Influence of Reinforcing Index on Rheology of Fiber-Reinforced Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Reinforcing Index on Rheology of Fiber-Reinforced Mortar

Author(s): Mingli Cao, Li Li, and Shirley Shen

Publication: Materials Journal

Volume: 116

Issue: 6

Appears on pages(s): 95-105

Keywords: critical reinforcing index; hybrid fibers; polyvinyl alcohol fiber; regression analysis; rheology; whisker

DOI: 10.14359/51716816

Date: 11/1/2019

Abstract:
The relationships between the reinforcing index (RI: the product of volume fraction and length-to-diameter ratio of fibers) and rheological parameters (hysteresis loop area, yield stress, plastic viscosity, flow spread, and flow rate) of a single type of fiber-reinforced cementitious composites (SgFRCCs) and hybrid fiber-reinforced cementitious composites (HyFRCCs) with steel, polyvinyl alcohol (PVA) fibers, and calcium carbonate (CaCO3) whiskers, were systematically studied for the first time. After shearing action, short whiskers between cement particles prevented the cement particles from coming close to each other, leading to more irreversible broken structures in the entire rheological test process, which means higher hysteresis loop areas than those of longer fibers. The new hybrid fiber system decreased the yield stress and plastic viscosity to a certain extent, as a result of the “grading effect” of hybrid fibers and whiskers. Based on the theoretical framework of random loose packing, the critical RI values for single PVA fibers and hybrid fibers were approximately 1.0 and 2.0, respectively, which supports this theoretical framework and the effect of critical RI values in fiber-reinforced mortar. The influence of the RI on the characteristics of fresh HyFRCCs can be quantified well into a multivariate linear relationship. Moreover, these findings can be used to optimize fiber mixtures in practical project applications.

Related References:

1. Alberti, M. G.; Enfedaque, A.; Gálvez, J. C.; Cánovas, M. F.; and Osorio, I. R., “Polyolefin Fiber-Reinforced Concrete Enhanced with Steel-Hooked Fibers in Low Proportions,” Materials & Design, V. 60, 2014, pp. 57-65. doi: 10.1016/j.matdes.2014.03.050

2. Cao, M.; Mao, Y.; Khan, M.; Si, W.; and Shen, S., “Different Testing Methods for Assessing the Synthetic Fiber Distribution in Cement-Based Composites,” Construction and Building Materials, V. 184, 2018, pp. 128-142. doi: 10.1016/j.conbuildmat.2018.06.207

3. Ferrara, L.; Park, Y.; and Shah, S. P., “Correlation among Fresh State Behavior, Fiber Dispersion, and Toughness Properties of SFRCs,” Journal of Materials in Civil Engineering, ASCE, V. 20, No. 7, 2008, pp. 493-501. doi: 10.1061/(ASCE)0899-1561(2008)20:7(493)

4. Ferrara, L., and Meda, A., “Relationships between Fibre Distribution, Workability and the Mechanical Properties of SFRC Applied to Precast Roof Elements,” Materials and Structures, V. 39, No. 4, 2007, pp. 411-420. doi: 10.1617/s11527-005-9017-4

5. Martinie, L.; Rossi, P.; and Roussel, N., “Rheology of Fiber Reinforced Cementitious Materials: Classification and Prediction,” Cement and Concrete Research, V. 40, No. 2, 2010, pp. 226-234. doi: 10.1016/j.cemconres.2009.08.032

6. Kuder, K. G.; Ozyurt, N.; Mu, E. B.; and Shah, S. P., “Rheology of fiber-Reinforced Cementitious Materials,” Cement and Concrete Research, V. 37, No. 2, 2007, pp. 191-199. doi: 10.1016/j.cemconres.2006.10.015

7. Ou, Y.; Tsai, M.; Liu, K.; and Chang, K., “Compressive Behavior of Steel-Fiber-Reinforced Concrete with a High Reinforcing Index,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 2, 2012, pp. 207-215. doi: 10.1061/(ASCE)MT.1943-5533.0000372

