2019 Decorative Concrete Award Winners

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 2019 Decorative Concrete Award Winners

Author(s):

Publication: Concrete International

Volume: 41

Issue: 3

Appears on pages(s): 24-26

Keywords: cast-in-place, polished, stained, overlay

DOI: 10.14359/51715607

Date: 3/1/2019

Abstract:
The Decorative Concrete Council, a specialty council of the American Society of Concrete Contractors, St. Louis, MO, announced the winners of its 11th annual Decorative Concrete Awards competition. Sawmill Lakes Recreation Center Splashpad in Sienna Plantation, Missouri City, TX, won the WOW! Award for the best overall project. The design included 14 custom colors, 400 stars, six constellations, three template trees, a four-color grassy area, and a four-color template moon.