Mechanical and Durability Properties of Coral Aggregate Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanical and Durability Properties of Coral Aggregate Concrete

Author(s): Wen Zhou, Yongxiang Zhou, Peng Feng, Zuqi Wang, Jing Wang, and Putao Song

Publication: Symposium Paper

Volume: 330

Issue:

Appears on pages(s): 175-188

Keywords: coral concrete; mixture proportion design; mechanical property; durability

DOI: 10.14359/51711249

Date: 9/26/2018

Abstract:

Preparing concrete with coral gravel and coral sand as aggregates is of great significance for the construction of offshore islands short of building materials. LC30 and LC50 coral aggregate concrete (CAC) using aggregate from South China Sea were prepared and basic properties of CAC were studied and compared with ordinary concrete (OC) and lightweight aggregate concrete (LAC). The results show that prewetting aggregates improves the compressive strength of CAC with low water-cement ratio (w/c). With the same level of cube compressive strength (fcu), the compressive strength (fc) of CAC is higher than that of OC and LAC, the splitting tensile strength (fsp) of CAC is close to that of OC and higher than that of LAC, the elastic modulus (Ec) of CAC is between that of OC and LAC. Test results on durability properties show that 3-day shrinkage of CAC is 43% of OC; and CAC’s ability to resist chloride diffusion is inferior to OC but better than LAC.

Related References:

1. PRC Ministry of Construction, “Technical specification for lightweight aggregate concrete: JGJ51-2002,” China Architecture & Building Press, China, 2002.

2. PRC Ministry of Construction, “Standard for test method of performance on ordinary fresh concrete: GB/T 50080-2016,” China Architecture & Building Press, China, 2016.

3. PRC Ministry of Construction, “Standard for test method of mechanical properties on ordinary concrete: GB/T 50081-2002,” China Architecture & Building Press, China, 2003.

4. Ye, L., “Concrete Structure,” Tsinghua University Press, China, 2002.

5. PRC Ministry of Construction, “Code for Design of Concrete Structures: GB 50010-2010,” China Architecture & Building Press, China, 2014.

6. Jiao, Y.; Zhu, X.; and Wei, X., “Influence of Design Parameters on Elastic Modulus of Concrete,” Liaoning Building Materials, China, V. 02, 2008, pp. 46-47.

7. PRC Ministry of Construction, “Standard for test method of long-term performance and durability of ordinary concrete: GB/T 50082-2009,” China Architecture & Building Press, China, 2010.