Effect of Calcium Formate on Hydration Mechanism of Cement Fly Ash Blends

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Calcium Formate on Hydration Mechanism of Cement Fly Ash Blends

Author(s): T. Hemalatha, Karunanithi Arthi, and Maitri Mapa

Publication: Materials Journal

Volume: 116

Issue: 4

Appears on pages(s): 51-59

Keywords: calcium formate; degree of hydration; fly ash; heat of hydration

DOI: 10.14359/51716680

Date: 7/1/2019

Abstract:
The evolution of properties of cement fly ash blends are greatly influenced by the degree of hydration of both fly ash and cement. Due to the complexity in the reaction mechanism of fly ash in cement, despite the broad-based research carried out in the past few decades, hydration mechanisms of cement fly ash is not well established yet. Nowadays, the third ingredient such as calcium formate, calcium chloride, and calcium carbonate are added to cement fly ash blends to eliminate the well-known drawbacks of reduced early-age strength and delayed setting time of fly ash, that makes the hydration mechanism even more complex. This study attempts to investigate the influence of incorporation of calcium formate on hydration mechanism of cement fly ash blends at various replacement levels at both early and later ages. Study shows that the incorporation of calcium formate improved the strength of cement fly ash blends at early ages.

Related References:

1. Tkaczewska, E., and Malolepszy, J., “Hydration of Coal Biomass Fly Ash Cement,” Construction and Building Materials, V. 23, No. 7, 2009, pp. 2694-2700. doi: 10.1016/j.conbuildmat.2008.12.018

2. Pacewska, B.; Blonkowski, G.; and Wilinska, I., “Investigations of the Influence of Different Fly Ashes on Cement Hydration,” Journal of Thermal Analysis and Calorimetry, V. 86, No. 1, 2006, pp. 179-186. doi: 10.1007/s10673-005-7136-7

3. Wong, H., and Buenfeld, N., “Determining the Water Cement Ratio, Cement Content, Water Content and Degree of Hydration of Hardened Cement Paste: Method Development and Validation on Paste Samples,” Cement and Concrete Research, V. 39, No. 10, 2009, pp. 957-965. doi: 10.1016/j.cemconres.2009.06.013

4. Yu, Z., and Ye, G., “The Pore Structure of Cement Paste Blended with Fly Ash,” Construction and Building Materials, V. 45, 2013, pp. 30-35. doi: 10.1016/j.conbuildmat.2013.04.012

5. Rahhal, V.; Bonavetti, V.; Trusilewicz, L.; Pedrajas, C.; and Talero, R., “Role of the Filler on Portland Cement Hydration at Early Ages,” Construction and Building Materials, V. 27, No. 1, 2012, pp. 82-90. doi: 10.1016/j.conbuildmat.2011.07.021

6. Lam, L.; Wong, Y.; and Poon, C., “Degree of Hydration and Gel/Space Ratio of High-Volume Fly Ash/Cement Systems,” Cement and Concrete Research, V. 30, No. 5, 2000, pp. 747-756. doi: 10.1016/S0008-8846(00)00213-1

7. Hemalatha, T.; Mapa, M.; George, N.; and Sasmal, S., “Physico-Chemical and Mechanical Characterization of High Volume Fly Ash Incorporated and Engineered Cement System Towards Developing Greener Cement,” Journal of Cleaner Production, V. 125, 2016, pp. 268-281. doi: 10.1016/j.jclepro.2016.03.118

8. Thongsanitgarn, P.; Wongkeo, W.; Chaipanich, A.; and Poon, C. S., “Heat of Hydration of Portland High-Calcium Fly Ash Cement Incorporating Limestone Powder: Effect of Limestone Particle Size,” Construction and Building Materials, V. 66, 2014, pp. 410-417. doi: 10.1016/j.conbuildmat.2014.05.060

9. Heikal, M., “Effect of Calcium Formate as an Accelerator on the Physico-Chemical and Mechanical Properties of Pozzolanic Cement Pastes,” Cement and Concrete Research, V. 34, No. 6, 2004, pp. 1051-1056. doi: 10.1016/j.cemconres.2003.11.015

10. Justnes, H., and Nygaard, E. C., “Technical Calcium Nitrate as Set Accelerator for Cement at Low Temperatures,” Cement and Concrete Research, V. 25, No. 8, 1995, pp. 1766-1774. doi: 10.1016/0008-8846(95)00172-7

11. Hill, R., and Daugherty, K., “The Interaction of Calcium Nitrate and a Class C Fly Ash During Hydration,” Cement and Concrete Research, V. 26, No. 7, 1996, pp. 1131-1143. doi: 10.1016/0008-8846(96)00074-9

12. Dodson, V., Concrete Admixtures, Van Nostrand Reinhold, New York, 1990, pp. 73-102.

13. Renichi, K.; Masaki, D.; Etsuro, S.; and Hirotaka, U., “Influence of Inorganic Salts on the Hydration of Tricalcium Silicate,” Journal of Applied Chemistry & Biotechnology, V. 27, 1977, pp. 191-197.

