Effectiveness of Steel Fibers as Hoops in Exterior Beam-to-Column Joints under Cyclic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effectiveness of Steel Fibers as Hoops in Exterior Beam-to-Column Joints under Cyclic Loading

Author(s): Chang-Sik Choi and Baek-Il Bae

Publication: Structural Journal

Volume: 116

Issue: 2

Appears on pages(s): 205-219

Keywords: beam-to-column subassemblies; fiber contents; hoop; seismic evaluation; steel fiber

DOI: 10.14359/51712278

Date: 3/1/2019

Abstract:
In this study, the seismic performance of reinforced concrete beam-column joint subassemblies reinforced with steel fiber was evaluated through experiments. A total of seven specimens were used, and four steel fiber-reinforced specimens were planned based on the amount of steel fiber, the presence or absence of hoops of joints, and the spacing of hoops arranged in the beam. The steel fibers used were determined to have properties that could be used to replace the minimum shear reinforcement in beams proposed by ACI 318. To evaluate the seismic performance quantitatively, a loading protocol was applied based on the displacement control protocol of ACI 374. Experimental results showed that reinforcement of steel fiber improves the shear strength of the joint itself. The shear strength of the joint increased as the amount of steel fiber was increased. However, the increase rate of the shear strength of the joint decreased with increasing steel fiber content. A large seismic performance improvement was confirmed when the hoop spacing on the beam was widened and the steel fiber was used with the hoop of the joint. Simultaneous reinforcement of steel fiber and the hoop with increased hoop spacing on the beam caused more damage on the beam and reduced the joint shear strength. Seismic performance evaluations according to ACI 374 showed that performance similar to that of the hoop reinforced joint can be expected when steel fiber with 2% volume fraction is used instead of the hoop in the joint region.

Related References:

1. Park, R., and Paulay, T., Reinforced Concrete Structures, John Wiley & Sons, Inc., New York, 1975, pp. 716-758.

2. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

3. NZS 3101:2006, “The Design of Concrete Structures,” Standards New Zealand, Wellington, New Zealand, 2006, 12 pp.

4. Eurocode 8, “Design of Structures for Earthquake Resistance Part 1: General Rules, Seismic Actions and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004, 121 pp.

5. Dhake, P. D.; Patil, Y. D.; and Patil, H. S., “Anchorage Behavior and Development Length of Headed Bars in Exterior Beam-Column Joint,” Magazine of Concrete Research, V. 67, No. 2, 2015, pp. 579-590. doi: 10.1680/macr.14.00144

6. Lee, H. J., and Yu, S. Y., “Cyclic Response of Exterior Beam-Column Joint with Different Anchorage Methods,” ACI Structural Journal, V. 106, No. 3, May-June 2009, pp. 329-339.

7. Chutarat, N., and Aboutaha, R. S., “Cyclic Response of Exterior Reinforced Concrete Beam-Column Joints Reinforced with Headed Bars—Experimental Investigation,” ACI Structural Journal, V. 100, No. 2, Mar.-Apr. 2003, pp. 259-264.

8. Alaee, P., and Li, B., “High-Strength Concrete Exterior Beam-Column Joints with High-Yield Strength Steel Reinforcements,” Engineering Structures, V. 145, 2017, pp. 305-321. doi: 10.1016/j.engstruct.2017.05.024

9. Hwang, H. J.; Park, H. G.; Choi, W. S.; Chung, L.; and Kim, J. K., “Cyclic Loading Test for Beam-Column Connections with 600 MPa (87 ksi) Beam Flexural Reinforcing Bars,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 913-924. doi: 10.14359/51686920

10. ACI Committee 544, “Measurement of Properties of Fiber Reinforced Concrete,” ACI Materials Jounal, V. 85, No. 6, Nov.-Dec. 1988, pp. 583-593.

11. ACI Committee 318. “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary, American Concrete Institute, Farmington Hills, MI, 2008, 473 pp.

12. Parra-Montesinos, G. J., “Shear Strength of Beams with Deformed Steel Fibers,” Concrete International, V. 28, No. 11, Nov. 2006, pp. 57-66.10.1680/macr.12.00078

13. Patel, P. A.; Desai, A. K.; and Desai, J. A., “Evaluation of RC and SFRC Exterior Beam-Column Joint under Cyclic Loading for Reduction in Lateral Reinforcement of the Joint Region,” Magazine of Concrete Research, V. 65, No. 7, 2013, pp. 405-414. doi: 10.1680/macr.13.00310

14. Tran, T.; Hadi, M. N.; and Pham, T. M., “A New Empirical Model for Shear Strength of Reinforced Concrete Beam-Column Connections,” Magazine of Concrete Research, V. 66, No. 10, 2014, pp. 514-530. doi: 10.1680/macr.14.00110

15. Fan, G., and Song, Y., “Effect of Axial Compression Ratio on Dynamic Mechanical Properties of RC Beam-Column Joints,” Magazine of Concrete Research, V. 66, No. 23, 2014, pp. 1219-1236. doi: 10.1016/j.conbuildmat.2012.04.114

16. Gencoglu, M., “The Effect of Stirrups and the Extents of Regions used SFRC in Exterior Beam-Column Joints,” Structural Engineering and Mechanics, V. 27, No. 2, 2007, pp. 223-241. doi: 10.1016/j.matdes.2015.07.164

17. Röhm, C.; Novak, B.; Sasmal, S.; Karusala, R.; and Srinivas, V., “Behaviour of Fiber Reinforced Beam-Column Sub-Assemblages under Reversed Cyclic Loading,” Construction and Building Materials, V.  36, 2012, pp. 319-329. doi: 10.1061/(ASCE)0733-9445(1992)118:2(341)

18. Siva Chidambaram, R., and Agarwal, P. “Seismic Behavior of Hybrid Fiber Reinforced Cementitious Composite Beam-Column Joints,” Materials and Design, V. 86, Dec. 2015, pp. 771-781.

19. Jiuru, T.; Chaobin, H.; Kaijian, Y.; and Yongcheng, Y., “Seismic Behavior and Shear Strength of Framed Joint Using Steel Fiber Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 118, No. 2, 1992, pp. 341-358.

20. ACI Committee 374, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 18 pp.

21. Joint ACI-ASCE Committee 352, “Recommendations for Design of Beam-Column Joints in Monolithic Reinforced Concrete Structures (ACI 352R-02),” American Concrete Institute, Farmington Hills, MI, 2002, 37 pp.

22. KS B 0802, “Method of Tensile Test for Metallic Materials,” Korean Standards Association, Seoul, Korea, 2013, 7 pp.

23. Park, R., “Evaluation of Ductility of Structures and Structural Assemblages from Laboratory Testing,” Bulletin of the New Zealand National Society for Earthquake Engineering, V. 22, No. 3, 1989, pp. 155-166.

24. Henager, C. H., and Doherty, T. J., “Analysis of Reinforced Fibrous Concrete Beams,” Proceedings, ASCE, V. 12, ST-l, Jan. 1976, pp. 177-188.


ALSO AVAILABLE IN:

Electronic Structural Journal