Effects of Mixture Proportioning, Curing, and Finishing on Concrete Surface Hardness

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Mixture Proportioning, Curing, and Finishing on Concrete Surface Hardness

Author(s): Kamran Amini, Seyedhamed Sadati, Halil Ceylan, and Peter C. Taylor

Publication: Materials Journal

Volume: 116

Issue: 2

Appears on pages(s): 119-126

Keywords: curing; finishing; salt scaling; slag cement; surface hardness

DOI: 10.14359/51714457

Date: 3/1/2019

Abstract:
With adoption of winter maintenance strategies that typically include incorporation of aggressive deicer chemicals, pavement surfaces in cold regions are exposed to the risk of scaling damage. Reduced ride quality due to surface deterioration can eventually lead into a variety of maintenance and repair programs. Such pavement preservation programs impose significant charges to the owner agencies, while raising concerns regarding the safety issues associated with work zone areas. The present study addresses the correlation between surface hardness and concrete hardened properties. Moreover, factors that influence the concrete performance with respect to surface-abrasion resistance (hardness) were investigated. Of special interest was the relationship between surface hardness and concrete salt-scaling performance. An extensive investigation was carried out to assess the effects of various mixture proportions, curing regimes, and finishing times on surface hardness of the concrete specimens. In addition, compressive strength, depth-sensing indentation (DSI), and salt scaling tests were used to evaluate the correlation between concrete surface hardness and performance. A scaling quality classification table using abrasion mass loss values was developed. The results reflect further understanding of the relationship between abrasion resistance and salt scaling resistance that can cause defects when more than two cycles of abrasion testing are applied.

Related References:

1. Carrasco-Maldonado, F.; Spörl, R.; Fleiger, K.; Hoenig, V.; Maier, J.; and Scheffknecht, G., “Oxy-Fuel Combustion Technology for Cement Production – State of the Art Research and Technology Development,” International Journal of Greenhouse Gas Control, V. 45, 2016, pp. 189-199. doi: 10.1016/j.ijggc.2015.12.014

2. Olivier, J. G. J.; Janssens-Maenhout, G.; Muntean, M.; and Peters, J. A., “Trends in Global CO2 Emissions: 2015 Report,” European Commission, Joint Research Centre, 2015, 80 pp.

3. Suraneni, P.; Monical, J.; Unal, E.; Farnam, Y.; and Weiss, J., “Calcium Oxychloride Formation Potential in Cementitious Pastes Exposed to Blends of Deicing Salt,” ACI Materials Journal, V. 114, No. 4, July-Aug. 2017, pp. 631-641. doi: 10.14359/51689607

4. Kosmatka, S., and Wilson, M., Design and Control of Concrete Mixtures: The Guide to Applications, Methods, and Materials, Portland Cement Association, Skokie, IL, 2011, 458 pp.

5. Sonebi, M., and Khayat, K., “Testing Abrasion Resistance of High-Strength Concrete,” Cement, Concrete and Aggregates, V. 23, No. 1, 2001, pp. 34-43. doi: 10.1520/CCA10523J

6. Glinicki, M., and Zielinski, M., “Frost Salt Scaling Resistance of Concrete Containing CFBC Fly Ash,” Materials and Structures, V. 42, No. 7, 2009, pp. 993-1002. doi: 10.1617/s11527-008-9438-y

7. Tremblay, M.-H.; Lory, F.; Marchand, J.; Scherer, G. W.; and Valenza, J. J., “Ability of the Glue Spall Model to Account for the Deicer Salt Scaling Deterioration of Concrete,” Proceedings, 12th International Congress on the Chemistry of Cement, Montreal, QC, Canada, 2007.

8. Amini, K.; Cetin, K.; Ceylan, H.; and Taylor, P., “Development of Prediction Models for Mechanical Properties and Durability of Concrete Using Combined Nondestructive Tests,” Journal of Materials in Civil Engineering, ASCE, V. 31, No. 2, 2019, p. 04018378. doi: 10.1061/(ASCE)MT.1943-5533.0002569

9. ACI Committee 233, “Slag Cement in Concrete and Mortar (ACI 233R-03) (Reapproved 2011),” American Concrete Institute, Farmington Hills, MI, 2003, 18 pp.

10. ASTM C31/C31M-10, “Standard Practice for Making and Curing Concrete Test Specimens in the Field,” ASTM International, West Conshohocken, PA, 2010, 6 pp.

11. BNQ NQ 2621-900, “Determination of the Scaling Resistance of Concrete Surfaces Exposed to Freezing-and-Thawing Cycles in the Presence of De-icing Chemicals,” Bureau de Normalisation du Québec, Québec, QC, Canada, 2002, pp. 19-22.

12. ASTM C944/C944M-12, “Standard Test Method for Abrasion Resistance of Concrete or Mortar Surfaces by the Rotating-Cutter Method,” ASTM International, West Conshohocken, PA, 2012, 5 pp.

13. Puertas, F.; Palacios, M.; Manzano, H.; Dolado, J. S.; Rico, A.; and Rodríguez, J., “A Model for the C-A-S-H Gel Formed in Alkali-Activated Slag Cements,” Journal of the European Ceramic Society, V. 31, No. 12, 2011, pp. 2043-2056. doi: 10.1016/j.jeurceramsoc.2011.04.036

14. Richardson, I. G.; Brough, A. R.; Groves, G. W.; and Dobson, C. M., “The Characterization of Hardened Alkali-Activated Blast-Furnace Slag Pastes and the Nature of the Calcium Silicate Hydrate (C-S-H) Phase,” Cement and Concrete Research, V. 24, No. 5, 1994, pp. 813-829. doi: 10.1016/0008-8846(94)90002-7

15. Brough, A., and Atkinson, A., “Sodium Silicate-Based, Alkali-Activated Slag Mortars: Part I. Strength, Hydration and Microstructure,” Cement and Concrete Research, V. 32, No. 6, 2002, pp. 865-879. doi: 10.1016/S0008-8846(02)00717-2

16. ACI Committee 201, “Guide to Durable Concrete (ACI 201.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 49 pp


ALSO AVAILABLE IN:

Electronic Materials Journal