Title: Evaluation of the 90-Minute Rule as an Acceptance Criteria

Author(s): Mohamed Mahgoub and Wayne Rawlins

Publication: Web Session

Volume: ws_F18_Mahgoub.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 12/14/2018

Abstract:
These co-speakers will present the research report “Evaluation of the 90-Minute Rule as an Acceptance Criteria” carried out by the Department of Engineering Technology at NJIT. • Actual field concrete batches were tested • A multitude of strength, durability, and shrinkage variables were evaluated • Hydration stabilizers were studied • Numerous concrete ages and temperatures were evaluated in this study