14. Ramachandran, V. S., “Investigation of the Role of Chemical Admixture in Concrete, a Differential Thermal Approach,” 7th International Conference on Thermal Analysis, 1982, pp. 1296-1302.

15. Bensted, J., “Early Strength Behavior of Portland Cement in Water, Calcium Chloride and Calcium Formate,” Silic. Ind., V. 45, 1980, pp. 67-69.

16. Malhotra, V. M., “Durability of Concrete Incorporating High-Volume of Low Calcium (ASTM Class F) Fly Ash,” Cement and Concrete Composites, V. 12, No. 4, 1990, pp. 271-277. doi: 10.1016/0958-9465(90)90006-J

17. Shaikh, F., and Supit, S., “Mechanical and Durability Properties of High Volume Fly Ash (HVFA) Concrete Containing Calcium Carbonate (CaCO3) Nanoparticles,” Construction and Building Materials, V. 70, 2014, pp. 309-321. doi: 10.1016/j.conbuildmat.2014.07.099

18. De la Varga, I.; Castro, J.; Bentz, D.; and Weiss, J., “Application of Internal Curing for Mixtures Containing High Volumes of Fly Ash,” Cement and Concrete Composites, V. 34, No. 9, 2012, pp. 1001-1008. doi: 10.1016/j.cemconcomp.2012.06.008

19. Zhao, L.; Guo, X.; Liu, Y.; Ge, C.; Guo, L.; Shu, X.; and Liu, J., “Synergistic Effects of Silica Nanoparticles/Polycarboxylate Superplasticizer Modified Graphene Oxide on Mechanical Behavior and Hydration Process of Cement Composites,” RSC Advances, V. 7, No. 27, 2017, pp. 16688-16702. doi: 10.1039/C7RA01716B

20. De Schutter, G., and Taerwe, L., “General Hydration Model for Portland Cement and Blast Furnace Slag Cement,” Cement and Concrete Research, V. 25, No. 3, 1995, pp. 593-604. doi: 10.1016/0008-8846(95)00048-H

21. Wu, X.; Roy, D. M.; and Langton, C. A., “Early Stage Hydration of Slag Cement,” Cement and Concrete Research, V. 13, No. 2, 1983, pp. 277-286. doi: 10.1016/0008-8846(83)90111-4

22. Deschner, F.; Winnefeld, F.; Lothenbach, B.; Seufert, S.; Schwesig, P.; Dittrich, S.; Goetz-Neunhoeffer, F.; and Neubauer, J., “Hydration of Portland Cement with High Replacement by Siliceous Fly Ash,” Cement and Concrete Research, V. 42, No. 10, 2012, pp. 1389-1400. doi: 10.1016/j.cemconres.2012.06.009

23. Poon, C.; Qiao, X.; and Lin, Z., “Pozzolanic Properties of Reject Fly Ash in Blended Cement Pastes,” Cement and Concrete Research, V. 33, No. 11, 2003, pp. 1857-1865. doi: 10.1016/S0008-8846(03)00213-8

24. Li, S.; Roy, D. M.; and Kumar, A., “Quantitative Determination of Pozzolanas in Hydrated Systems of Cement or Ca(OH)2 with Fly Ash or Silica Fume,” Cement and Concrete Research, V. 15, No. 6, 1985, pp. 1079-1086. doi: 10.1016/0008-8846(85)90100-0

25. Gaviria, X.; Borrachero, M. V.; Payá, J.; Monzó, J. M.; and Tobón, J. I., “Mineralogical Evolution of Cement Pastes at Early Ages Based on Thermo Gravimetric Analysis (TG),” Journal of Thermal Analysis and Calorimetry, V. 132, No. 1, 2018, pp. 39-46. doi: 10.1007/s10973-017-6905-0

26. Hemalatha, T., and Sasmal, S., “Early-Age Strength Development in Fly Ash Blended Cement Composites: Investigation Through Chemical Activation,” Magazine of Concrete Research, V. 71, No. 5, 2019, pp. 260-270. doi: 10.1680/jmacr.17.00336

27. Ramachandran, V. S., Concrete Admixtures Handbook. Properties, Science and Technology, Chapter 3, second edition, Noyes Publications, USA, 1995, pp 96-102.

28. Singh, N. B., and Abha, K., “Effect of Calcium Formate on the Hydration of Tricalcium Silicate,” Cement and Concrete Research, V. 13, No. 5, 1983, pp. 619-625. doi: 10.1016/0008-8846(83)90050-9

29. Levitt, M., Precast Concrete, Applied Science Publishers, London, 1982.

30. Gebler, S., “Evaluation of Calcium Formate and Sodium Formate as Accelerating Admixtures for Portland Cement Concrete,” ACI Journal Proceedings, V. 80, No. 5, Sept. 1983, pp. 439-444.


ALSO AVAILABLE IN:

Electronic Materials Journal