Learning from the Japanese Experience with High-Strength Longitudinal Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Learning from the Japanese Experience with High-Strength Longitudinal Reinforcement

Author(s): Tomomi Suzuki, Lucas Laughery, and Santiago Pujol

Publication: Concrete International

Volume: 40

Issue: 9

Appears on pages(s): 47-58

Keywords: columns, test, database, parameters

DOI: 10.14359/51711114

Date: 9/1/2018

Abstract:
More than 200 columns with high-strength reinforcement have been tested in Japan since the late 1980s. Results from these tests are often published only in Japanese, limiting access for non-Japanese readers. To broaden access, a database was compiled with parameters describing the specimens, test setup, and test results. These parameters were based on those used in the ACI 369 rectangular column database to facilitate comparison with existing reinforced-concrete column databases.

Related References:

1. Aoyama, H., Design of Modern Highrise Reinforced Concrete Structures (Series on Innovation in Structures and Construction: Volume 3), Imperial College Press, London, UK, 2001, 442 pp.

2. Suzuki, T., “High-Strength Steel in Reinforced Concrete Columns,” 2015, https://datacenterhub.org/resources/278.

3. Fujimoto, J.; Miyako, M.; and Shoda, Y., “An Experimental Study on Seismic Performance of Using High-Strength Concrete (Fc 60〜80 MPa) RC Columns (高強度コンク リート(Fc 60〜100 MPa)を用い RC柱の曲 げせん断実験),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1999, pp. 845-846. (in Japanese)

4. Hamada, M.; Yoshimatsu, K.; Ishibashi, H.; and Horie, K., “Experimental Study on Reinforced Concrete Columns with Super High-Strength Materials (超高強度材料を使 用 し た RC 柱に関す る実験研究),” Proceedings of the Japan Concrete Institute, V. 18, No. 2, 1996, pp. 893-898. (in Japanese)

5. Hosoya, H.; Funayama, Y.; Kono, M.; and Masuo, K., “Experimental Study on Structural Performance of Fc 150 N/mm2 Reinforced Concrete Columns (Fc 150 N/mm2 級コンクリートを用いた柱部材の構造性能の実験 的研究),” Journal of Technology and Design, Architectural Institute of Japan, Tokyo, Japan, V. 19, No. 42, 2013, pp. 549-554. (in Japanese)

6. Huang, K.; Li, K-N; and Kabeyasawa, T., “Experimental Study on Strength and Deformability of High-Strength Reinforced Concrete Columns under High Axial Load (高軸力を受ける高強度鉄筋コンク リート柱の強度と変形能力に関する実験的研究),” Proceedings of the Japan Concrete Institute, V. 12, No. 2, 1990, pp. 427-432. (in Japanese)

7. Ishikawa, Y.; Kimura, H.; Sawamura, M.; and Ueda, T., “Performance of High-Strength Main Bars under Combined High Axial Load and Bending Moment (高強度コ ンクリ一卜 ・高強度鉄筋を 用いた柱の高軸力下における力学性状),” Proceedings of the Japan Concrete Institute, V. 22, No. 3, 2000, pp. 943-948. (in Japanese)

8. Kato, D., “Ductility of Reinforced Concrete Columns with High-Strength Concrete and Reinforcement (高強度材料を用いたRC柱の 曲げ性能の評価に関する実験的研究),” Proceedings of the Japan Concrete Institute, V. 13, No. 2, 1991, pp. 415-420. (in Japanese)

9. Kato, D.; Suzuki, H.; and Honda, Y., “Static Loading Tests of High-Strength RC Columns with Buckling Main Bars under Varying Axial Load (主筋の座屈挙動に着目した変動軸力を受ける高強度RC 柱の静加力実験),” Proceedings of the Japan Concrete Institute, V. 17, No. 2, 1995, pp. 351-356. (in Japanese)

10. Kitada, Y.; Sakaguchi, N.; Kawachi, T.; Kouda, S.; Nozaki, J.; and Kuzuki, M., “Flexural and Shear Strength of Reinforced Concrete Columns Using Ultra-High-Strength Materials, Part 1: Outline of Experiment (超高強度鉄筋コンクリート造柱の曲げせん断実験, そ の1: 実験概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, Structures II, 1988, pp. 697-698. (in Japanese)

11. Kouda, S.; Sakaguchi, N.; Kitada, Y.; Kawachi, T.; Nozaki, T.; and Kuzuki, M., “Flexural and Shear Strength of Reinforced Concrete Columns Using Ultra-High-Strength Materials, Part 2: Flexural Behavior of Columns (超高強度鉄筋コンクリート造柱の曲げせん断実験, そ の2: 曲げ特性),” Summaries of Technical Papers of Annual Meeting of the Architectural Institute of Japan, Structures II, 1988, pp.699-700. (in Japanese)

12. Komuro, T.; Imai, K.; Muramatsu, A.; Korenaga, T.; and Watanabe, F., “Compressive Properties of Reinforced Concrete Columns Using High-Strength Concrete with Compressive Strength of 100〜180 N/mm2 (100〜180 N/mm2の超高強度コンクリートを用いた鉄筋コ ンクリート柱の圧縮特性),” Journal of Structural and Construction Engineering, Architectural Institute of Japan, Tokyo, Japan, V. 69, No. 577, 2004, pp.77-84. (in Japanese)

13. Kosugi, K.; Yamanaka, H.; Oda, M.; Saito, M.; and Kando, S., “Experimental Study on Shear and Flexural Behavior of RC Column with High-Strength Materials, Part 1: Outline of the Experiment and the Results (高強度RC造柱の曲げおよびせん断性状, その1: 実験計画 および結果の概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1997, pp. 69-70. (in Japanese)

14. Oda, M.; Kosugi, K.; Yamanaka, H.; Saito, M.; and Kando, S., “Experimental Study on Shear and Flexural Behavior of RC Column with High-Strength Materials, Part 2: Discussions of Strain of Reinforcement Bar and Ultimate Strength (高強度RC造柱の曲げおよ びせん断性状, その2: 補強筋のひずみと耐力の検討),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1997, pp. 71-72. (in Japanese)

15. Kumagai, H., “Structural Performance of Ultra-High-Strength Reinforced Concrete Columns (超高強度鉄筋コンクリート柱の構 性能),” Concrete Journal, V. 39, No. 3, 2001, pp. 44-50. (in Japanese)

16. Maruta, M.; Kimura, A.; and Suzuki, N., “Bending Shear Test on High-Strength RC Column Using 100 N/mm2 Strength Concrete. Part 1: Outline of Experiment and Results of Experiment (100 N/mm2コンク リートを用いた高強度鉄筋コンクリート柱の曲げせん断実験: そ の1. 実験概要及び実験結果),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 2001, pp. 419-420. (in Japanese)

17. Mihara, Y.; Hibi, J.; Kotani, S.; and Aoyama, H., “Experimental Study on Shear Behavior of Reinforced Concrete Columns Using High-Strength Concrete after Flexural Yielding, Part 1: Outline of the Tests (高強度コンクリートを用いた鉄筋コンクリート造柱の曲げ降伏後 のせん断変形態に関する実験的研究, その1: 曲げせん断実験とそ の結果の概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C, Structures II, 1991, pp. 199-200. (in Japanese)

18. Murakami, H.; Miyawaki, Y.; Fujiwara, M.; and Fujii, A., “Experimental Study on Structural Property of RC Columns Using High-Strength Concrete (超高強度コンクリートを用いたRC柱部材 の構造特性に関する実験研究),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1995, pp. 379-380. (in Japanese)

19. Murata, K.; