Role of Porosity on Durability of Carbon Fiber-Reinforced Polymer-Concrete Bond

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Role of Porosity on Durability of Carbon Fiber-Reinforced Polymer-Concrete Bond

Author(s): Mostfa Al Azzawi, Gray Mullins, and Rajan Sen

Publication: Structural Journal

Volume: 116

Issue: 6

Appears on pages(s): 75-86

Keywords: bond; carbon fiber-reinforced polymer; composite section; durability; exposure; pulloff; water

DOI: 10.14359/51716801

Date: 11/1/2019

Abstract:
This paper investigates the influence of concrete porosity on durability of the bond between fiber-reinforced polymer (FRP) and concrete. Twenty-four slab specimens were cast using three different concrete mixtures with water-cementitious materials ratios (w/cm) of 0.53, 0.41, and 0.21, representing high, medium, and low porosities, respectiviely. The slabs were preconditioned by oven-drying and two commercially used carbon fiber-reinforced polymer (CFRP) materials bonded to surfaces that had been sand-blasted to provide a concrete surface profile (CSP) 3 rating. Repaired specimens were submerged in 30°C (86°F) potable water for 15 weeks and residual bond was evaluated through pulloff tests. Results showed 1 to 3% bond reduction in the high-porosity, low-strength concrete compared to a reduction in excess of 20% in its low-porosity, higher-strength counterpart. The likely reason for the better performance was deeper epoxy penetration into the more porous concrete substrate. Findings suggest that surface preparation and installation methods that allow epoxy to penetrate deeper into low-porosity, high-strength concrete can result in increased durability under moisture exposure.

Related References:

1. Myers, J. J., “Durability of External Fiber-Reinforced Polymer Strengthening Systems,” Durability of Composites for Civil Structural Applications, V. M. Karbhari, ed., Woodhead Publishing Limited, Cambridge, UK, 2007, pp. 247-283.

2. Dolan, C.; Tanner, J.; Mukai, D.; Hamilton, H.; and Douglas, E., “Report for Evaluating the Durability of Bonded CFRP Repair/Strengthening of Concrete Beams: Technical Data and Discussion Supporting the Draft Final Report of NCHRP Project 12-73,” National Cooperative Highway Research Program, Transportation Research Board, 2009.

3. Sen, R., “Developments in the Durability of FRP-Concrete Bond,” Construction and Building Materials, V. 78, 2015, pp. 112-125. doi: 10.1016/j.conbuildmat.2014.12.106

4. ACI Committee 440, “Guide to Accelerated Conditioning Protocols for Durability Assessment of Internal and External Fiber-Reinforced Polymer (FRP) Reinforcement (ACI 440.9R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 10 pp.

5. Stewart, A., “Study of Cement-Epoxy Interfaces, Accelerated Testing, and Surface Modification,” PhD dissertation, University of Florida, Gainesville, FL, 2012.

6. Tuakta, C., and Büyüköztürk, O., “Deterioration of FRP/Concrete Bond System under Variable Moisture Conditions Quantified by Fracture Mechanics,” Composites. Part B, Engineering, V. 42, No. 2, 2010, pp. 145-154.

7. Mehta, P. K., and Monteiro, P. J., Concrete: Microstructure, Properties and Materials, McGraw-Hill, New York, 2006, 704 pp.

8. Emmons, P. H., Concrete Repair and Maintenance Illustrated, R.S. Means Co., Kingston, MA, 1993.

9. Jeffries, J., “Bond Behavior of Fiber Reinforced Polymer Laminates to Concrete Subjected to Varied Surface Preparation,” MS thesis, Missouri University of Science and Technology, Rolla, MO, 2004.

10. Chajes, M.; Finch, J. W.; Januszka, T. F.; and Thomson, T. A., “Bond and Force Transfer of Composite Material Plates Bonded to Concrete,” ACI Structural Journal, V. 93, No. 2, Mar.-Apr. 1996, pp. 209-217. doi: 10.14359/1491

11. Yoshizawa, H.; Myojo, T.; Okoshi, M.; Mizukoshi, M.; and Kliger, H., “Effect of Sheet Bonding Condition on Concrete Members Having Externally Bonded Carbon Fiber Sheet,” Fourth Materials Engineering Conference, Washington, DC, 1996.

12. Momber, W., “Surface Preparation of Concrete—The German Experience,” Conference of New Application of Water Jet Technology, Isniomaki, Japan, 1999.

