Mechanical Properties of Concrete Made from Different Expanded Lightweight Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanical Properties of Concrete Made from Different Expanded Lightweight Aggregates

Author(s): Kyung-Ho Lee, Keun-Hyeok Yang, Ju-Hyun Mun, and Seung-Jun Kwon

Publication: Materials Journal

Volume: 116

Issue: 2

Appears on pages(s): 9-19

Keywords: design equations; expanded granules; lightweight aggregate concrete; mechanical properties

DOI: 10.14359/51712265

Date: 3/1/2019

Abstract:
The objective of the present study is to provide a databank and comprehensible design equations of the mechanical properties of concrete prepared using different expanded lightweight aggregates. For the statistical database, 25 lightweight aggregate concrete (LWAC) mixtures using expanded bottom ash and dredged soil granules were tested under design compressive strengths of 18, 24, and 35 MPa (2.61, 3.48, and 5.08 ksi) and targeted ovendried densities between 1300 and 1800 kg/m3 (81.6 and 112.4 lb/ft3). Wherever feasible, the mechanical properties measured in the present concrete specimens were compared with those data compiled from LWAC specimens made of expanded clay and/or fly ash granules. The mechanical properties including the moduli of elasticity and rupture, stress-strain relationship, splitting and direct tensile strengths, shear friction strength, and bond strength were proposed as power functions of the compressive strength and oven-dried density of concrete. The mechanical properties predicted using the proposed equations closely agreed with the test results; the coefficient of variation of the ratios between the experiments and predictions was mostly less than 0.18. In addition, the proposed formulae for the compressive strength development and stress-strain relationship corresponded adequately with the experimental response of LWAC. Meanwhile, the design equations of the fib model resulted in overestimations while predicting the early strength gain, direct tensile strength, and bond strength of LWAC. Overall, the proposed equations possessed adequate potential to properly evaluate the different mechanical properties of concrete prepared using expanded lightweight aggregates.

Related References:

1. Öz, H. O.; Gesoglu, M.; Guneyisi, E.; and Sor, N. H., “Self-Consolidating Concrete Made with Cold-bonded Fly Ash Lightweight Aggregates,” ACI Materials Journal, V. 114, No. 3, May-June 2017, pp. 385-395. doi: 10.14359/51689606

2. Hunag, L. J.; Wang, H. Y.; and Wang, S. Y., “A Study of the Durability of Recycled Green Building Materials in Lightweight Aggregate Concrete,” Construction and Building Materials, V. 96, 2015, pp. 353-359. doi: 10.1016/j.conbuildmat.2015.08.018

3. Lotfy, A.; Hossain, K. M. A.; and Lachemi, M., “Transport and Durability Properties of Self-Consolidating Concrete Using Three Types of Lightweight Aggregates,” ACI Materials Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 679-690. doi: 10.14359/51689112

4. Kim, H. K., and Lee, H. K., “Autogenous Shrinkage Reduction with Untreated Coal Bottom Ash for High-Strength Concrete,” ACI Materials Journal, V. 113, No. 3, May-June 2016, pp. 277-285. doi: 10.14359/51688700

5. Soltan, A. M. M.; Kahl, W. A.; El-Raoof, F. A.; El-Kaliouby, B. A. H.; Serry, M. A. K.; and Abdel-Kader, N. A., “Lightweight Aggregates from Mixtures of Granite Wastes with Clay,” Journal of Cleaner Production, V. 117, 2016, pp. 139-149. doi: 10.1016/j.jclepro.2016.01.017

6. Khankhaje, E.; Salim, M. R.; Mirza, J.; Hussin, M. W.; and Rafieizonooz, M., “Properties of Sustainable Lightweight Pervious Concrete Containing Oil Palm Kernel Shell as Coarse Aggregate,” Construction and Building Materials, V. 126, 2016, pp. 1054-1065. doi: 10.1016/j.conbuildmat.2016.09.010

7. Mehta, P. K., and Monteiro, P. M. J., Concrete: Microstructure, Properties, and Materials, McGraw Hill Professional, New York, 2013.

8. Yang, K. H.; Kim, G. H.; and Choi, Y. H., “An Initial Trial Mixture Proportioning Procedure for Structural Lightweight Aggregate Concrete,” Construction and Building Materials, V. 55, 2014, pp. 431-439. doi: 10.1016/j.conbuildmat.2013.11.108

9. Wang, H. Y., and Tsai, K. C., “Engineering Properties of Lightweight Aggregate Concrete Made from Dredged Silt,” Cement and Concrete Composites, V. 28, No. 5, 2006, pp. 481-485. doi: 10.1016/j.cemconcomp.2005.12.005

10. Chandra, S., and Berntsson, L., Lightweight Aggregate Concrete: Science, Technology and Applications, Noyes Publications, New York, 2003.

