Transport and Durability Properties of Alkali-Activated Natural Pozzolan/Slag Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Transport and Durability Properties of Alkali-Activated Natural Pozzolan/Slag Concrete

Author(s): Meysam Najimi and Nader Ghafoori

Publication: Materials Journal

Volume: 116

Issue: 2

Appears on pages(s): 81-94

Keywords: acid attack; activator combination; alkali activation; corrosion; frost resistance; natural pozzolan; precursor combination; slag; sodium hydroxide concentration; transport properties

DOI: 10.14359/51714455

Date: 3/1/2019

Abstract:
The current study aims to assess the transport and durability properties of alkali-activated concretes made with hybrid aluminosilicate precursors having different proportions of natural pozzolan as a low-calcium precursor and ground-granulated blast furnace slag as a high-calcium precursor, which are activated with different concentrations and combinations of sodium hydroxide and sodium silicate. The studied parameters included precursor combination (natural pozzolan/slag combinations of 30/70, 50/50, and 70/30), sodium hydroxide concentration (1, 1.75, and 2.5 M), and activator combination (sodium hydroxide/sodium silicate combinations of 70/30, 75/25, and 80/20). The resulting concrete mixtures were tested for slump flow, setting time, compressive strength, absorption, rapid chloride penetration, rapid chloride migration, resistance to sulfuric acid attack, chloride-induced corrosion, and frost resistance. Mercury intrusion porosimetry and X-ray diffraction were used to justify the observed behaviors. The performance of alkali-activated natural pozzolan/slag concretes was also compared with that of a reference concrete made with solely portland cement binder. In view of overall performance, an equal proportion of natural pozzolan and slag (50/50) and a 30/70 combination of sodium silicate and sodium hydroxide proved to be the optimum precursor and activator combinations. The optimum sodium hydroxide concentration was dependent on the precursor and activator combinations as well as the expected fresh, strength, transport and durability performance. In terms of the measured transport properties (that is, absorption, chloride penetration depth, and passing charges) and resistance to acid attack and chloride-induced corrosion, all the studied alkali-activated concretes performed considerably superior to the reference portland cement concrete. In the case of frost resistance, only alkali-activated concretes with 50 and 70% slag performed superior to the reference portland cement concrete.

Related References:

1. McLellan, B.; Williams, R.; Lay, J.; Van Riessen, A.; and Corder, G., “Costs and Carbon Emissions for Geopolymer Pastes in Comparison to Ordinary Portland Cement,” Journal of Cleaner Production, V. 19, No. 9-10, 2011, pp. 1080-1090. doi: 10.1016/j.jclepro.2011.02.010

2. Juenger, M. C. G.; Winnefeld, F.; Provis, J. L.; and Ideker, J. H., “Advances in Alternative Cementitious Binders,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1232-1243. doi: 10.1016/j.cemconres.2010.11.012

3. Palomo, A.; Grutzeck, M. W.; and Blanco, M. T., “Alkali-Activated Fly Ashes: A Cement for the Future,” Cement and Concrete Research, V. 29, No. 8, 1999, pp. 1323-1329. doi: 10.1016/S0008-8846(98)00243-9

4. Pacheco-Torgal, F.; Castro-Gomes, J.; and Jalali, S., “Alkali-Activated Binders: A Review: Part 1. Historical Background, Terminology, Reaction Mechanisms and Hydration Products,” Construction & Building Materials, V. 22, No. 7, 2008, pp. 1305-1314. doi: 10.1016/j.conbuildmat.2007.10.015

5. Shi, C.; Jiménez, A. F.; and Palomo, A., “New Cements for the 21st Century: The Pursuit of an Alternative to Portland Cement,” Cement and Concrete Research, V. 41, No. 7, 2011, pp. 750-763. doi: 10.1016/j.cemconres.2011.03.016

6. Pacheco-Torgal, F.; Labrincha, J. A.; Leonelli, C.; Palomo, A.; and Chindaprasirt, P., Handbook of Alkali-Activated Cements, Mortars and Concretes, Woodhead Publishing, Sawston, UK, 2015.

7. Shi, C.; Krivenko, P. V.; and Roy, D. M., Alkali-Activated Cements and Concrete, Taylor & Francis, Abingdon, UK, 2006.

8. Duxson, P., and Van Deventer, J., “Commercialization of Geopolymers for Construction – Opportunities and Obstacles,” Geopolymers: Structure, Processing, Properties and Applications, J. Provis and J. Van Deventer, eds., Woodhead Publishing, Sawston, UK, 2009, pp. 379-400.

