Overview of Factors Influencing Concrete Modulus of Elasticity

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Overview of Factors Influencing Concrete Modulus of Elasticity

Author(s): Van K. Bui

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/20/2018

Abstract:
The requirements for achieving sufficient modulus of elasticity (MOE) of concrete is increasing not only for high rise structures, but also for concrete precast/prestressed components and repair application. However, achieving high modulus of elasticity, while maintaining good workability, pumpability and consolidation of concrete is of challenge for concrete producers and contractors. This presentation will highlight main factors influencing on concrete modulus of elasticity. These factors include materials, concrete compositions, microstructure and interface between cementitious material paste and aggregates. The influence of mixer efficiency, workability, rheology and consolidation on MOE will be discussed. Some examples of highly workable high-performance concrete used in high profile projects such as One World Trade Center and Trump Tower in Chicago as well as laboratory development of concrete having extremely high MOE of approx. 9 million psi (62 MPa) will be also presented.