Recycled Glass as Aggregate for Architectural Mortars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recycled Glass as Aggregate for Architectural Mortars

Author(s): Francesca Tittarelli , Chiara Giosuè, Alessandra Mobili

Publication: IJCSM

Volume: 12

Issue:

Appears on pages(s):

Keywords: waste glass, architectural mortar, alkali–silica reaction, recycling, durability

DOI: https://doi.org/10.1186/s40069-018-0290-3

Date: 9/30/2018

Abstract:
The possibility of recycling mixed colour waste glass as it is for manufacturing decorative architectural mortars, has been investigated. In mortars, the 0–33–66–100% of calcareous gravel volume has been replaced with recycled glass cullets, with no other inorganic addition. To mitigate the possible alkali–silica reaction, mixes with a hydrophobic admixture were also compared. The obtained results show that the replacement of calcareous gravel with glass cullets of similar grain size distribution permits to reduce the dosage of the superplasticizer admixture to obtain the same workability of fresh mortar; it does not affect significantly the mechanical performances, the water vapour permeabil-ity and the capillary water absorption but it reduces significantly the drying shrinkage deformation. The used recycled glass is classified as no reactive in terms of alkali–silica reaction neither in water nor in NaOH solution following the parameters of the current normative, even in the absence of the hydrophobic admixture. The hydrophobic admixture further delays the expansion trigger but not the speed of its propagation.