Uncertainty Modeling of Carbon Fiber-Reinforced Polymer- Confined Concrete in Acid-Induced Damage

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Uncertainty Modeling of Carbon Fiber-Reinforced Polymer- Confined Concrete in Acid-Induced Damage

Author(s): Yail J. Kim, Yongcheng Ji, and Troy Butler

Publication: Structural Journal

Volume: 116

Issue: 6

Appears on pages(s): 97-108

Keywords: fiber-reinforced polymer (FRP); inverse problem; mathematical modeling; stochastic; sulfuric acid; uncertainty quantification

DOI: 10.14359/51716761

Date: 11/1/2019

Abstract:
This paper presents a novel modeling approach to predict the response of parameters constituting the strength of concrete cylinders confined with carbon fiber-reinforced polymer (CFRP) sheets under an acidic environment (pre-conditioned concrete is strengthened). Contrary to conventional modeling that requires specific parameter values to solve for the strength of the confined concrete, the stochastic inverse method mathematically infers individual parameter values without prior information based on a known confined strength. Accordingly, the implications of each parameter on the strength development of the confined concrete are quantified. The modeling approach is validated against a previously conducted experimental program and is employed for parametric investigations with various geometric and material properties as well as with variable sulfuric acid exposure periods. The cylinder diameter affects the surety of the strength variation in terms of occurrence probability. The rate of strength decrease in the confined concrete is pronounced when the core concrete has been initially exposed to sulfuric acid, while the rate slows down as the exposure time progresses. High-strength CFRP materials noticeably increase the strength of the confined concrete; however, the efficiency of enhancement diminishes with the CFRP strength. The functionality of the concrete confined by multiple CFRP layers is examined. Upon assessing the empirically calibrated factors of existing design guidelines, new factors are proposed for strength prediction of the confined concrete. To substantiate the distinct effects of the sulfuric acid exposure time, the strength of the confined concrete is characterized by a Euclidean distance-based clustering technique. The uncertainty associated with the CFRP-confinement is elucidated and contributing attributes are identified.

Related References:

1. Li, C. Q., and Melchers, R. E., “Time-Dependent Reliability Analysis of Corrosion-Induced Concrete Cracking,” ACI Structural Journal, V. 102, No. 4, July-Aug. 2005, pp. 543-549.

2. Attigbe, E. K., and Rizkalla, S. H., “Response of Concrete to Sulfuric Acid Attack,” ACI Materials Journal, V. 85, No. 6, Nov.-Dec. 1988, pp. 481-488.

3. O’Connell, M.; McNally, C.; and Richardson, M. G., “Biochemical Attack on Concrete in Wastewater Applications: A State-of-the-Art Review,” Cement and Concrete Composites, V. 32, No. 7, 2010, pp. 479-485. doi: 10.1016/j.cemconcomp.2010.05.001

4. Monteny, J.; De Belie, N.; Vincke, E.; Verstraete, W.; and Taerwe, L., “Chemical and Microbiological Tests to Simulate Sulfuric Acid Corrosion of Polymer-Modified Concrete,” Cement and Concrete Research, V. 31, No. 9, 2001, pp. 1359-1365. doi: 10.1016/S0008-8846(01)00565-8

5. Araghi, H. J.; Nikbin, I. M.; Reskati, S. R.; Rahmani, E.; and Allahyari, H., “An Experimental Investigation on the Erosion Resistance of Concrete Containing Various PET Particles Percentages Against Sulfuric Acid Attack,” Construction and Building Materials, V. 77, 2015, pp. 461-471. doi: 10.1016/j.conbuildmat.2014.12.037

6. Aydin, H.; Gravina, R. J.; and Visintin, P., “Effects of Moisture, Chlorides and Sulphuric Acid Attack on CFRP to Concrete Bond Interfaces,” 23rd Australasian Conference on the Mechanics of Structures and Materials (ACMSM23), Byron Bay, NSW, Australia, 2014, pp. 409-414.

7. Kim, Y. J., and Ji, Y., “Axial Load-Bearing Concrete Confined with Carbon Fiber-Reinforced Polymer Sheets in Acidic Environment,” ACI Structural Journal, V. 114, No. 3, May-June 2017, pp. 775-786. doi: 10.14359/51689464

8. Folland, G. B., Real Analysis: Modern Techniques and Their Applications, John Wiley & Sons, Inc., New York, 2008.

9. Butler, T.; Estep, D.; Tavener, S.; Dawson, C.; and Westerink, J. J., “A Measure-Theoretic Computational Method for Inverse Sensitivity Problems III: Multiple Quantities of Interest,” SIAM/ASA Journal on Uncertainty Quantification, V. 2, No. 1, 2012, pp. 174-202.

10. Montgomery, D. C., and Runger, G. C., Applied Statistics and Probability for Engineers, John Wiley & Sons, Inc., New York, 2003.

11. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 2017, 112 pp.

12. ACI Committee 440, “Report on Fiber-Reinforced Polymer (FRP) Reinforcement for Concrete Structures (ACI 440R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 100 pp.

13. Liu, J., and Vipulanandan, C., “Modeling Water and Sulfuric Acid Transport through Coted Cement Concrete,” Journal of Engineering Mechanics, ASCE, V. 129, No. 4, 2003, pp. 426-437. doi: 10.1061/(ASCE)0733-9399(2003)129:4(426)

14. Fan, Y.-F., and Luan, H.-Y., “Pore Structure in Concrete Exposed to Acid Deposit,” Construction and Building Materials, V. 49, 2013, pp. 407-416. doi: 10.1016/j.conbuildmat.2013.08.075

15. Gmurman, V. E., Fundamentals of Probability Theory and Mathematical Statistics, Elsevier, New York, 1968.

16. Lam, L., and Teng, J. G., “Design-Oriented Stress-Strain Model for FRP-Confined Concrete,” Construction and Building Materials, V. 17, No. 6-7, 2003, pp. 471-489. doi: 10.1016/S0950-0618(03)00045-X

17. Wu, J., Advances in K-Means Clustering, Springer, Berlin, Germany, 2012.

18. Chun, M.-H.; Han, S.-J.; and Tak, N.-I., “An Uncertainty Importance Measure Using a Distance Metric for the Change in a Cumulative Distribution Function,” Reliability Engineering & System Safety, V. 70, No. 3, 2000, pp. 313-321. doi: 10.1016/S0951-8320(00)00068-5


ALSO AVAILABLE IN:

Electronic Structural Journal