Numerical Analysis of Behavior of Glass Fiber-Reinforced Polymer Bar-Reinforced Concrete Beams under Impact Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical Analysis of Behavior of Glass Fiber-Reinforced Polymer Bar-Reinforced Concrete Beams under Impact Loads

Author(s): Zein Saleh, M. Neaz Sheikh, Alex Remennikov, and Abheek Basu

Publication: Structural Journal

Volume: 116

Issue: 5

Appears on pages(s): 151-160

Keywords: beam; glass fiber-reinforced polymer (GFRP); impact; modeling; reinforced concrete

DOI: 10.14359/51715658

Date: 9/1/2019

Abstract:
This paper numerically investigates the behavior of glass fiber-reinforced polymer (GFRP) bar-reinforced concrete beams (GFRP-RC beams) under low-velocity impact loads. A finite element model has been developed and calibrated against the experimental investigation results of six GFRP-RC beams. The results of the numerical analysis have been found in very good agreement with the experimental investigation results. The finite element model captured the failure modes, crack profiles, midspan deflection, impact and reaction forces, and dynamic strain of the GFRP-RC beams. Moreover, a parametric study has been carried out to investigate the influence of the reinforcement ratio, compressive strength of concrete, drop mass, drop velocity, and impact energy on the response of GFRP-RC beams under low-velocity impact loads. It was found that the drop mass and velocity significantly influenced the damage profiles of the beams, and the reinforcement ratio significantly influenced the midspan deflection and reactions at the support.

Related References:

1. Alsayed, S.; Al-Salloum, Y.; and Almusallam, T., “Performance of Glass Fiber Reinforced Plastic Bars as a Reinforcing Material for Concrete Structures,” Composites. Part B, Engineering, V. 31, No. 6-7, 2000, pp. 555-567. doi: 10.1016/S1359-8368(99)00049-9

2. Toutanji, H. A., and Saafi, M., “Flexural Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars,” ACI Structural Journal, V. 97, No. 5, Sept.-Oct. 2000, pp. 712-719.

3. Ashour, A., “Flexural and Shear Capacities of Concrete Beams Reinforced with GFRP Bars,” Construction and Building Materials, V. 20, No. 10, 2006, pp. 1005-1015. doi: 10.1016/j.conbuildmat.2005.06.023

4. El-Mogy, M.; El-Ragaby, A.; and El-Salakawy, E., “Effect of Transverse Reinforcement on the Flexural Behavior of Continuous Concrete Beams Reinforced with FRP,” Journal of Composites for Construction, ASCE, V. 15, No. 5, 2011, pp. 672-681. doi: 10.1061/(ASCE)CC.1943-5614.0000215

5. Kishi, N.; Mikami, H.; Matsuoka, K.; and Ando, T., “Impact Behavior of Shear-Failure-Type RC Beams Without Shear Rebar,” International Journal of Impact Engineering, V. 27, No. 9, 2002, pp. 955-968. doi: 10.1016/S0734-743X(01)00149-X

6. Fujikake, K.; Li, B.; and Soeun, S., “Impact Response of Reinforced Concrete Beam and Its Analytical Evaluation,” Journal of Structural Engineering, ASCE, V. 135, No. 8, 2009, pp. 938-950. doi: 10.1061/(ASCE)ST.1943-541X.0000039

7. Saatci, S., and Vecchio, F. J., “Effects of Shear Mechanisms on Impact Behavior of Reinforced Concrete Beams,” ACI Structural Journal, V. 106, No. 1, Jan.-Feb. 2009, pp. 78-86.

8. Kishi, N., and Mikami, H., “Empirical Formulas for Designing Reinforced Concrete Beams under Impact Loading,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 509-519.

9. Somraj, A.; Fujikake, K.; and Li, B., “Influence of Loading Rate on Shear Capacity of Reinforced Concrete Beams,” International Journal of Protective Structures, V. 4, No. 4, 2013, pp. 521-543. doi: 10.1260/2041-4196.4.4.521

10. Adhikary, S. D.; Li, B.; and Fujikake, K., “Effects of High Loading Rate on Reinforced Concrete Beams,” ACI Structural Journal, V. 111, No. 3, May-June 2014, pp. 651-660.

