Strength of Reinforced Concrete Pier Caps—Experimental Validation of Strut-and-Tie Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength of Reinforced Concrete Pier Caps—Experimental Validation of Strut-and-Tie Method

Author(s): Indu Geevar and Devdas Menon

Publication: Structural Journal

Volume: 116

Issue: 1

Appears on pages(s): 261-273

Keywords: bearing; disturbed regions; hammerhead; pier cap; shear; strut-and-tie

DOI: 10.14359/51711138

Date: 1/1/2019

Abstract:
The strut-and-tie method (STM) is commonly used to design reinforced concrete (RC) pier caps, where the traditional methods of shear and flexural design cannot be used due to nonlinear strain distribution. This paper presents experimental studies on scaleddown pier cap specimens subject to four concentrated loads, to study the influence of various parameters and the applicability of STM. The STM prescribed by ACI 318 and AASHTO are found to give reasonably conservative results only when the beneficial effect of triaxial confinement near the bearing node is invoked; otherwise, the predictions are overly conservative. Variations in bearing plate size, distributed reinforcement, and loading eccentricity did not have much influence on the load capacity, but distributed reinforcement was seen to be beneficial in limiting crack widths. The formation of the assumed STM is validated using strain measurements in concrete and steel, and it is observed that this develops only after significant cracking.

Related References:

1. Schlaich, J.; Schäfer, K.; and Jennewein, M., “Toward a Consistent Design of Structural Concrete,” PCI Journal, V. 32, No. 3, 1987, pp. 74-150. doi: 10.15554/pcij.05011987.74.150

2. MacGregor, J. G., “Derivation of Strut-and-Tie Models for the 2002 ACI Code,” Examples for the Design of Structural Concrete with Strut-and-Tie Models, SP-208, American Concrete Institute, Farmington Hills, MI, 2002, pp. 7-40.

3. Mattock, A. H.; Chen, K. C.; and Soongswang, K., “The Behaviour of Reinforced Concrete Corbels,” PCI Journal, V. 21, No. 2, 1976, pp. 52-77. doi: 10.15554/pcij.03011976.52.77

4. Armstrong, S. D.; Salas, R. M.; Wood, B. A.; Breen, J. E.; and Kreger, M. E., “Behavior and Design of Large Structural Concrete Bridge Pier Overhangs,” Research Report CTR-1364-1, Center for Transportation, Austin, Texas, 1997, 90 pp.

5. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

6. Joint ACI-ASCE Committee 445, “Recent Approaches to Shear Design of Structural Concrete (ACI 445R-99),” American Concrete Institute, Farmington Hills, MI, 1999, 55 pp.

7. Aguilar, G.; Matamoros, A. B.; Parra-Montesinos, G. J.; Ramírez, J. A.; and Wight, J. K., “Experimental Evaluation of Design Procedures for Shear Strength of Deep Reinforced Concrete Beams,” ACI Structural Journal, V. 99, No. 4, July-Aug. 2002, pp. 539-548.

8. AASHTO, “AASHTO LRFD Bridge Design Specifications,” eighth edition, American Association of State Highway and Transportation Officials, Washington DC, 2017.

9. Ritter, W., “Construction Techniques of Hennebique (Die Bauweise Hennebique),” Schweizerische Bauzetung, V. 33, No. 7, 1899, pp. 59-61. (in German)

10. Morsch, E., Concrete-Steel Construction, McGraw-Hill, New York, 1909.

11. Nielson, M. P., Limit Analysis and Concrete Plasticity, CRC Press, Boca Raton, FL, 1999, pp. 1-19.

12. Muttoni, A.; Schwartz, J.; and Thürlimann, B., Design of Concrete Structures with Stress Fields, Birkhäuser Verlag, Switzerland, 1996, pp. 18-24.

13. He, Z. Q.; Liu, Z.; and Ma, Z. J., “Investigation of Load-Transfer Mechanisms in Deep Beams and Corbels,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 467-476.

14. Birrcher, D.; Tuchscherer, R.; Huizinga, M.; Bayrak, O.; Wood, S. L.; and Jirsa, J. O., “Strength and Serviceability Design of Reinforced Concrete Deep Beams,” Report No. FHWA/TX-09/0-5253-1, Center for Transportation Research, Austin, TX, 2009, pp. 23-350.

15. Young, B. S.; Bracci, J. M.; Keating, P. B.; and Hueste, M. B. D., “Cracking in Reinforced Concrete Bent Caps,” ACI Structural Journal, V. 99, No. 4, July-Aug. 2002, pp. 488-498.

16. Hwang, S. J., and Lee, H. J., “Strength Prediction for Discontinuity Regions by Softened Strut-and-Tie Model,” Journal of Structural Engineering, ASCE, V. 128, No. 12, 2002, pp. 1519-1526. doi: 10.1061/(ASCE)0733-9445(2002)128:12(1519)

17. Sami, A., “The Response of Reinforced Concrete Bridge Pier Caps,” MS thesis, McGill University, Montreal, QC, Canada, 1990.

18. Lim, E., and Hwang, S. J., “Modeling of the Strut-and-Tie Parameters of Deep Beams for Shear Strength Prediction,” Engineering Structures, V. 108, 2016, pp. 104-112. doi: 10.1016/j.engstruct.2015.11.024

19. Adrija, D., “Strength Assessment of RC Deep Beams and Corbels,” MS thesis, IIT Madras, Chennai, India, 2017.

20. Denio, R. J.; Yura, J. A.; and Kreger, M. E., “Behavior of Reinforced Concrete Pier Caps under Concentrated Bearing Loads,” Report No. FHWA/TX-97/1302-1, University of Texas at Austin, Austin, TX, 1995.

21. Zhang, N.; Tan, K. H.; and Leong, C. L., “Single-Span Deep Beams Subjected to Unsymmetrical Loads,” Journal of Structural Engineering, ASCE, V. 135, No. 3, 2009, pp. 239-252. doi: 10.1061/(ASCE)0733-9445(2009)135:3(239)

22. Geevar, I., “Strut-and-Tie Modelling of RC Pier Caps,” PhD thesis, IIT Madras, Chennai, India, 2018.

23. Tuchscherer, R. G.; Brown, M. D.; and Bayrak, O., “Example 1: Bridge Pier—Hammerhead Bent Cap,” Further Examples for the Design of Structural Concrete with Strut-and-Tie Models, American Concrete Institute, Farmington Hills, MI, 2011.

24. Geevar, I., and Menon, D., “Development of Strut-and-Tie Models for RC Bridge Pier Caps Subjected to Asymmetric Loading,” Proceedings of the 11th fib International PhD Symposium in Civil Engineering, University of Tokyo, Japan, 2016, pp. 345-351.

25. Zhang, N., and Tan, K. H., “Size Effect in RC Deep Beams: Experimental Investigation and STM Verification,” Engineering Structures, V. 29, No. 12, 2007, pp. 3241-3254. doi: 10.1016/j.engstruct.2007.10.005

26. Harris, H. G., and Sabnis, G., Structural Modeling and Experimental Techniques, CRC press, Washington, DC, 1999, pp. 63-67.

27. Wang, C.; Salmon, C. G.; and Pincheira, J. A., Reinforced Concrete Design, John Wiley & Sons Inc., 2007, pp. 125-126.


ALSO AVAILABLE IN:

Electronic Structural Journal