Title: Modeling of Hysteretic Response for Concrete Shear Walls Reinforced with Glass Fiber-Reinforced Polymer Bars

Author(s): Ahmed Hassanein, Nayera Mohamed, Ahmed Sabry Farghaly, and Brahim Benmokrane

Publication: Structural Journal

Volume: 116

Issue: 6

Appears on pages(s): 17-29

Keywords: analytical modeling; energy dissipation; glass fiber-reinforced ploymer GFRP bars; hysteretic response; lateral load; reinforced concrete; seismic performance; shear wall; stiffness

DOI: 10.14359/51716798

Date: 11/1/2019

Abstract:
Glass fiber-reinforced-polymer (GFRP) bars are increasingly recognized as being suitable as the primary reinforcement in concrete structures. In recent years, many researchers have been studying their seismic performance as a lateral resisting system. Because of the lack of experimental data, GFRP bars are still not recommended for seismic design. Given the need for comprehensive seismic-performance assessment, hysteretic models must be developed depending on GFRP bar properties. The primary purpose of this study was to identify the various parameters controlling the hysteretic response of GFRP-reinforced shear walls. Six fullscale specimens reinforced entirely with GFRP bars were recently constructed and tested under the combined action of reversed cyclic lateral load and constant axial load. The test results show stable performance and an acceptable level of deformability. An analytical model was developed using the experimental results for correlation, aiming to reproduce the hysteretic response. The model was achieved by investigating the parameters that control the hysteretic response and studying their effect on the deterioration rate. The cumulative dissipated energy, the cyclic distortion due to stiffness degradation, and the idealized load-displacement curve were analyzed. The proposed model was compared with the experimentally generated response and simulated the hysteretic response of GFRP-reinforced shear walls with acceptable accuracy.

Related References:

ACI Committee 440, 2006, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.

Aktan, A. E.; Bertero, V. V.; and Sakino, K., 1985, “Lateral Stiffness Characteristics of Reinforced Concrete Frame-Wall Structures,” Deflections of Concrete Structures, SP-86, American Concrete Institute, Farmington Hills, MI, pp. 231-262.

ASCE/SEI 41-13, 2013, “Seismic Evaluation and Retrofit of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 518 pp.

ASTM D7205/7205M-06(2011), 2011, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA.

Benmokrane, B.; Chaallal, O.; and Masmoudi, R., 1996, “Flexural Response of Concrete Beams with FRP Reinforcing Bars,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb., pp. 46-55.

Canadian Commission on Building and Fire Codes, 2015, “National Building Code of Canada (NBCC),” National Research Council of Canada, Montreal, QC, Canada.

Canadian Standards Association, 2012, “Design and Construction of Building Components with Fiber-Reinforced Polymers (CSA S806-12),” CSA Group, Mississauga, ON, Canada, 208 pp.

Canadian Standards Association, 2014, “Design of Concrete Structures (CSA A23.3-14),” CSA Group, Mississauga, ON, Canada, 290 pp.

Clough, R. W., and Johnston, S. B., 1966, “Effect of Stiffness Degradation on Earthquake Ductility Requirements,” Proceedings of Japan Earthquake Engineering Symposium, Tokyo, Japan.

Mohamed, N.; Farghaly, A. S.; Benmokrane, B.; and Neale, K. W., 2014, “Experimental Investigation of Concrete Shear Walls Reinforced with Glass Fiber-Reinforced Bars under Lateral Cyclic Loading,” Journal of Composites for Construction, ASCE, V. 18, No. 3, p. 04014001. doi: 10.1061/(ASCE)CC.1943-5614.0000393

Rahnama, M., and Krawinkler, H., 1993, “Effects of Soft Soil and Hysteresis Model on Seismic Demands,” John A. Blume Earthquake Engineering Center Report No. 108, Department of CEE, Stanford University, Stanford, CA.

Roufaiel, M. S. L., and Meyer, C., 1987, “Analytical Modeling of Hysteretic Behavior of R/C Frames,” Journal of Structural Engineering, ASCE, V. 113, No. 3, pp. 429-444. doi: 10.1061/(ASCE)0733-9445(1987)113:3(429)

Sharbatdar, M. K., 2003, “Concrete Columns and Beams Reinforced with FRP Bars and Grids under Monotonic and Cyclic Loading,” PhD thesis, University of Ottawa, Ottawa, ON, Canada.

Sivaselvan, M. V., and Reinhorn, A. M., 2000, “Hysteretic Models for Deteriorating Inelastic Structures,” Journal of Engineering Mechanics, ASCE, V. 126, No. 6, pp. 633-640. doi: 10.1061/(ASCE)0733-9399(2000)126:6(633)

Song, J., and Pincheira, J. 2000, “Spectral Displacement Demands of Stiffness and Strength Degrading Systems,” Earthquake Spectra, V. 16, No. 4, pp. 817-851. doi: 10.1193/1.1586141

Takeda, T.; Sozen, M. A.; and Nielson, N. N., 1970, “Reinforced Concrete Response to Simulated Earthquakes,” Journal of the Structural Division, V. 96, pp. 2557-2573.

Veletsos, A. S.; Newmark, N. M.; and Chelapati, C. V., 1965, “Deformation Spectra for Elastic and Elastoplastic Systems Subjected to Ground Shock and Earthquake Motions,” Proceedings of 3rd World Conference on Earthquake Engineering, V. II, pp. 663-682.

Wen, Y. K., 1976, “Method for Random Vibration of Hysteretic Systems,” Journal of the Engineering Mechanics Division, V. 112, pp. 249-263.