Title: A New Model for Crack Control in Reinforced Concrete Tank Walls—Part I: Analytical Investigation

Author(s): Mariusz Zych

Publication: Structural Journal

Volume: 116

Issue: 3

Appears on pages(s): 85-94

Keywords: codes of practice; crack control; early-age concrete; imposed deformation; reinforced concrete tank walls; semi-massive tanks; thermal stress

DOI: 10.14359/51713317

Date: 5/1/2019

Abstract:
A new calculation model for crack control in semi-massive reinforced concrete tanks used for liquid storage is proposed. The model includes three basic stages for the development of the crack width. The first stage covers the formation of early-age cracks occurring as a result of imposed loads acting during concrete hardening. The second stage concerns the formation of a stabilized spacing of basic cracks as well as the early period of imposed loads acting on a structure. The third stage involves sufficiently high values of imposed loads or, most frequently, service loads that result in the occurrence of second-order cracks and a simultaneous increase in the width of cracks formed in previous stages. In addition, instead of the degree of restraint, an average degree of relaxation was suggested as the basic parameter determining the crack width and spacing.

Related References:

1. Stoffers, H., “Cracking Due to Shrinkage and Temperature Variation in Walls,” third edition, Delft University of Technology and I.B.B.C., Delft, the Netherlands, V. 23, No. 3, 1978, 68 pp.

2. ACI Committee 207, “Report on Thermal and Volume Change Effects on Cracking of Mass Concrete (ACI 207.2R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 28 pp.

3. BS, “Design of Concrete Structures for Retaining Aqueous Liquids (8007),” British Standards Institution, London, UK, 1987, 28 pp.

4. CEN, “Eurocode 2 – Design of Concrete Structures — Part 3: Liquid Retaining and Containment Structures (EN 1992-3),” European Committee for Standardization, Brussels, Belgium, 2006, 23 pp.

5. NZS, “Design of Concrete Structures for the Storage of Liquids (3106:2009),” Standards New Zealand, Wellington, New Zealand, 2009, 81 pp.

6. Iványi, G., “Bemerkungen zu Mindestbewehrung in Wänden,” Beton- und Stahlbetonbau, V. 90, No. 11, 1995, pp. 283-289. doi: 10.1002/best.199500460

7. Rostásy, F. S., and Henning, W., “Zwang in Stahlbetonwänden auf Fundamenten,” Beton- und Stahlbetonbau, V. 84, No. 8-9, 1989, pp. 208-214 and 232-237.

8. Zych, M., “The Influence of Ambient Temperature on RC Tank Walls Watertightness in Research and Theory,” Periodica Polytechnica. Civil Engineering, V. 59, No. 3, 2015, pp. 267-278. doi: 10.3311/PPci.7728

9. CEN, “Eurocode 2 - Design of Concrete Structures — Part 1-1: General Rules and Rules for Buildings (EN 1992-1-1),” European Committee for Standardization, Brussels, Belgium, 2004, 205 pp.

10. Buffo-Lacarrière, L.; Sellier, A.; Turatsinze, A.; and Escadeillas, G., “Finite Element Modelling of Hardening Concrete, Application to the Prediction of Early Age Cracking for Massive Reinforced Structures,” Materials and Structures, V. 44, No. 10, 2011, pp. 1821-1835. doi: 10.1617/s11527-011-9740-y

11. Klemczak, B., and Knoppik-Wróbel, A., “Degree of Restraint Concept in Analysis of Early-Age Stresses in Concrete Walls,” Engineering Structures, V. 102, No. 11, 2015, pp. 369-386.

12. Liu, X.; Yuan, Y.; and Su, Q., “Sensitivity Analysis of the Early-Age Cracking Risk in an Immersed Tunnel,” Structural Concrete, V. 15, No. 2, 2014, pp. 179-190. doi: 10.1002/suco.201300064

13. Wu, S.; Huang, D.; Lin, F.-B.; Zhao, H.; and Wang, P., “Estimation of Cracking Risk of Concrete at Early Age Based on Thermal Stress Analysis,” Journal of Thermal Analysis and Calorimetry, V. 105, No. 1, 2011, pp. 171-186. doi: 10.1007/s10973-011-1512-y

14. Kheder, G. F., “A New Look at the Control of Volume Changes Cracking Base Restrained Concrete Walls,” ACI Structural Journal, V. 94, No. 3, May-June 1997, pp. 262-271.

15. Kheder, G. F.; Al-Rawi, R. S.; and Al-Dhahi, J. K., “A Study of the Behavior of Volume Change Cracking in Base Restrained Concrete Walls,” Materials and Structures, V. 27, No. 7, 1994, pp. 383-392. doi: 10.1007/BF02473441

16. Al Rhawi. R. S., and Kheder, G. F., “Control of Cracking Due to Volume Change in Base-Restrained Concrete Members,” ACI Structural Journal, V. 87, No. 4, July-Aug. 1990, pp. 397-405.

