An Enhanced Procedure to Measure Strength and Durability of Pozzolans

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Enhanced Procedure to Measure Strength and Durability of Pozzolans

Author(s): Edwin R. Dunstan Jr.

Publication: Materials Journal

Volume: 116

Issue: 4

Appears on pages(s): 183-192

Keywords: alkali-silica reaction; chemical reaction; durability; fly ash; pozzolan; pozzolanic reaction; self-cementing reaction; strength; sulfate resistance

DOI: 10.14359/51716721

Date: 7/1/2019

Abstract:
The current ASTM C311 test method to determine strength activity index (SAI) of fly ash and pozzolans was introduced in the 1980s. ASTM C618 specifies that a fly ash or pozzolan should have a minimum SAI of 75%. The SAI limit is inadequate because marginal materials, which are neither pozzolanic nor partially cementitious materials, are known to meet the 75% limit. A strength efficiency test procedure is proposed to replace the current SAI test. Strength efficiency of a fly ash or pozzolan is subdivided into efficiency from chemical reaction (pozzolanic and cementitious) and efficiency from changes in water-cement ratio (non-chemical impacts). A new specification limit is proposed based on chemical efficiency. In turn, chemical reaction is subdivided into pozzolanic and self-cementing reactions, which coincides with the recent 18% CaO% specification that separates Class C and Class F fly ashes.

Related References:

1. Dunstan Jr., E. R., “Performance of Lignite and Subbituminous Fly Ash in Concrete—A Progress Report,” Report No. REC-ERC-76-1, Bureau of Reclamation. Denver, CO, Jan. 1976.

2. Dunstan Jr., E. R., “Fly Ash and Fly Ash Concrete,” Report No. REC-ERC-82-1, Bureau of Reclamation, Denver, CO, May 1984.

3. Dunstan Jr. ,E. R., “A Possible Method for Identifying Fly Ashes Which Will Improve the Sulfate Resistance of Concretes,” Cement, Concrete and Aggregates, V. 2, No. 1, 1980, pp. 20-30. doi: 10.1520/CCA10175J

4. Dunstan Jr., E. R., “A SPEC Odyssey—Sulfate Resistant Concrete for the 1980’s,” George Verbeck Symposium on Sulfate Resistance of Concrete, SP-77, American Concrete Institute, Farmington Hills, MI, 1982, pp. 41-62.

5. Dunstan Jr., E. R., “The Effect of Fly Ash on Alkali-Aggregate Reaction in Concrete,” Cement, Concrete and Aggregates, V. 2, No. 2, 1981, pp. 101-104.

6. Powers, T. C., “The Physical Structure and Engineering Properties of Concrete,” Bulletin 90, Portland Cement Association, Chicago, IL, July 1958, 29 pp.

7. Dunstan Jr., E. R., and Zayed, A., “A Logical Pozzolanic Index and Its Use in Concrete Proportioning,” Journal of ASTM International, V. 3, No. 4, Apr. 2006, pp. 1-12.

8. Dunstan Jr., E. R., “Ash-in-Concrete Model Development,” GS-6129, Research Project 2422-16, Electric Power Research Institute, Palo Alto, CA, Jan. 1989.

9. Davis, R. E.; Carlson, R. W.; Kelly, J. W.; and Davis, H. E., “Properties of Cements and Concretes Containing Fly Ash,” ACI Journal Proceedings, V. 33, No. 5, May 1937, pp. 577-612.

10. Schlorholtz, S., “Supplementary Cementitious Materials,” STP 169D-EB, ASTM International, May 2006, pp. 495-511.

11. Dunstan Jr., E. R., “What is a “Practical” (ASTM C618) SAI Strength Activity Index for Fly Ashes That Can be Used to Proportion Concretes Containing Fly Ash?” Proceedings of World of Coal Ash 2017, Lexington, KY, May 2017.

12. Smith, I. A., “The Design of Fly Ash Concrete,” Paper 6982, Proceedings of Institute of Civil Engineers, London, UK, V. 36, Apr. 1967, pp. 767-789.

13. Dalziel, J. A., and Gutteridge, W. A., “The Influence of Pulverized Fuel Ash on the Hydration Characteristics and Physical Properties of Portland Cement Pastes,” Technical Report 560, Cement and Concrete Association, 1986, 28 pp.

14. von Fay, K. F., “Effects of Various Fly Ashes on Compressive Strength, Resistance to Freezing and Thawing, Resistance to Sulfate Attack, and Adiabatic Temperature Rise of Concrete,” Report No. R-95-02, Bureau of Reclamation, Denver, CO, Feb. 1959.

15. Drahusnak-Crow, R., “Freeze-thaw Durability of Fly Ash Concrete,” Proceedings: Eighth International Ash Utilization Symposium, American Coal Ash Association, Washington, DC, 1987.

16. von Fay, K. F., and Pierce, J. S., “Sulfate Resistance of Concretes with Various Fly Ashes,” ASTM Standardization News, V. 17, No. 12, Dec. 1989, pp. 32-37.

17. Mills, R. H., “Factors Influencing Cessation of Hydration of Water Cured Cement Pastes,” Special Report 90, Symposium on Structure of Portland Cement Pastes and Concretes, Highway Research Board, National Academy of Sciences, Washington DC, 1966, pp. 187-195.

18. Shashiprakash, S. G., and Thomas, M. D. A., 2001, “Sulfate Resistance of Mortars Containing High-Calcium Fly Ashes and Combinations of Highly Reactive Pozzolans and Fly Ash,” Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete, Proceedings of the Seventh CANMET/ACI International Conference, SP-199, V. 1, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI., pp. 221-237.

19. Shehata, M. H., and Thomas, M. D. A., “The Effect of Fly Ash Composition on the Expansion of Concrete Due to Alkali Silica Reaction,” Cement and Concrete Research, V. 30, No. 7, 2000, pp. 1063-1072. doi: 10.1016/S0008-8846(00)00283-0

20. Massaza, F., “Pozzolana and Pozzolanic Cements,” Lea’s Chemistry of Cement and Concrete, fourth edition, P. Hewlett, ed., John Wiley and Sons, Inc., New York, 489 pp.


ALSO AVAILABLE IN: