ASCE 41 versus TEASPA: Comparison of Seismic Evaluation Results of RC Frame Buildings Damaged During 2016 Meinong Earthquake, Taiwan

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASCE 41 versus TEASPA: Comparison of Seismic Evaluation Results of RC Frame Buildings Damaged During 2016 Meinong Earthquake, Taiwan

Author(s): Jiun-Wei Lai, ShyhJiann Hwang, Insung Kim, Daniel Zepeda, Garrett Hagen, Kirk Johnston

Publication: Web Session

Volume: ws_F18_Jiu-Wei.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/15/2018

Abstract:
Seismic evaluation results of 3 RC frame buildings in accordance with ASCE 41-13 and Taiwan Earthquake Assessment for Structures by Pushover Analysis (TEASPA) will be presented. The comparison of evaluation results with the actual damages in the buildings observed from the reconnaissance trip will be presented as well.