17. Scott, R. H., and Gill, P., “Short Term Distribution of Strain and Bond Stress Along Tension Reinforcement,” Structural Engineering, V. 65B, No. 2, 1987, pp. 39-43.

18. Beeby, A. W., and Forth, J. P., “Control of Cracking Walls Restrained Along Their Base against Early Thermal Movements,” Proceedings of the 6th International Congress on Global Construction, Ultimate Concrete Opportunities, Thomas Telford, London, UK, 2005, pp. 123-132.

19. Beeby, A. W., and Narayanan, R. S., “Designers’ Guide to EN 1992-1-1 and EN 1992-1-2 Eurocode 2: Design of Concrete Structures. General Rules and Rules for Buildings and Structural Fire Design,” Thomas Telford, London, UK, 2005, 242 pp.

20. Anson, M., and Rowlinson, P. M., “Early-Age Strain and Temperature Measurements in Concrete Tank Walls,” Magazine of Concrete Research, V. 40, No. 145, 1988, pp. 216-226. doi: 10.1680/macr.1988.40.145.216

21. Anson, M., and Rowlinson, P. M., “Field Measurements for Early-Age Strains in Concrete,” Magazine of Concrete Research, V. 42, No. 153, 1990, pp. 203-212. doi: 10.1680/macr.1990.42.153.203

22. Pettersson, D., and Thelandersson, S., “Crack Development in Concrete Structures Due to Imposed Strains. Part I: Modelling,” Materials and Structures, V. 34, No. 1, 2001, pp. 7-13. doi: 10.1007/BF02482194

23. Pettersson, D.; Alemo, J.; and Thelandersson, S., “Influence on Crack Development in Concrete Structures from Imposed Strains and Varying Boundary Conditions,” Construction and Building Materials, V. 16, No. 4, 2002, pp. 207-213. doi: 10.1016/S0950-0618(02)00007-7

24. Zych, M., “Degree of External Restraint of Wall Segments in Semi-Massive Reinforced Concrete Tanks: Part II: Rectangular and Cylindrical Segments,” Structural Concrete: Journal of the fib, V. 19, No. 3, 2018, pp. 829-838. doi: 10.1002/suco.201700037

25. Eurocode 2, “Bemessung und Konstruktion von Stahlbeton- und Spannbetontragwerken – Teil 1-1: Allgemeine Bemessungsregeln und Regeln für den Hochbau (DIN EN 1992-1-1:/NA2011-01),” Nationaler Anhang, Berlin, Germany, 2011.

26. Zych, M., “Degree of External Restraint of Wall Segments in Semi-Massive Reinforced Concrete Tanks: Part I Rectangular Segments,” Structural Concrete: Journal of the fib, V. 19, No. 3, 2018, pp. 820-828. doi: 10.1002/suco.201700036

27. Zych, M., “Thermal Cracking of the Cylindrical Tank under Construction. II: Early Age Cracking,” Journal of Performance of Constructed Facilities, ASCE, V. 29, No. 4, 2015, pp. 1-10. doi: 10.1061/(ASCE)CF.1943-5509.0000577

28. Zych, M., “Case Study of Concrete Mechanical Properties Development Based on Heat Temperature Measurements,” Cement, Wapno, Beton, No. 6, 2015, pp. 383-392.

29. Seruga, A., and Zych, M., “Research of Concrete Creep at Early Age under Compressive and Tensile Stresses,” Cement, Wapno, Beton, No. 2, 2016, pp. 65-77.

30. Seruga, A., and Zych, M., “Thermal Cracking of the Cylindrical Tank under Construction. I: Case Study,” Journal of Performance of Constructed Facilities, ASCE, V. 29, No. 4, 2015, pp. 1-9. doi: 10.1061/(ASCE)CF.1943-5509.0000581

31. Zych, M., “Analysis of RC Tank’s Walls during Early Hardening Period of Concrete, in Aspect of Water-Tightness,” doctoral thesis, Division of Structural Engineering, Cracow University of Technology, Krakow, Poland, 2011, 246 pp.

32. Ouzaa, K., and Benmansour, M. B., “Cracks in Base-Restrained Plain and Reinforced Concrete Walls,” Turkish Journal of Engineering and Environmental Sciences, V. 34, No. 3, 2010, pp. 215-230.

33. Seruga, A.; Szydłowski, R.; and Zych, M., “The Evaluation of Sequential Process of Cracking of Wall Segments in Monolithic Cylindrical Reinforced Concrete Tanks,” Technical Transactions, Civil Engineering, No. 1-B, 2008, pp. 135-163.

34. Flaga, K., “Shrinkage Stresses and Surface Reinforcement in Concrete Structures,” Monograph 391, Cracow University of Technology, Kracow, Poland, 2011.

35. Bamforth, P. B., “Early-Age Thermal Crack Control in Concrete,” CIRIA C660, London, UK, 2007.