. SSP 999F31, “Construction Specification for Non-Prestressed Precast Concrete Bridge Elements,” Ontario Ministry of Transportation, Toronto, ON, Canada, 2016, 19 pp.

4. OPSS, PROV 909, “Construction Specification for Prestressed Concrete – Precast Girder,” Ontario Ministry of Transportation, Toronto, ON, Canada, 2016, 32 pp.

5. ASTM C42/42M-13, “Standard Test Method for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete,” ASTM International, West Conshohocken, PA, 2013, 7 pp.

6. ASTM C39/C39M-18, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

7. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 8 pp.

8. ASTM C1760-12, “Standard Test Method for Bulk Electrical Conductivity of Hardened Concrete,” ASTM International, West Conshohocken, PA, 2012, 5 pp.

9. Layssi, H.; Ghods, P.; Alizadeh, A. R.; and Salehi, M., “Electrical Resistivity of Concrete,” Concrete International, V. 37, No. 5, May 2015, pp. 41-46.

10. Goto, S., and Roy, D. M., “The Effect of w/c Ratio and Curing Temperature on the Permeability of Hardened Cement Paste,” Cement and Concrete Research, V. 11, No. 4, 1981, pp. 575-579. doi: 10.1016/0008-8846(81)90087-9

11. Shideler, J. J., and Chamberlin, W. H., “Early Strength of Concrete as Affected by Steam Curing Temperatures,” ACI Journal Proceedings, V. 46, No. 12, Dec. 1949, pp. 273-282.

12. Nokken, M. R., and Hooton, R. D., “Electrical Conductivity Testing,” Concrete International, V. 28, No. 10, Oct. 2006, pp. 58-63.

13. Hassan, K. E.; Cabrera, J. G.; and Maliehe, R. S., “The Effect of Mineral Admixtures on the Properties of High-Performance Concrete,” Cement and Concrete Composites, V. 22, No. 4, pp. 2000, 267-271.

14. Suprenant, B., “An Introduction to Concrete Core Testing,” Civil Engineering for Practicing and Design Engineers, V. 4, 1985, pp. 607-615.

15. Bartlett, F. M., and MacGregor, J. G., “Assessment of Concrete Strength in Existing Structures,” Department of Civil Engineering, University of Alberta, Edmonton, AB, Canada, 1994, 321 pp.

16. Bloem, D. L., “Concrete Strength Measurement—Cores Versus Cylinders,” Proceedings, American Society for Testing and Materials, V. 65, 1965, pp. 668-696.

17. Khoury, S.; Aliabdo, A. A.-H.; and Ghazy, A., “Reliability of Core Test—Critical Assessment and Proposed New Approach,” Alexandria Engineering Journal, V. 53, No. 1, 2014, pp. 169-184. doi: 10.1016/j.aej.2013.12.005

18. Bartlett, F. M., and MacGregor, J. G., “Effect of Moisture Condition on Concrete Core Strengths,” ACI Materials Journal, V. 91, No. 3, May-June 1994, pp. 227-236.


ALSO AVAILABLE IN:

Electronic Materials Journal