Study on Polycarboxylate Superplasticizer with Slump Retention Capacity

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on Polycarboxylate Superplasticizer with Slump Retention Capacity

Author(s): Zhenping Sun, Lelin Wu, Yanliang Ji, Xu Yang, Yuansong Sun, and Chao Chen

Publication: Symposium Paper

Volume: 329

Issue:

Appears on pages(s): 31-40

Keywords: polycarboxylate superplasticizer; slump retention; synthesis

DOI: 10.14359/51711201

Date: 9/24/2018

Abstract:

The synthesis and performance of slump retention type polycarboxylate superplasticizer using different functional monomers are shown. These polycarboxylate superplasticizers are synthesized using methyl acrylate, hydroxyethyl acrylate, hydroxypropyl acrylate respectively. The best molar proportion of different monomers for synthesis is tested. Properties of these polycarboxylate superplasticizers are compared according to the fluidity of cement paste and their slump retention of concrete. The compositions of these polycarboxylate superplasticizers are described by IR and GPC. From these comparisons, polycarboxylate superplasticizers using hydroxypropyl acrylate have the best properties. Relatively better reaction conditions are determined as: 45°C (113°F) as reaction temperature, 3 hours as dropping time and 1% H2O2/0.15% ascorbic acid as initiator, 0.35% TGA as chain transfer agent. According to the results, polycarboxylate superplasticizers with higher slump retention capacity would be able to produce.