Effect of Common Surface Pretreatments on Shear Strength of Bonded Concrete Overlays

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Common Surface Pretreatments on Shear Strength of Bonded Concrete Overlays

Author(s): Andrew S. Pultorak and Frederick R. Rutz

Publication: Concrete International

Volume: 40

Issue: 12

Appears on pages(s): 55-60

Keywords: bond, substrate, bonding agent, moisture

DOI: 10.14359/51714415

Date: 12/1/2018

Abstract:
Concrete repairs frequently involve placing a new concrete surface (overlay) on existing concrete (substrate). In this study, pull-off, direct shear, and jacking tests were used to evaluate the bond of overlays applied to mechanically roughened and cleaned substrates. Test parameters included substrate moisture condition and the use of cement slurry bonding agent.

Related References:

1. ACI Committee 345, “Guide to Highway Bridge Deck Construction (ACI 345R-11),” American Concrete Institute, Farmington Hills, MI, 2011, 32 pp.

2. Pultorak, A.S., “The Effects of Common Surface Pretreatments on the Shear Strength of Bonded Concrete Overlays,” MS thesis, University of Colorado Denver, Denver, CO, 2016, 123 pp.

3. Wells, J.A.; Stark, R.D.; and Polyzois, D., “Getting Better Bond in Concrete Overlays,” Concrete International, V. 21, No. 3, Mar. 1999, pp. 49-52.

4. Felt, E.J., “Resurfacing and Patching Concrete Pavements with Bonded Concrete,” Proceedings of the Thirty-Fifth Annual Meeting of the Highway Research Board, V. 35, 1956, pp. 444-469.

5. Saucier, F., and Pigeon, M., “Durability of New-to-Old Concrete Bondings,” Evaluation and Rehabilitation of Concrete Structures and Innovations in Design, SP-128, V.M. Malhotra ed., American Concrete Institute, Farmington Hills, MI, 1991, pp. 689-705.

6. Wall, J.S., and Shrive, N.G., “Factors Affecting Bond Between New and Old Concrete,” ACI Materials Journal, V. 85, No. 2, Mar.-Apr. 1988, pp. 117-125.

7. “Resurfacing Concrete Floors,” IS144.07T, Portland Cement Association, Skokie, IL, 1996, 8 pp.

8. Bissonnette, B.; Vaysburd, A.M.; and von Fay, K.F., “Best Practices for Preparing Concrete Surface Prior to Repairs and Overlays,” Report No. MERL 12-17, Bureau of Reclamation, Denver, CO, 2012, 84 pp.

9. Silfwerbrand, J., and Paulsson, J., “Better Bonding of Bridge Deck Overlays,” Concrete International, V. 20, No. 10, Oct. 1998, pp. 56-61.

10. ACI Committee 325, “Concrete Overlays for Pavement Rehabilitation (ACI 325.13R-06),” American Concrete Institute, Farmington Hills, MI, 2006, 39 pp.

11. Rosen, C.J., “Shear Strength at the Interface of Bonded Concrete Overlays,” MS thesis, University of Colorado Denver, Denver, CO, 2016, 102 pp.

12. “ICRI 310.2R2013 - Selecting and Specifying Concrete Surface Preparation for Sealers, Coatings, Polymer Overlays, and Concrete Repair,” International Concrete Repair Institute, Inc., St. Paul, MN, 2013, 48 pp.

13. Hindo, K.R., “In-Place Bond Testing and Surface Preparation of Concrete,” Concrete International, V. 12, No. 4, Apr. 1990, pp. 46-48.

14. “Test Method for Determination of the Shear Strength at the Interface of Bonded Layers of Concrete,” FHWA-RD-07-052, Federal Highway Administration, Washington, DC, 2007, www.fhwa.dot.gov/publications/research/infrastructure/pavements/ltpp/07052/pro67.cfm.

15. “Standard Method of Test for Shear Strength of Bonded Polymer Concrete,” Illinois Department of Transportation, Springfield, IL, 2012, 8 pp.

16. Riding, K.A., and DonJuan, J., “Evaluation of Bonding Agent Application on Concrete Patch Performance,” Report No. 25-1121-0003-166, Research and Innovative Technology Administration, Washington, DC, 2014, 73 pp.

17. Vaysburd, A.M., and McDonald, J.E., “An Evaluation of Equipment and Procedures for Tensile Bond Testing of Concrete Repairs,” Technical Report REMR-CS-61, U.