11. Goldston, M.; Remennikov, A.; and Sheikh, M. N., “Experimental Investigation of the Behaviour of Concrete Beams Reinforced with GFRP Bars under Static and Impact Loading,” Engineering Structures, V. 113, 2016, pp. 220-232. doi: 10.1016/j.engstruct.2016.01.044

12. Goldston, M.; Remennikov, A.; and Sheikh, M. N., “Flexural Behaviour of GFRP Reinforced High Strength and Ultra High Strength Concrete Beams,” Construction and Building Materials, V. 131, 2017, pp. 606-617. doi: 10.1016/j.conbuildmat.2016.11.094

13. Daudeville, L., and Malécot, Y., “Concrete Structures under Impact,” European Journal of Environmental and Civil Engineering, V. 15, No. sup1, 2011, pp. 101-140.

14. Kishi, N.; Khasraghy, S. G.; and Kon-No, H., “Numerical Simulation of Reinforced Concrete Beams under Consecutive Impact Loading,” ACI Structural Journal, V. 108, No. 4, July-Aug. 2011, pp. 444-452.

15. Ožbolt, J., and Sharma, A., “Numerical Simulation of Reinforced Concrete Beams with Different Shear Reinforcements under Dynamic Impact Loads,” International Journal of Impact Engineering, V. 38, No. 12, 2011, pp. 940-950. doi: 10.1016/j.ijimpeng.2011.08.003

16. Adhikary, S. D.; Li, B.; and Fujikake, K., “Low Velocity Impact Response of Reinforced Concrete Beams: Experimental and Numerical Investigation,” International Journal of Protective Structures, V. 6, No. 1, 2015, pp. 81-111. doi: 10.1260/2041-4196.6.1.81

17. Adhikary, S. D.; Li, B.; and Fujikake, K., “Residual Resistance of Impact-Damaged Reinforced Concrete Beams,” Magazine of Concrete Research, V. 67, No. 7, 2015, pp. 364-378. doi: 10.1680/macr.14.00312

18. Zhao, D.-B.; Yi, W.-J.; and Kunnath, S. K., “Shear Mechanisms in Reinforced Concrete Beams under Impact Loading,” Journal of Structural Engineering, ASCE, V. 143, No. 9, 2017, p. 1362-1370. doi: 10.1061/(ASCE)ST.1943-541X.0001818

19. Hallquist, J. O., “LS-DYNA Keyword User’s Manual,” Livermore Software Technology Corporation, Livermore, CA, 2017.

20. Hallquist, J. O., “LS-DYNA Theory Manual,” Livermore Software Technology Corporation, Livermore, CA, 2017.

21. Adhikary, S. D.; Li, B.; and Fujikake, K., “Parametric Study of RC Beams under a Wide Range of Loading Rates,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 168, No. 10, 2015, pp. 729-746. doi: 10.1680/jstbu.15.00024

22. Jiang, H., and Zhao, J., “Calibration of the Continuous Surface Cap Model for Concrete,” Finite Elements in Analysis and Design, V. 97, 2015, pp. 1-19. doi: 10.1016/j.finel.2014.12.002

23. Guo, J.; Cai, J.; and Chen, W., “Inertial Effect on RC Beam Subjected to Impact Loads,” International Journal of Structural Stability and Dynamics, V. 17, No. 04, 2017, p. 1750053 doi: 10.1142/S0219455417500535

24. Liao, W.; Li, M.; Zhang, W.; and Tian, Z., “Experimental Studies and Numerical Simulation of Behavior of RC Beams Retrofitted with HSSWM-HPM under Impact Loading,” Engineering Structures, V. 149, 2017, pp. 131-146. doi: 10.1016/j.engstruct.2016.07.040

25. Jiang, H., and Chorzepa, M. G., “An Effective Numerical Simulation Methodology to Predict the Impact Response of Prestressed Concrete Members,” Engineering Failure Analysis, V. 55, 2015, pp. 63-78. doi: 10.1016/j.engfailanal.2015.05.006

26. Bhatti, A. Q.; Kishi, N.; Mikami, H.; and Ando, T., “Elasto-Plastic Impact Response Analysis of Shear-Failure-Type RC Beams with Shear Rebars,” Materials & Design, V. 30, No. 3, 2009, pp. 502-510. doi: 10.1016/j.matdes.2008.05.068

27. Jiang, H.; Wang, X.; and He, S., “Numerical Simulation of Impact Tests on Reinforced Concrete Beams,” Materials & Design, V. 39, 2012, pp. 111-120. doi: 10.1016/j.matdes.2012.02.018

