A Dual-Functional Intervention Method for Sea-Sand Concrete Structure
Author(s):
Ji-Hua Zhu, Zhi Wang, Wanqian Li, Hanshi Liang, Zhiwen Zeng, Mei-ni Su, Dawang Li, and Feng Xing
Publication:
Symposium Paper
Volume:
330
Issue:
Appears on pages(s):
219-226
Keywords:
C-FRCM; corrosion; impressed current cathodic protection (ICCP); reinforced concrete; sea sand; simply supported beams; structural strengthening.
DOI:
10.14359/51711253
Date:
9/26/2018
Abstract:
With the rapid development of economy and infrastructure, more and more new reinforced concrete (RC) structures are being constructed every day, with the increasing demand for raw materials, such as sands, cement and aggregates. One solution to materials can cause resource shortage is to use sea sand to replace river sand. However, sea sand concrete might cause corrosion of steel re-bars in RC structures, thus resulting in structure deterioration. This study proposes a new dual-functional method to retrofit the sea-sand RC structures by using the carbon - fiber reinforced cementitious matrix (C-FRCM). The C-FRCM composite, consists of carbon fiber mesh and inorganic cementitious material, is both the anodic material in the impressed current cathodic protection process as well as the structural strengthening material. The proposed technique has been shown to be effective in retarding the corrosion of re-bars, and maintaining the loading capacity of the corroded specimens.
Related References:
1. Zhu, J.H., Su, M.N., Huang, Ueda, T., Xing, F., The ICCP-SS Technique for Retrofitting Reinforced Concrete Compressive Members subjected to Corrosion. Constructional & Building Materials, 167: 669-679.
2. Su, M.N., WEI, L.L., ZENG, Z.W., Ueda, T., Xing, F., Zhu, J.H., A solution for sea-sand reinforced concrete beams, Constructional & Building Materials, submitted.
3. ASTM E8/E8M. Standard test methods for tension testing of metallic materials. ASTM International, U.S.A., 2016.
4. ASTM D4018. Standard test methods for properties of continuous filament carbon and graphite fiber tows. ASTM, U.S.A., 1999.
5. BS EN 196-1. Methods of testing cement-Part 1: Determination of strength. 2005.
6. AC434. Acceptance criteria for masonry and concrete strengthening using fiber-reinforced cementitious matrix (FRCM) composite system.2016.
7. ASTM C876. Standard test method for corrosion potential of uncoated reinforcing steel in concrete. U.S.A., 2009.
8. Lambert, P.; Van Nguyen, C.; Mangat, P. S.; O’Flaherty, F. J.; and Jones, G., “Dual function carbon fibre fabric strengthening and impressed current cathodic protection (ICCP) anode for reinforced concrete structures,” Materials and Structures, V. 48, No. 7, 2015, pp. 2157-2167. doi: 10.1617/s11527-014-0300-0
9. ACI 440.2R. Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures. American Concrete Institute U.S.A.2008.