8. Silva, E. R.; Coelho, J. F. J.; and Bordado, J. C., “Strength Improvement of Mortar Composites Reinforced with Newly Hybrid-Blended Fibres: Influence of Fibres Geometry and Morphology,” Construction and Building Materials, V. 40, 2013, pp. 473-480. doi: 10.1016/j.conbuildmat.2012.11.017

9. Pyo, S.; El-Tawil, S.; and Naaman, A. E., “Direct Tensile Behavior of Ultra High Performance Fiber Reinforced Concrete (UHP-FRC) at High Strain Rates,” Cement and Concrete Research, V. 88, 2016, pp. 144-156. doi: 10.1016/j.cemconres.2016.07.003

10. Gencel, O.; Brostow, W.; Datashvili, T.; and Thedford, M., “Workability and Mechanical Performance of Steel Fiber-Reinforced Self-Compacting Concrete with Fly Ash,” Composite Interfaces, V. 18, No. 2, 2011, pp. 169-184. doi: 10.1163/092764411X567567

11. Cao, M.; Xu, L.; and Zhang, C., “Rheology, Fiber Distribution and Mechanical Properties of Calcium Carbonate (CaCO3) Whisker Reinforced Cement Mortar,” Composites. Part A, Applied Science and Manufacturing, V. 90, 2016, pp. 662-669. doi: 10.1016/j.compositesa.2016.08.033

12. Hughes, B. P., and Fattuhi, N. I., “The Workability of Steel-Fibre-Reinforced Concrete,” Magazine of Concrete Research, V. 28, No. 96, 1976, pp. 157-161. doi: 10.1680/macr.1976.28.96.157

13. Grünewald, S., and Walraven, J. C., “Parameter-Study on the Influence of Steel Fibers and Coarse Aggregate Content on the Fresh Properties of Self-Compacting Concrete,” Cement and Concrete Research, V. 31, No. 12, 2001, pp. 1793-1798. doi: 10.1016/S0008-8846(01)00555-5

14. Bayasi, M. Z., and Soroushian, P., “Effect of Steel Fiber Reinforcement on Fresh Mix Properties of Concrete,” ACI Materials Journal, V. 89, No. 4, July-Aug. 1992, pp. 369-374.

15. Krieger, I. M., and Dougherty, T. J., “A Mechanism for Non‐Newtonian Flow in Suspensions of Rigid Spheres,” Transactions of the Society of Rheology, V. 3, No. 1, 1959, pp. 137-152. doi: 10.1122/1.548848

16. Mehdipour, I.; Vahdani, M.; Libre, N. A.; and Shekarchi, M., “Relationship between Workability and Mechanical Properties of Fibre-Reinforced Self-Consolidating Mortar,” Magazine of Concrete Research, V. 65, No. 17, 2013, pp. 1011-1022. doi: 10.1680/macr.12.00088

17. Emdadi, A.; Mehdipour, I.; Libre, N. A.; and Shekarchi, M., “Optimized Workability and Mechanical Properties of FRCM by Using Fiber Factor Approach: Theoretical and Experimental Study,” Materials and Structures, V. 48, No. 4, 2015, pp. 1149-1161. doi: 10.1617/s11527-013-0221-3

18. Mehdipour, I.; Libre, N. A.; Shekarchi, M.; and Khanjani, M., “Effect of Workability Characteristics on the Hardened Performance of FRSCCMs,” Construction and Building Materials, V. 40, 2013, pp. 611-621. doi: 10.1016/j.conbuildmat.2012.11.051

19. Sahmaran, M.; Yurtseven, A.; and Yaman, I. O., “Workability of Hybrid Fiber Reinforced Self-Compacting Concrete,” Building and Environment, V. 40, No. 12, 2005, pp. 1672-1677. doi: 10.1016/j.buildenv.2004.12.014

20. Wallevik, O. H., and Wallevik, J. E., “Rheology as a Tool in Concrete Science: The Use of Rheographs and Workability Boxes,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1279-1288. doi: 10.1016/j.cemconres.2011.01.009

21. Okamura, H., and Ouchi, M., “Self-Compacting Concrete,” Journal of Advanced Concrete Technology, V. 1, No. 1, 2003, pp. 5-15. doi: 10.3151/jact.1.5

22. Cao, M.; Li, L.; and Xu, L., “Relations between Rheological and Mechanical Properties of Fiber Reinforced Mortar,” Computers and Concrete, V. 20, No. 4, 2017, pp. 449-459.

