439.6R-19: Guide for the Use of ASTM A1035/A1035M Type CS Grade 100 (690) Steel Bars for Structural Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 439.6R-19: Guide for the Use of ASTM A1035/A1035M Type CS Grade 100 (690) Steel Bars for Structural Concrete

Author(s): ACI Committee 439

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 100

Keywords: bar; design; guide; high-strength steel; structural

DOI:

Date: 2/4/2019

Abstract:

This guide provides recommendations on design provisions for the use of ASTM A1035/ASTM A1035M Type CS Grade 100 (690) deformed steel bars for reinforced concrete members. The recommendations address only those requirements of ACI 318-14 that limit efficient use of such steel bars. Other code requirements are not affected. Any other ACI 318 versions will be explicitly specified.

Although there are limiting ACI 318 requirements, ACI 318-14 Section 1.10 would allow the use of high-strength reinforcement. “Sponsors...shall have the right to present the data on which their design is based to the building official or to a board of examiners appointed by the building official.”

The International Building Code (IBC 2012) would allow the same under Section 104.11, “Alternative materials, design and methods of construction and equipment”. To approve an alternative material under this section, a building department would typically require an ICC Evaluation Service (ICC-ES) Evaluation Report, which would be based on an ICC-ES Acceptance Criteria (AC) document. An AC document (ICC-ES AC429) and an Evaluation Report (ICC-ES ESR-2107) exist, permitting the use of ASTM A1035/A1035M Grade 100 reinforcement.

This guide includes a discussion of the material characteristics of Grade 100 (690) ASTM A1035/A1035M (CS) deformed steel bars and recommends design criteria for beams, columns, slab, systems, walls, and footings for Seismic Design Category (SDC) A, B, or C, and for structural components not designated as part of the seismic-force-resisting system for SDC D, E, or F.

A structure assigned to SDC A, B, or C is required to be designed for all applicable gravity and environmental loads. In the case of SDC A structures, seismic forces are notional structural integrity forces. This guide addresses all design required for SDC A, B, and C structures.

Because the modulus of elasticity for ASTM A1035/A1035M (CS) is similar to that of carbon steel (ASTM A615/A615M) using higher specified minimum yield strength fy may result in higher steel stress at service load condition and potentially cause wider cracks and larger deflections, which may be objectionable if aesthetics and water-tightness are critical design requirements. Higher deflection can also contribute to serviceability issues. Also, with higher fy, the required development length will be longer.