28. Pham, A. T.; Tan, K. H.; and Yu, J., “Numerical Investigations on Static and Dynamic Responses of Reinforced Concrete Sub-Assemblages under Progressive Collapse,” Engineering Structures, V. 149, 2017, pp.  2-20. doi: 10.1016/j.engstruct.2016.07.042

29. Shi, Y.; Li, Z.-X.; and Hao, H., “Bond Slip Modelling and Its Effect on Numerical Analysis of Blast-Induced Responses of RC Columns,” Structural Engineering and Mechanics, V. 32, No. 2, 2009, pp. 251-267. doi: 10.12989/sem.2009.32.2.251

30. Xu, S.; Wu, C.; Liu, Z.; and Li, J., “Numerical Study of Ultra-High-Performance Steel Fibre-Reinforced Concrete Columns under Monotonic Push Loading,” Advances in Structural Engineering, V. 21, No. 8, 2018, pp. 1234-1248. doi: 10.1177/1369433217747710

31. Bao, Y.; Lew, H. S.; and Kunnath, S. K., “Modeling of Reinforced Concrete Assemblies under Column-Removal Scenario,” Journal of Structural Engineering, ASCE, V. 140, No. 1, 2014, p. 04013026 doi: 10.1061/(ASCE)ST.1943-541X.0000773

32. Broadhouse, B., and Neilson, A., “Modelling Reinforced Concrete Structures in Dyna3d,” Book Modelling Reinforced Concrete Structures in Dyna3d, UKAEA Atomic Energy Establishment, 1987.

33. Broadhouse, B., “The Winfrith Concrete Model in LS-DYNA3D,” Report: SPD/D (95), V. 363, 1995.

34. Abu-Odeh, A., “Modeling and Simulation of Bogie Impacts on Concrete Bridge Rails Using LS-DYNA®,” 2008, pp. 8-10.

35. Schwer, L., Modeling Rebar: The Forgotten Sister in Reinforced Concrete Modeling, 2014, 28 pp.

36. Algaard, W.; Lyle, J.; and Izatt, C., Perforation of Composite Floors, 2005, pp. 1123-1130.

37. Wu, Y.; Crawford, J. E.; and Magallanes, J. M., “Performance of LS-DYNA Concrete Constitutive Models,” 12th International LS-DYNA Users Conference, 2012, pp. 3-5.

38. Thai, D.-K., and Kim, S.-E., “Failure Analysis of Reinforced Concrete Walls under Impact Loading Using the Finite Element Approach,” Engineering Failure Analysis, V. 45, 2014, pp. 252-277. doi: 10.1016/j.engfailanal.2014.06.006

39. Thiagarajan, G.; Kadambi, A. V.; Robert, S.; and Johnson, C. F., “Experimental and Finite Element Analysis of Doubly Reinforced Concrete Slabs Subjected to Blast Loads,” International Journal of Impact Engineering, V. 75, 2015, pp. 162-173. doi: 10.1016/j.ijimpeng.2014.07.018

40. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

41. RILEM, “RILEM Technical Recommendations for the Testing and Use of Construction Materials,” E & FN Spon, London, UK, 1994.

42. Yan, F.; Lin, Z.; and Yang, M., “Bond Mechanism and Bond Strength of GFRP Bars to Concrete: A Review,” Composites. Part B, Engineering, V. 98, 2016, pp. 56-69. doi: 10.1016/j.compositesb.2016.04.068

43. CSA S806:2012:R2017, “Design and Construction of Building Structures with Fibre-Reinforced Polymers,” Canadian Standards Association, Toronto, ON, Canada, 2012.

44. Adhikary, S. D.; Li, B.; and Fujikake, K., “Dynamic Behavior of Reinforced Concrete Beams under Varying Rates of Concentrated Loading,” International Journal of Impact Engineering, V. 47, Sept, 2012, pp. 24-38. doi: 10.1016/j.ijimpeng.2012.02.001

45. Achillides, Z., and Pilakoutas, K., “Bond Behavior of Fiber Reinforced Polymer Bars under Direct Pullout Conditions,” Journal of Composites for Construction, ASCE, V. 8, No. 2, 2004, pp. 173-181. doi: 10.1061/(ASCE)1090-0268(2004)8:2(173)

46. Okelo, R., and Yuan, R. L., “Bond Strength of Fiber Reinforced Polymer Rebars in Normal Strength Concrete,” Journal of Composites for Construction, ASCE, V. 9, No. 3, 2005, pp. 203-213. doi: 10.1061/(ASCE)1090-0268(2005)9:3(203)


ALSO AVAILABLE IN:

Electronic Structural Journal