13. De Lorenzis, L.; Miller, B.; and Nanni, A., “Bond of Fiber-Reinforced Polymer Laminates to Concrete,” ACI Materials Journal, V. 98, No. 3, May-June 2001, pp. 256-264. doi: 10.14359/10281

14. Maerz, H.; Chepur, P.; Myers, J.; and Linz, J., “Concrete Roughness Characterization Using Laser Profilometry for Fiber-Reinforced Polymer Sheet Application,” Transportation Research Record: Journal of the Transportation Research Board, V. 1775, No. 1, 2001, pp. 132-139. doi: 10.3141/1775-16

15. Shen, X., “Effect of Surface Roughness and Putty Thickness on the Bond Performance of FRP Laminates,” MS thesis, Missouri University of Science and Technology, Rolla, MO, 2002.

16. ICRI, “Selecting and Specifying Concrete Surface Preparation for Sealers, Coatings, Polymers Overlays, and Concrete Repair (ICRI No. 310.2R-2013),” International Concrete Repair Institute, St. Paul, MN, 2013.

17. ACI Committee 440, “Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-02),” American Concrete Institute, Farmington Hills, MI, 2002, 45 pp.

18. Hamlton, H. R.; Brown, J.; Tartar, J.; Lisek, M.; and Benkus, N. R., “Durability Evaluation of Florida’s Fiber-Reinforced Polymer (FRP) Composite Reinforcement for Concrete Structures,” Final Report for FDOT Contract No. BVD31-977-01, 2017.

19. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 2017, 112 pp.

20. Al Azzawi, M.; Hopkins, P.; Mullins, G.; and Sen, R., “FRP-Concrete Bond after 12 Year Exposure in Tidal Waters,” Journal of Composites for Construction, ASCE, V. 22, No. 5, 2018, pp. 1-15. doi: 10.1061/(ASCE)CC.1943-5614.0000864

21. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

22. ASTM C39/C39M-18, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens, ASTM International, West Conshohocken, PA, 2018, 8 pp.

23. Delagrave, A.; Bigas, J.; Ollivier, J. P.; Marchand, J.; and Pigeon, M., “Influence of the Interfacial Zone on the Chloride Diffusivity of Mortars,” Advanced Cement Based Materials, V. 5, No. 3-4, 1997, pp. 86-92. doi: 10.1016/S1065-7355(96)00008-9

24. Winslow, D. N., and Diamond, S., “A Mercury Porosometry Study of the Porosity In Portland Cement,” Journal of Materials, V. 5, 1970, pp. 564-585.

25. Cho, S.-W., “Using Mercury Intrusion Porosometry to Study the Interfacial Properties of Cement-Based Materials,” Journal of Marine Science and Technology, V. 20, 2012, pp. 269-273.

26. Aligizaki, K. K., Pore Structure of Cement-Based Materials: Testing, Interpretation, and Requirements, CRC Press, Boca Raton, FL, 2005.

27. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 3 pp.

28. ASTM D7522/D7522M-09, “Standard Test Method for Pulloff Strength for FRP Laminate Systems Bonded to Concrete Substrate,” ASTM International, West Conshohocken, PA, 2009, 6 pp.

29. Al Azzawi, M.; Hopkins, P.; Ross, J.; Mullins, G.; and Sen, R., “Carbon Fiber-Reinforced Polymer Concrete Masonry Unit Bond after 20 Years of Outdoor Exposure,” ACI Structural Journal, V. 115, No. 4, July 2018, pp. 971-982. doi: 10.14359/51702226

30. Al Azzawi, M., “Investigations on FRP-Concrete Bond,” PhD dissertation, Department of Civil and Environmental Engineering, University of South Florida, Tampa, FL, 2018.

31. Lau, D., and Büyüköztürk, O., “Fracture Characterization of Concrete/Epoxy Interface Affected by Moisture,” Mechanics of Materials, V. 42, No. 12, 2010, pp. 1031-1042. doi: 10.1016/j.mechmat.2010.09.001

32. Detwiler, R. J.; Thomas, W.; Stangebye, T.; and Urahn, M., “Variability of 4x8 Cylinder Tests,” Concrete International, V. 31, No. 5, May 2009, pp. 43-47.

33. Illig, G., “Concrete Repair, Strengthening and Protection,” guest lecture, University of South Florida, Tampa, FL, Apr. 11, 2018.


ALSO AVAILABLE IN:

Electronic Structural Journal