9. Provis, J. L., and Van Deventer, J. S. J., “Alkali Activated Materials: State-of-the-Art Report,” RILEM TC 224-AAM, 2014.

10. Kumar, S.; Kumar, R.; and Mehrotra, S., “Influence of Granulated Blast Furnace Slag on the Reaction, Structure and Properties of Fly Ash Based Geopolymer,” Journal of Materials Science, V. 45, No. 3, 2010, pp. 607-615. doi: 10.1007/s10853-009-3934-5

11. Wang, W. C.; Wang, H. Y.; and Lo, M. H., “The Fresh and Engineering Properties of Alkali Activated Slag as a Function of Fly Ash Replacement and Alkali Concentration,” Construction & Building Materials, V. 84, 2015, pp. 224-229. doi: 10.1016/j.conbuildmat.2014.09.059

12. Abdalqader, A. F.; Jin, F.; and Al-Tabbaa, A., “Development of Greener Alkali-Activated Cement: Utilisation of Sodium Carbonate for Activating Slag and Fly Ash Mixtures,” Journal of Cleaner Production, V. 113, 2016, pp. 66-75. doi: 10.1016/j.jclepro.2015.12.010

13. Ismail, I.; Bernal, S. A.; Provis, J. L.; Hamdan, S.; and Van Deventer, J. S. J., “Microstructural Changes in Alkali Activated Fly Ash/Slag Geopolymers with Sulfate Exposure,” Materials and Structures, V. 46, No. 3, 2013, pp. 361-373. doi: 10.1617/s11527-012-9906-2

14. Najimi, M., “Alkali-Activated Natural Pozzolan/Slag Binder for Sustainable Concrete,” PhD dissertation, University of Nevada Las Vegas, Las Vegas, NV, Dec. 2016, 431 pp.

15. ASTM C618-15, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2015, 5 pp.

16. ASTM C989/C989M-16, “Standard Specification for Slag Cement for Use in Concrete and Mortars,” ASTM International, West Conshohocken, PA, 2016, 7 pp.

17. ASTM C33/C33M-16. “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2016, 11 pp.

18. Najimi, M.; Ghafoori, N.; and Sharbaf, M., “Alkali-Activated Natural Pozzolan/Slag Mortars: A Parametric Study,” Construction & Building Materials, V. 164, 2018, pp. 625-643. doi: 10.1016/j.conbuildmat.2017.12.222

19. Kosmatka, S. H.; Kerkhoff, B.; and Panarese, W. C., Design and Control of Concrete Mixtures, 14th edition, Portland Cement Association, Skokie, IL, 2002, 372 pp.

20. ASTM C143/C143M-15, “Standard Test Method for Slump of Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2015, 4 pp.

21. ASTM C403/C403M-16, “Standard Test Method for Slump of Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2016, 7 pp.

22. ASTM C39/C39M-15, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

23. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 3 pp.

24. ASTM C1202-10, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2010, 7 pp.

25. NT BUILD 492, “Concrete, Mortar and Cement-Based Repair Materials: Chloride Migration Coefficient from Non-Steady-State Migration Experiments,” NORDTEST, Espoo, Finland, 1999.

26. Melo Neto, A. A.; Cincotto, M. A.; and Repette, W., “Drying and Autogenous Shrinkage of Pastes and Mortars with Activated Slag Cement,” Cement and Concrete Research, V. 38, No. 4, 2008, pp. 565-574. doi: 10.1016/j.cemconres.2007.11.002

27. Chi, M., and Huang, R., “Binding Mechanism and Properties of Alkali-Activated Fly Ash/Slag Mortars,” Construction & Building Materials, V. 40, 2013, pp. 291-298. doi: 10.1016/j.conbuildmat.2012.11.003

28. Allahverdi, A., and Škvára, F., “Sulfuric Acid Attack on Hardened Paste Of Geopolymer Cements Part 1. Mechanism of Corrosion at Relatively High Concentrations,” Ceramics-Silikáty, V. 49, No. 4, 2005, pp. 225-229.

29. Ismail, I.; Bernal, S. A.; Provis, J. L.; San Nicolas, R.; Brice, D. G.; Kilcullen, A. R.; Hamdan, S.; and Van Deventer, J. S. J., “Influence of Fly Ash on the Water and Chloride Permeability of Alkali Activated Slag Mortars and Concretes,” Construction & Building Materials, V. 48, 2013, pp. 1187-1201. doi: 10.1016/j.conbuildmat.2013.07.106


ALSO AVAILABLE IN:

Electronic Materials Journal