Shear Strength of Top Slab of Reinforced Concrete Box Culverts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Top Slab of Reinforced Concrete Box Culverts

Author(s): Masoud Ghahremannejad, Ali Abolmaali, and Maziar Mahdavi

Publication: Structural Journal

Volume: 116

Issue: 6

Appears on pages(s): 63-74

Keywords: box culverts; displacement control; framework; shear behavior; uniformly distributed load

DOI: 10.14359/51716800

Date: 11/1/2019

Abstract:
An increase in the fill height of buried box culverts leads to an increase in the thickness of the slab and wall, as well as in the number or size of longitudinal slab reinforcements required to resist flexure. This geometrical configuration imposes a shear behavioral mode. This study focuses on determining the shear strength of reinforced concrete (RC) box culverts with uniformly distributed load at the top slab. A framework, consisting of several subframes, was designed to convert the single displacement applied at the top of the framework to the equivalent uniformly distributed forces at the top slab of the culvert, allowing a displacement control analysis algorithm to be performed. To validate the loading mechanism, using the proposed framework, the load was applied on the top of an RC beam in the laboratory, and numerical studies were conducted. After validation, two sizes of RC box culverts were experimentally and numerically investigated. The results from the experimental program and verified numerical models differed from ACI 318-14 formulation for the shear strength of top slabs of RC box culverts.

Related References:

1. AASHTO, “AASHTO LRFD Bridge Design Specification,” seventh edition, American Association of State Highway and Transportation Officials, Washington, DC, 2014.

2. ASTM C1577-15a, “Standard Specification for Precast Reinforced Concrete Monolithic Box Section for Culverts, Storm Drains, and Sewer Designed According to AASHTO LRFD,” ASTM International, West Conshohocken, PA, 2015, 22 pp.

3. Abolmaali, A., and Garg, A. K., “Effect of Wheel Live Load on Shear Behavior of Precast Reinforced Concrete Box Culverts,” Journal of Bridge Engineering, ASCE, V. 13, No. 1, 2008, pp. 93-99. doi: 10.1061/(ASCE)1084-0702(2008)13:1(93)

4. Hassan, T. K.; Seliem, H. M.; Dwairi, H.; Rizkalla, S. H.; and Zia, P., “Shear Behavior of Large Concrete Beams Reinforced with High-Strength Steel,” ACI Structural Journal, V. 105, No. 2, Mar.-Apr. 2008, pp. 173-179.

5. Zarrinpour, M. R., and Chao, S. H., “Shear Strength Enhancement Mechanisms of Steel Fiber-Reinforced Concrete Slender Beams,” ACI Structural Journal, V. 114, No. 3, May-June 2017, pp. 729-742. doi: 10.14359/51689449

6. Bažant, Z. P., and Kim, J. K., “Size Effect in Shear Failure of Longitudinally Reinforced Beams,” ACI Journal Proceedings, V. 81, No. 5, Sept.-Oct. 1984, pp. 456-468.

7. Shioya, T.; Iguro, M.; Nojiri, Y.; Akiyama, H.; and Okada, T., “Shear Strength of Large Reinforced Concrete Beams,” Special Publication, Fracture Mechanics, V. 118, 1990, pp. 259-280.

8. Vecchio, F. J., and Shim, W., “Experimental and Analytical Reexamination of Classic Concrete Beam Tests,” Journal of Structural Engineering, ASCE, V. 130, No. 3, 2004, pp. 460-469. doi: 10.1061/(ASCE)0733-9445(2004)130:3(460)

9. Collins, M. P.; Mitchell, D.; Adebar, P.; and Vecchio, F. J., “A General Shear Design Method,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb. 1996, pp. 36-45.

10. Vecchio, F. J., and Collins, M. P., “The Modified Compression-Field Theory for Reinforced Concrete Element Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

11. Yee, R. A., “Shear Behavior of Concrete Box Culverts,” Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2003.

12. CHBDC, “Canadian Highway Bridge Design Code,” Canadian Standards Association, Mississauga, ON, Canada, 2000.

13. Sherwood, E. G.; Lubell, A. S.; Bentz, E. C.; and Collins, M. P., “One-Way Shear Strength of Thick Slabs and Wide Beams,” ACI Structural Journal, V. 103, No. 6, Nov.-Dec. 2006, pp. 794-802.

