Abstract:
Glass fiber reinforced polymer (GFRP) bars are emerging as a feasible, economical solution to eliminate the corrosion problem of steel reinforcements in concrete structures. Confirmation of GFRP long-term durability is crucial to extend its application especially in structures exposed to aggressive environments. The objective of this study is to investigate the performance of GFRP bars exposed to the concrete alkalinity and ambient condition in two bridges with more than a decade old located in the City of Rolla, Missouri: i) Walker Bridge (built in 1999), which consists of GFRP-reinforced concrete box culverts; and; ii) Southview Bridge (built in 2004), which incorporates GFRP bars in the post-tensioned concrete deck. In order to monitor the possible changes in GFRP and concrete after years of service, samples were extracted from both bridges for various analyses. Carbonation depth, chloride diffusion, and pH of the concrete surrounding the GFRP bars were measured. Scanning electron microscopy (SEM) imaging and energy dispersive X-ray spectroscopy (EDS) were performed to monitor any microstructural degradation or change in the GFRP chemical compositions. Finally, GFRP horizontal shear strength, glass transition temperature (Tg) and fiber content were determined and compared with the results of similar tests performed on pristine samples produced in 2015. SEM and EDS did not show any sign of GFRP microstructural deterioration or existence of a chemical attack. Horizontal shear strength and Tg showed slight improvements while the fiber content was similar to the pristine values. The results of this study suggest that GFRP bars maintained their microstructural integrity and mechanical properties during years of service as concrete reinforcement in both bridges.
Related References:
1. Nanni, A., De Luca, A., Jawaheri Zadeh, H. "Reinforced Concrete with FRP Bars: Mechanics and Design," CRC Press, 2014.
2. Mufti, A., Banthia, N., Benmokrane, B., Boulfiza, M., Newhook, J., "Durability of GFRP Composite Rods," Concrete International, V. 29, 2007, pp. 37-42.
3. Gooranorimi, O., Nanni, A., “GFRP Reinforcement in Concrete After 15 Years of Service,”, Journal of Composites for Construction, V. 21, No. 5, 2017.
4. Alkhrdaji, T., Nanni, A., “Construction and Long-Term Monitoring of a Concrete Box Culvert Bridge Reinforced with GFRP Bars,” Center for Infrastructure Engineering Studies, Technical Report: #RDT01-016, 2001.
5. Holdener, D., Myers, J., Nanni, A., “An Overview of Composites Usage in Bridge Facilities in The State of Missouri, USA,” Proceedings of the International Conference and Exhibition on Reinforced Plastics, ICERP, Mumbai, India, 2008.
6. Fico, R., Galati, N., Prota, A., Nanni, A., “Southview Bridge Rehabilitation in Rolla, MO – Volume I: Design and Construction,” University Transportation Center Program at the University of Missouri-Rolla, Report # URC R103, 2006
7. Grubb, J., Limaye, H., Kakade, A., "Testing pH of Concrete: Need for A Standard Procedure," Concrete International, V. 29, 2007, pp. 78-83.
8. CPC-18 (RILEM Recommendations), "Measurement of Hardened Concrete Carbonation Depth," V. 21, 1988, pp. 453- 455.
9. Otsuki, N., Nagataki, S., Nakashita, K., “Evaluation of AgNO3 Solution Spray Method for Measurement of Chloride Penetration into Hardened Cementitious Matrix Materials,? ACI Material Journal, V. 89, 1992, pp. 587-592.
10. Gooranorimi, O., Suaris, W., Dauer, E., Nanni, A., “Microstructural Investigation of Glass Fiber Reinforced Polymer Bars,”, Journal of Composites Part B: Engineering, V. 110, 2017, pp. 388-395.
11. ASTM (ASTM International) D4475, "Standard Test Method for Apparent Horizontal Shear Strength of Pultruded Reinforced Plastic Rods by the Short-Beam Method," West Conshohocken, PA, 2008.
12. ASTM (ASTM International) E1640, "Standard Test Method for Assignment of the Glass Transition Temperature by Dynamic Mechanical Analysis," West Conshohocken, PA, 2013.
13. Stutz, H., K. H. Illers, J. Mertez., “A Generalized Theory for the Glass Transition Temperature of Crosslinked and Uncrosslinked Polymers,” Journal of Polymer Science Part B: Polymer Physics, V. 28, No. 9, 1990, pp. 1483-1498.
14. ASTM (ASTM International) D2584, "Standard Test Method for Ignition Loss of Cured Reinforced Resins," West Conshohocken, PA, 2011.
15. ICC (International Code Council-Evaluation Service) AC-454, “Acceptance Criteria for Fibre-Reinforced Polymers (FRP) Bars for Internal Reinforcement of Concrete Members,” 2015.