11. Cui, H. Z.; Lo, T. Y.; Memon, S. A.; Xing, F.; and Shi, X., “Analytical Model for Compressive Strength, Elastic Modulus and Peak Strain of Structural Lightweight Aggregate Concrete,” Construction and Building Materials, V. 36, 2012, pp. 1036-1043. doi: 10.1016/j.conbuildmat.2012.06.034

12. He, Y.; Zhang, X.; Zhang, Y.; and Zhou, Y., “Effects of Particle Characteristics of Lightweight Aggregate on Mechanical Properties of Lightweight Aggregate Concrete,” Construction and Building Materials, V. 72, No. 7, 2014, pp. 270-282. doi: 10.1016/j.conbuildmat.2014.07.043

13. Sim, J. I.; Yang, K. H.; Kim, H. Y.; and Choi, B. J., “Size and Shape Effects on Compressive Strength of Lightweight Concrete,” Construction and Building Materials, V. 38, No. 1, 2013, pp. 854-864. doi: 10.1016/j.conbuildmat.2012.09.073

14. Wang, Q.; Yan, P.; Yang, J.; and Zhang, B., “Influence of Steel Slag on Mechanical Properties and Durability of Concrete,” Construction & Building Materials, V. 47, 2013, pp. 1414-1420. doi: 10.1016/j.conbuildmat.2013.06.044

15. Wasserman, R., and Bentur, A., “Interfacial Interactions in Lightweight Aggregate Concretes and Their Influence on the Concrete Strength,” Cement and Concrete Composites, V. 18, No. 1, 1996, pp. 67-76. doi: 10.1016/0958-9465(96)00002-9

16. Lee, K. H., and Yang, K. H., “Evaluation on Compressive Strength Development of Lightweight Aggregate Concrete using Expanded Bottom Ash and Dredged Soil Granules,” Journal of Architectural Institute of Korea, V. 34, No. 7, 2018, pp. 19-26.

17. Yang, K. H.; Mun, J. H.; Cho, M. S.; and Kang, T. H. K., “A Stress-Strain Model for Various Unconfined Concrete in Compression,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 819-826.

18. Sim, J. I., “The Influence of Unit Weight of Concrete on Size Effect of Compressive Strength, Direct Tensile Strength and Fracture Energy,” PhD dissertation, Kyonggi University, Suwon, South Korea, 2013.

19. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

20. Comité Euro-International du Beton, “fib Model Code for Concrete Structures 2010,” International Federation for Structural Concrete (fib), Lausanne, Switzerland, 2010.

21. ASTM C150/C150M-12, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2012, 9 pp.

22. ASTM C330/C330M-09, “Standard Specification for Lightweight Aggregates for Structural Concrete,” ASTM International, West Conshohocken, PA, 2009, 4 pp.

23. ASTM C31/C31M-10, “Standard Practice for Making and Curing Concrete Test Specimens in the Field,” ASTM International, West Conshohocken, PA, 2010, 6 pp.

24. ASTM C900-06, “Standard Test Method for Pullout Strength of Hardened Concrete,” ASTM International, West Conshohocken, PA, 2006, 10 pp.

25. ACI Committee 213, “Guide for Structural Lightweight-Aggregate Concrete (ACI 213R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 53 pp.

26. Neville, A., Properties of Concrete, fifth edition, Pearson Education Limited, Harlow, UK, 2011.

27. Choi, S. J.; Yang, K. H.; Sim, J. I.; and Choi, B. J., “Direct Tensile Strength of Lightweight Concrete with Different Specimen Depths and Aggregate Sizes,” Construction and Building Materials, V. 63, 2014, pp. 132-141. doi: 10.1016/j.conbuildmat.2014.04.055

28. Yang, K. H., and Ashour, A. F., “Modification Factor for Shear Capacity of Lightweight Concrete Beams,” ACI Structural Journal, V. 112, No. 4, July-Aug. 2015, pp. 485-492. doi: 10.14359/51687658

29. Kwon, S. J.; Yang, K.-H.; Hwang, Y.-H.; and Ashour, A. F., “Shear Friction Strength of Monolithic Concrete Interfaces,” Magazine of Concrete Research, V. 69, No. 5, 2017, pp. 230-244. doi: 10.1680/jmacr.16.00190

30. Harries, K. A.; Zeno, G.; and Shahrooz, B., “Toward an Improved Understanding of Shear-Friction Behavior,” ACI Structural Journal, V. 109, No. 6, Nov.-Dec. 2012, pp. 835-844.


ALSO AVAILABLE IN:

Electronic Materials Journal