14. Ghahremannejad, M., and Abolmaali, A., “Prediction of Shear Strength of Reinforced Concrete Beams using Displacement Control Finite Element Analysis,” Engineering Structures Journal, V. 169, 2018, pp. 226-237. doi: 10.1016/j.engstruct.2018.05.048

15. Ghahremannejad, M., and Abolmaali, A., “Shear Capacity of Reinforced Concrete Box Culverts Compared with AASHTO Shear Equation,” Journal of Bridge Engineering, ASCE, V. 24, No. 5, 2019, p. 04019032. doi: 10.1061/(ASCE)BE.1943-5592.0001389

16. Ghahremannejad, M., “Experimental and Numerical Investigation of the Concrete Shear Strength of Reinforced Concrete Box Culverts under Uniformly Distributed Load,” PhD dissertation, The University of Texas at Arlington, Civil Engineering Department, Arlington, TX.

17. Ghahremannejad, M.; Mahdavi, M.; Saleh, A. E.; Abhaee, S.; and Abolmaali, A., “Experimental Investigation and Identification of Single and Multiple Cracks in Synthetic Fiber Concrete Beams,” Case Studies in Construction Materials, V. 9, 2018. doi: 10.1016/j.cscm.2018.e00182

18. Pang, P. L. R., and Millar, M. A., “Experimental Behavior of a Fixed Ended Beam under Simulated Uniformly Distributed Load,” International Journal of Mechanical Sciences, V. 20, No. 10, 1978, pp. 675-683. doi: 10.1016/0020-7403(78)90054-1

19. Brown, M. D., and Bayrak, O., “Investigation of Deep Beams with Various Load Configurations,” ACI Structural Journal, V. 104, No. 5, Sept.-Oct. 2007, pp. 518-611.

20. Zararis, P. D., and Zararis, I. P., “Shear Strength of Reinforced Concrete Beams under Uniformly Distributed Loads,” ACI Structural Journal, V. 105, No. 6, Nov.-Dec. 2008, pp. 711-719.

21. Iguro, M.; Shioya, T.; Nojiri, Y.; and Akiyama, H., “Experimental Studies on Shear Strength of Large Reinforced Concrete Beams under Uniformly Distributed Load,” Concrete Library of JSCE, No. 5, 1985.

22. Klaus, T. P. R., “Shear Behavior of Reinforced Concrete Box Culverts,” Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2007.

23. May, I. M.; Naji, J. H.; and Ganaba, T. H., “Displacement Control for the Non-Linear Analysis of Reinforced Concrete Structures,” Journal of Engineering Computations, V. 5, No. 4, 1988, pp. 266-273. doi: 10.1108/eb023745

24. Zheng, H.; Liu, D. F.; Lee, C. F.; and Tham, L. G., “Displacement-Controlled Method and Its Applications to Material Non-Linearity,” International Journal for Numerical and Analytical Methods in Geomechanics, V. 29, No. 3, 2005, pp. 209-226. doi: 10.1002/nag.410

25. ASTM A615-615M, “Standard Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016, 6 pp.

26. ABAQUS 6.14 Documentation, ABAQUS Manual, version 6.14, Pawtucket, RI, 2016.

27. Garg, A. K., and Abolmaali, A., “Finite-Element Modeling and Analysis of Reinforced Concrete Box Culverts,” Journal of Transportation Engineering, ASCE, V. 135, No. 3, 2009, pp. 121-128. doi: 10.1061/(ASCE)0733-947X(2009)135:3(121)

28. Chen, G. M.; Chen, J. F.; and Teng, J. G., “On the Finite Element Modeling of RC Beams Shear-Strengthened with FRP,” Construction and Building Materials, V. 32, 2012, pp. 13-26. doi: 10.1016/j.conbuildmat.2010.11.101

29. Jankowiak, T., and Lodygowski, T., “Identification of Parameters of Concrete Damage Plasticity Constitutive Model,” Foundations of Civil and Environmental Engineering, No. 6, 2005, pp. 53-69.

30. Nagy, N. M.; Eltehawy, E. A.; Elhanafy, H. M.; and Eldesouky, A., “Numerical Modeling of Geometrical Analysis for Underground Structures,” 13th International Conference on Aerospace Science & Aviation Technology, Paper: ASAT-13-CV-22, 2009.

31. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal