Shake-Table Tests and Numerical Analysis of Self-Centering Prestressed Concrete Frame

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shake-Table Tests and Numerical Analysis of Self-Centering Prestressed Concrete Frame

Author(s): Tong Guo, Yaowen Hao, Lianglong Song, and Zhiliang Cao

Publication: Structural Journal

Volume: 116

Issue: 3

Appears on pages(s): 3-17

Keywords: concrete frame; numerical simulation; post-tensioning; seismic performance; self-centering; shake-table test

DOI: 10.14359/51714472

Date: 5/1/2019

Abstract:
This paper presents the shake-table tests and numerical analysis of a self-centering prestressed concrete (SCPC) frame to evaluate its seismic performance. The SCPC frame uses unbonded post-tensioned (PT) beam-column and column-foundation connections to provide the re-centering capability. Web friction devices are used at the beam ends to provide the adjustable energy dissipation capacity. A 0.5-scale, one-by-two bay, two-story specimen frame was designed and tested on a shake table under various ground motions with increasing intensities. The test results indicate that the SCPC frame had satisfactory seismic performance, and a desirable re-centering capability was observed with little structural damage even under severe earthquakes. An analytical model of the SCPC frame was also developed using the Open System for Earthquake Engineering Simulation (OpenSees) to replicate the test results. Good correlation is observed between the analytical and test results, indicating that the proposed model can be used to study the behavior of such self-centering (SC) structures.

Related References:

1. Miranda, E., “Enhanced Building-Specific Seismic Performance Assessment,” Advances in Performance-Based Earthquake Engineering, Springer, the Netherlands, 2010, pp. 183-191.

2. Ricles, J. M.; Sause, R.; Garlock, M. M.; and Zhao, C., “Posttensioned Seismic-Resistant Connections for Steel Frames,” Journal of Structural Engineering, ASCE, V. 127, No. 2, 2001, pp. 113-121. doi: 10.1061/(ASCE)0733-9445(2001)127:2(113)

3. Priestley, M. J. N., , “Overview of PRESSS Research Program,” PCI Journal, V. 36, No. 4, 1991, pp. 50-57. doi: 10.15554/pcij.07011991.50.57

4. Stone, W. C.; Cheok, G. S.; and Stanton, J. F., “Performance of Hybrid Moment-Resisting Precast Beam-Column Concrete Connections Subjected to Cyclic Loading,” ACI Structural Journal, V. 92, No. 2, Mar.-Apr. 1995, pp. 229-249.

5. Bradley, B. A.; Dhakal, R. P.; Mander, J. B.; and Li, L., “Experimental Multi-Level Seismic Performance Assessment of 3D RC Frame Designed for Damage Avoidance,” Earthquake Engineering & Structural Dynamics, V. 37, No. 1, 2008, pp. 1-20. doi: 10.1002/eqe.741

6. Li, L.; Mander, J. B.; and Dhakal, R. P., “Bidirectional Cyclic Loading Experiment on a 3D Beam-Column Joint Designed for Damage Avoidance,” Journal of Structural Engineering, ASCE, V. 134, No. 11, 2008, pp. 1733-1742. doi: 10.1061/(ASCE)0733-9445(2008)134:11(1733)

7. Rodgers, G. W.; Solberg, K. M.; Mander, J. B.; Chase, J. G.; Bradley, B. A.; and Dhakal, R. P., “High-Force-to-Volume Seismic Dissipators Embedded in a Jointed Precast Concrete Frame,” Journal of Structural Engineering, ASCE, V. 138, No. 3, 2010, pp. 375-386. doi: 10.1061/(ASCE)ST.1943-541X.0000329

8. Morgen, G. B., and Kurama, K. M., “A Friction Damper for Posttensioned Precast Concrete Moment Frames,” PCI Journal, V. 49, No. 4, 2004, pp. 112-133. doi: 10.15554/pcij.07012004.112.133

9. Priestley, M. J. N.; Sritharan, S.; Conley, J. R.; and Pampanin, S., “Preliminary Results and Conclusions from the PRESSS Five-Story Precast Concrete Test Building,” PCI Journal, V. 44, No. 6, 1999, pp. 42-67. doi: 10.15554/pcij.11011999.42.67

10. Lu, X.; Cui, Y.; Liu, J.; and Gao, W., “Shaking Table Test and Numerical Simulation of a 1/2-Scale Self-centering Reinforced Concrete Frame,” Earthquake Engineering & Structural Dynamics, V. 44, No. 12, 2015, pp. 1899-1917. doi: 10.1002/eqe.2560

11. Cui, Y.; Lu, X.; and Jiang, C., “Experimental Investigation of Tri-Axial Self-centering Reinforced Concrete Frame Structures through Shaking Table Tests,” Engineering Structures, V. 132, 2017, pp. 684-694. doi: 10.1016/j.engstruct.2016.11.066

12. Guo, T.; Song, L. L.; Zhang, G. D.; and Gu, Y., “Experimental Study on Beam-Column Connections of Self-centering Prestressed Concrete Frame with Web Friction Device,” Tumu Gongcheng Xuebao, V. 45, No. 6, 2012, pp. 23-32. (in Chinese)

13. Song, L. L.; Guo, T.; and Chen, C., “Experimental and Numerical Study of a Self-centering Prestressed Concrete Moment Resisting Frame Connection with Bolted Web Friction Devices,” Earthquake Engineering & Structural Dynamics, V. 43, No. 4, 2014, pp. 529-545. doi: 10.1002/eqe.2358

14. Song, L. L.; Guo, T.; Gu, Y.; and Cao, Z.-L., “Experimental Study of a Self-centering Prestressed Concrete Frame Subassembly,” Engineering Structures, V. 88, 2015, pp. 176-188. doi: 10.1016/j.engstruct.2015.01.040

15. Guo, T.; Song, L. L.; Cao, Z. L.; and Gu, Y., “Large-scale Tests on Cyclic Behavior of Self-centering Prestressed Concrete Frames,” ACI Structural Journal, V. 113, No. 6, Nov.-Dec. 2016, pp. 1263-1274. doi: 10.14359/51689248

16. Ministry of Housing and Urban-Rural Development of the People’s Republic of China, “GB 50010-2010 Code for Design of Concrete Structures,” Architecture and Building Press, Beijing, China, 2010. (in Chinese)

17. Ministry of Housing and Urban-Rural Development of the People’s Republic of China, “GB 50011-2010 Code for Seismic Design of Buildings,” Architecture and Building Press, Beijing, China, 2010. (in Chinese)

18. Garlock, M. M.; Sause, R.; and Ricles, J. M., “Behavior and Design of Posttensioned Steel Frame Systems,” Journal of Structural Engineering, ASCE, V. 133, No. 3, 2007, pp. 389-399. doi: 10.1061/(ASCE)0733-9445(2007)133:3(389)

19. Guo, T., and Song, L. L., “Theoretical Analysis of Beam-Column Connections of Self-Centering Prestressed Concrete Frame with Web Friction Device,” Tumu Gongcheng Xuebao, V. 45, No. 7, 2012, pp. 73-79. (in Chinese)

20. Computer program SeismoArtif, v1.0.0., “SeismoArtif’s help system-© 2002-2012,” Seismosoft Ltd.

21. Kim, H. J., and Christopoulos, C., “Seismic Design Procedure and Seismic Response of Post-tensioned Self-centering Steel Frames,” Earthquake Engineering & Structural Dynamics, V. 38, No. 3, 2009, pp. 355-376. doi: 10.1002/eqe.859

22. Akcelyan, S.; Lignos, D. G.; Hikino, T.; and Nakashima, M., “Evaluation of Simplified and State-of-the-Art Analysis Procedures for Steel Frame Buildings Equipped with Supplemental Damping Devices Based on E-Defense Full-Scale Shake Table Tests,” Journal of Structural Engineering, ASCE, V. 142, No. 6, 2016, pp. 1-17. doi: 10.1061/(ASCE)ST.1943-541X.0001474

23. McKenna, F.; Fenves, G. L.; Scott, M. H.; and Jeremic, B., “Open System for Earthquake Engineering Simulation (OpenSees),” Pacific Earthquake Engineering Research Center, University of California, Berkeley, Berkeley, CA, 2013.

24. Guo, T.; Song, L. L.; and Zhang, G. D., “Numerical Simulation of the Seismic Behavior of Self-centering Steel Beam-Column Connections with Bottom Flange Friction Devices,” Earthquake Engineering and Engineering Vibration, V. 10, No. 2, 2011, pp. 229-238. doi: 10.1007/s11803-011-0061-5

25. El-Sheikh, M. T., “Seismic Analysis, Behavior, and Design of Unbonded Post-Tensioned Precast Moment Frames,” PhD dissertation, Lehigh University, Bethlehem, PA, 1999, pp. 339-363.

26. Morgen, B. G., and Kurama, Y. C., “Seismic Response Evaluation of Posttensioned Precast Concrete Frames with Friction Dampers,” Journal of Structural Engineering, ASCE, V. 134, No. 1, 2008, pp. 132-145. doi: 10.1061/(ASCE)0733-9445(2008)134:1(132)


ALSO AVAILABLE IN:

Electronic Structural Journal