Post-tensioned NSM CFRP for Upgrading Concrete Bridges: Modeling, Testing, and Field Application

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Post-tensioned NSM CFRP for Upgrading Concrete Bridges: Modeling, Testing, and Field Application

Author(s): Yail J. Kim, Hee Young Lee, Wonseok Chung, Jae-Yoon Kang, Jong-Sup Park, and Woo-Tai Jung

Publication: Symposium Paper

Volume: 327

Issue:

Appears on pages(s): 4.1-4.18

Keywords: bridge; carbon fiber reinforced polymer (CFRP); near-surface-mounted (NSM); site application, strengthening; upgrade

DOI: 10.14359/51713324

Date: 11/1/2018

Abstract:
This paper presents an on-going research program to develop an effective strengthening method using post-tensioned near-surface-mounted (NSM) carbon fiber reinforced polymer (CFPP) composites for constructed bridges girders. Various technical aspects associated with strengthened girders are examined through computational modeling, laboratory experiments (small- and full-scale tests), and a field project that is the world’s first site application of post-tensioned NSM CFRP. The flexural behavior of the bridge girders is improved by strengthening (that is, cracking, yield, and ultimate loads, as well as serviceability) relative to unstrengthened control girders, and the post-tensioned NSM CFRP should cover at least 60% of the girder length. The influence of CFRP post-tensioning on the girder concrete adjacent to the anchorage exponentially decays and becomes negligible beyond a distance of 800 mm (31 in.), irrespective of girder size. The presence of initial damage in the girder does not affect the efficiency of the strengthening system until failure occurs. The site application is dedicated to upgrading the design live load capacity of a 56-year old bridge in South Korea from 318 kN (72 kips) to 424 kN (95 kips). Step-by-step procedures are detailed for the technology transfer. Long-term performance monitoring for this upgraded bridge is underway and corresponding results will be reported when sufficient data are available.

Related References:

1. Neale, K.W. 2000. FRPs for structural rehabilitation: a survey of recent progress, Progress in Structural Engineering and Materials, John Wiley & Sons, 2, 133-138.

2. Bakis, C.E., Bank, L.C., Brown, V.L., Cosenza, E., Davalos, J.F., Lesko, J.J., Machida, A., Rizkalla, S.H., and Triantafillou, T.C. 2002. Fiber-reinforced polymer composites for construction: state-of-the-art review, Journal of Composites for Construction, 6(2), 73-87.

3. ACI. 2008. Guide for the design and construction of externally bonded FRP systems for strengthening concrete structures (ACI440.2R-08), American Concrete Institute, Farmington Hills, MI.

4. AASHTO.2012. Guide specifications for design of bonded FRP systems for repair and strengthening of concrete bridge elements (1st edition), American Association of State Highway Transportation Officials, Washington, D.C.

5. CSA. 2017. Design and construction of building structures with fibre-reinforced polymers, Canadian Standard Associations, Toronto, ON, Canada.

6. Wight, R.G., Green, M.F., and Erki, M-A, 2001. Prestressed FRP sheets for poststrengthening reinforced concrete beams, Journal of Composites for Construction, 5(4), 214-220.

7. El-Hacha, R. and Soudki, K. 2013. Prestressed near-surface mounted fibre reinforced polymer reinforcement for concrete structures- a review, Canadian Journal of Civil Engineering, 40, 1127-1139.

8. Lee, D. and Cheng, L. 2011. Assessing the strengthening effect of various near-surface-mounted FRP reinforcements on concrete bridge slab overhangs, Journal of Composites for Construction, 15(4), 615-624.

9. Oudah, F. and El-Hacha, R. 2012. Fatigue behavior of RC beams strengthened with prestressed NSM CFRP rods, Composite Structures, 94, 1333-1342.

10. Peng, H., Zhang, J., Cai, C.S., and Liu, Y. 2014. An experimental study on reinforced concrete beams strengthened with prestressed near surface mounted CFRP strips, Engineering Structures, 79, 222-233.

11. Rezazadeh, M., Ramezansefat, H., and Barros, J. 2016. NSM CFRP prestressing techniques with strengthening potential for simultaneously enhancing load capacity and ductility performance, Journal of Composites for Construction, 20(5), 04016029.

12. Kim, Y.J., Kang, J.-Y., and Park, J.-S. 2015. Post-tensioned NSM CFRP strips for strengthening PC beams: a numerical investigation, Engineering Structures, 105, 37-47.

13. KHC. Standard drawing of highway bridges. Seongnam-si (Gyeonggi-do, Korea): Korea Highway Corporation; 2001.

14. Lee, H.Y., Jung, W.T., and Chung, W. 2017. Flexural strengthening of reinforced concrete beams with pre-stressed near surface mounted CFRP systems, Composite Structures, 163, 1-12.

15. Jung, W.-T., Keum, M.-S., Park, J.-S., Kang, J.-Y., Park, Y.-H., Chung, W., and Kim, Y.J. 2017. Composite strengthening of a bridge, Concrete International, 39(5), 48-53.