Splitting of Concrete with Steel, Glass Fiber-Reinforced Polymer, and Basalt Fiber-Reinforced Polymer Bars Exposed to MgSO4

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Splitting of Concrete with Steel, Glass Fiber-Reinforced Polymer, and Basalt Fiber-Reinforced Polymer Bars Exposed to MgSO4

Author(s): Yail J. Kim and Yufei Chai

Publication: Structural Journal

Volume: 117

Issue: 3

Appears on pages(s): 3-16

Keywords: bond; deterioration; durability; fiber-reinforced polymer (FRP); interface; magnesium sulfate; performance-based design

DOI: 10.14359/51726799

Date: 5/1/2020

Abstract:
This paper presents the splitting characteristics of concrete interfaced with various reinforcing bars when subjected to magnesium sulfate. Glass and basalt fiber-reinforced polymer composites (GFRP and BFRP, respectively) and conventional deformed steel bars are employed, and their performance is comparatively studied. Interface test specimens are prepared and submerged in a magnesium sulfate solution at a 5% concentration for 10 weeks. Based on the gray level co-occurrence matrix (GLCM) method, microscopic investigations are conducted to examine the surface texture of these reinforcing bars. The initiation and progression of splitting cracks are visually assessed by digital image correlation (DIC). The measured potential of hydrogen (pH) indicates that the concrete reacts with magnesium sulfate, which permeates through the cement paste and weakens the concrete-reinforcement interface. The surface morphology of the reinforcement controls the interfacial behavior together with the condition of the concrete substrate deteriorated by the solution. The capacity reduction rate of the BFRP bars is the least among the three reinforcing types, although the load-carrying capacity of the steel is higher than that of the GFRP and BFRP. The fracture energy of the interface is quantified, and its spatial distribution is elaborated. The developed analytical model predicts the circumferential stress and internal pressure of the test specimens, which are crucial to understand the splitting mechanism of the interface. The random uncertainty of the reinforcing bars interacting with the concrete deteriorated by magnesium sulfate is appraised. For design recommendations, environmental reduction factors are calibrated as per reliability performance.

Related References:

1. Shehata, M. H.; Adhikari, G.; and Radomski, S., “Long-Term Durability of Blended Cement against Sulfate Attack,” ACI Materials Journal, V. 105, No. 6, Nov.-Dec. 2008, pp. 594-602.

2. Monteiro, P. J. M., and Kurtis, K. E., “Time to Failure for Concrete Exposed to Severe Sulfate Attack,” Cement and Concrete Research, V. 33, No. 7, 2003, pp. 987-993. doi: 10.1016/S0008-8846(02)01097-9

3. O’Connell, M.; McNally, C.; and Richardson, M. G., “Biochemical Attack on Concrete in Wastewater Applications: A State of the Art Review,” Cement and Concrete Composites, V. 32, No. 7, 2010, pp. 479-485. doi: 10.1016/j.cemconcomp.2010.05.001

4. Bonen, D., and Cohen, M. D., “Magnesium Sulfate Attack on Portland Cement Paste II: Chemical and Mineralogical Analyses,” Cement and Concrete Research, V. 22, No. 4, 1992, pp. 707-718. doi: 10.1016/0008-8846(92)90023-O

5. Dyer, T., Concrete Durability, CRC Press, Boca Raton, FL, 2014.

6. Collepardi, M. “A State-of-the-Art Review on Delayed Ettringite Attack on Concrete,” Cement and Concrete Composites, V. 25, No. 4-5, 2003, pp. 401-407. doi: 10.1016/S0958-9465(02)00080-X

7. Nanni, A., “North American Design Guidelines for Concrete Reinforcement and Strengthening Using FRP: Principles, Applications, and Unresolved Issues,” Construction and Building Materials, V. 17, No. 6-7, 2003, pp. 439-446. doi: 10.1016/S0950-0618(03)00042-4

8. Cheng, L., and Karbhari, V. M., “New Bridge Systems Using FRP Composites and Concrete: a State-of-the-Art Review,” Progress in Structural Engineering and Materials, V. 8, No. 4, 2006, pp. 143-154. doi: 10.1002/pse.221

9. Benmokrane, B.; El-Salakawy, E.; El-Ragaby, A.; and El-Gamal, S., “Performance Evaluation of Innovative Concrete Bridge Deck Slabs Reinforced with Fiber-Reinforced Polymer Bars,” Canadian Journal of Civil Engineering, V. 34, No. 3, 2007, pp. 298-310. doi: 10.1139/l06-173

10. Ovitigala, T.; Ibrahim, M. A.; and Issa, M. A., “Serviceability and Ultimate Load Behavior of Concrete Beams Reinforced with Basalt Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 113, No. 4, July-Aug. 2016, pp. 757-768. doi: 10.14359/51688752

11. Kara, I. F.; Koroglu, M. A.; and Ashour, A. F., “Tests of Continuous Concrete Slabs with Basalt Fiber-Reinforced Plastic Bars,” ACI Structural Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 1201-1213. doi: 10.14359/51689784

12. Benmokrane, B.; Wang, P.; Ton-That, T. M.; Rahman, H.; and Robert, J.-F., “Durability of Glass Fiber-Reinforced Polymer Reinforcing Bars in Concrete Environment,” Journal of Composites for Construction, ASCE, V. 6, No. 3, 2002, pp. 143-153. doi: 10.1061/(ASCE)1090-0268(2002)6:3(143)

13. Wambeke, B. W., and Shield, C. K., “Development Length of Glass Fiber-Reinforced Polymer Bars in Concrete,” ACI Structural Journal, V. 103, No. 1, Jan.-Feb. 2006, pp. 11-17.