23. ACI Committee 238, “Report on Measurements of Workability and Rheology of Fresh Concrete (ACI 238.1R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 70 pp.

24. Ding, Y.; Liu, S.; Zhang, Y.; and Thomas, A., “The Investigation on the Workability of Fibre Cocktail Reinforced Self-Compacting High Performance Concrete,” Construction and Building Materials, V. 22, No. 7, 2008, pp. 1462-1470. doi: 10.1016/j.conbuildmat.2007.03.034

25. Pakravan, H. R.; Latifi, M.; and Jamshidi, M., “Hybrid Short Fiber Reinforcement System in Concrete: A Review,” Construction and Building Materials, V. 142, 2017, pp. 280-294. doi: 10.1016/j.conbuildmat.2017.03.059

26. Banyhussan, Q. S.; Yıldırım, G.; Bayraktar, E.; Demirhan, S.; and Şahmaran, M., “Deflection-Hardening Hybrid Fiber Reinforced Concrete: The Effect of Aggregate Content,” Construction and Building Materials, V. 125, 2016, pp. 41-52. doi: 10.1016/j.conbuildmat.2016.08.020

27. Li, Q.; Liu, J.; and Xu, S., “Progress in Research on Carbon Nanotubes Reinforced Cementitious Composites,” Advances in Materials Science and Engineering, V. 2015, 2015, pp. 1-16. doi: 10.1155/2015/249348

28. Parveen, S.; Rana, S.; and Fangueiro, R., “A Review on Nanomaterial Dispersion, Microstructure, and Mechanical Properties of Carbon Nanotube and Nanofiber Reinforced Cementitious Composites,” Journal of Nanomaterials, V. 2013, 2013, pp. 1-19. doi: 10.1155/2013/710175

29. Cao, M.; Zhang, C.; Li, Y.; and Wei, J., “Using Calcium Carbonate Whisker in Hybrid Fiber-Reinforced Cementitious Composites,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 4, 2015, p. 4014139 doi: 10.1061/(ASCE)MT.1943-5533.0001041

30. Kwan, A. K. H.; Fung, W. W. S.; and Wong, H. H. C., “Water Film Thickness, Flowability and Rheology of Cement–Sand Mortar,” Advances in Cement Research, V. 22, No. 1, 2010, pp. 3-14. doi: 10.1680/adcr.2008.22.1.3

31. Vikan, H., and Justnes, H., “Rheology of Cementitious Paste with Silica Fume or Limestone,” Cement and Concrete Research, V. 37, No. 11, 2007, pp. 1512-1517. doi: 10.1016/j.cemconres.2007.08.012

32. Wallevik, J. E., “Rheological Properties of Cement Paste: Thixotropic Behavior and Structural Breakdown,” Cement and Concrete Research, V. 39, No. 1, 2009, pp. 14-29. doi: 10.1016/j.cemconres.2008.10.001

33. Wallevik, J. E., “Thixotropic Investigation on Cement Paste: Experimental and Numerical Approach,” Journal of Non-Newtonian Fluid Mechanics, V. 132, No. 1-3, 2005, pp. 86-99. doi: 10.1016/j.jnnfm.2005.10.007

34. Kuder, K. G.; Ozyurt, N.; Mu, E. B.; and Shah, S. P., “Rheology of Fiber-Reinforced Cementitious Materials,” Cement and Concrete Research, V. 37, No. 2, 2007, pp. 191-199. doi: 10.1016/j.cemconres.2006.10.015

35. Banfill, P. F. G., “Rheology of Fresh Cement and Concrete,” Proceedings of an International Conference, The British Society of Rheology, Liverpool, UK, 2006.

36. Philipse, A. P., “The Random Contact Equation and its Implications for (Colloidal) Rods in Packings, Suspensions, and Anisotropic Powders,” Langmuir, V. 12, No. 24, 1996, p. 5971 doi: 10.1021/la960869o


ALSO AVAILABLE IN:

Electronic Materials Journal