14. Harajli, M., and Abouniaj, M., “Bond Performance of GFRP Bars in Tension: Experimental Evaluation and Assessment of ACI 440 Guidelines,” Journal of Composites for Construction, ASCE, V. 14, No. 6, 2010, pp. 659-668. doi: 10.1061/(ASCE)CC.1943-5614.0000139

15. Pay, A. C.; Canbay, E.; and Frosch, R. J., “Bond Strength of Spliced Fiber-Reinforced Polymer Reinforcement,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2014, pp. 257-266.

16. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

17. ACI Committee 440, “Guide to Accelerated Conditioning Protocols for Durability Assessment of Internal and External Fiber-Reinforced Polymer (FRP) Reinforcement (ACI 440.9R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 10 pp.

18. ASTM C39/C39M-16, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2016, 7 pp.

19. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

20. ACI Committee 440, “Guide Test Methods for Fiber-Reinforced Polymer (FRP) Composites for Reinforcing of Strengthening Concrete and Masonry Structures (ACI 440.3R-12),” American Concrete Institute, Farmington Hills, MI, 2012, 23 pp.

21. Joint ACI-ASCE Committee 408, “Bond and Development of Straight Reinforcing Bars in Tension (ACI 408R-03),” American Concrete Institute, Farmington Hills, MI, 2003, 49 pp.

22. Drimalas, T.; Clement, J. C.; Folliard, K. J.; Dhole, R.; and Thomas, M. D., “Laboratory and Field Evaluations of External Sulfate Attack in Concrete,” Center for Transportation Research, University of Texas at Austin, Austin, TX, 2011.

23. Hassan, A.; Mahmud, H. B.; Jumaat, M. Z.; Alsubari, B.; and Abdulla, A., “Effect of Magnesium Sulphate on Self-Compacting Concrete Containing Supplementary Cementitious Materials,” Advances in Materials Science and Engineering, V. 2013, 2013, 8 pp. doi: 10.1155/2013/232371

24. ASTM D1193-06, “Standard Specification for Reagent Water,” ASTM International, West Conshohocken, PA, 2006, 6 pp.

25. Hernández, B.; Olague, G.; Hammoud, R.; Trujillo, L.; and Romero, E., “Visual Learning of Texture Descriptors for Facial Expression Recognition in Thermal Imagery,” Computer Vision and Image Understanding, V. 106, No. 2-3, 2007, pp. 258-269. doi: 10.1016/j.cviu.2006.08.012

26. Beura, S.; Majhi, B.; and Dash, R., “Mammogram Classification Using Two Dimensional Discrete Wavelet Transform and Gray-Level Co-Occurrence Matrix for Detection of Breast Cancer,” Neurocomputing, V. 154, 2015, pp. 1-14. doi: 10.1016/j.neucom.2014.12.032

27. Ferreira, T., and Rashband, W., The ImageJ User Guide, National Institute of Health, Bethesda, MD, 2012.

28. Haralick, R. M.; Shanmugam, K.; and Dinstein, I., “Textural Features for Image Classification,” IEEE Transactions on Systems, Man, and Cybernetics, V. SMC-3, No. 6, 1973, pp. 610-621. doi: 10.1109/TSMC.1973.4309314

29. Liu, Z.; Deng, D.; De Schutter, G.; and Yu, Z., “The Effect of MgSO4 on Thaumasite Formation,” Cement and Concrete Composites, V. 35, No. 1, 2013, pp. 102-108. doi: 10.1016/j.cemconcomp.2012.08.011

30. Makhloufi, Z.; Aggoun, S.; Benabed, B.; Kadri, E. H.; and Bederina, M., “Effect of Magnesium Sulfate on the Durability of Limestone Mortars Based on Quaternary Blended Cements,” Cement and Concrete Composites, V. 65, 2016, pp. 186-199. doi: 10.1016/j.cemconcomp.2015.10.020

31. Mehta, P. K., and Monteiro, P. J. M., Concrete: Microstructure, Properties, and Materials, McGraw Hill, New York, 2014.

32. “CEB-FIP Model Code,” Comite Euro-international du Beton, Thomas Telford, Lausanne, Switzerland, 1993.

33. Ugural, A. C., and Fenster, S. K., Advanced Strength and Applied Elasticity, Prentice Hall, Upper Saddle River, NJ, 1995.

34. Gupta, S. V., Measurement Uncertainties, Springer, Berlin, Germany, 2012.

35. Lind, N. C., “Consistent Partial Safety Factors,” Journal of the Structural Division, ASCE, V. 97, 1971, pp. 1651-1669.

36. Barker, R. M., and Puckett, J. A., Design of Highway Bridges: An LRFD Approach, John Wiley & Sons, Inc., Hoboken, NJ, 2013.

37. ISO 13822, “Bases for the Design of Structures—Assessment of Existing Structures,” International Organization for Standardization, Geneva, Switzerland, 2010.

38. Darwin, D.; McCabe, S. L.; Idun, E. K.; and Schoenekase, S. P., “Development Length Criteria: Bars Not Confined by Transverse Reinforcement,” ACI Structural Journal, V. 89, No. 6, Nov.-Dec. 1992, pp. 709-720.


ALSO AVAILABLE IN:

Electronic Structural Journal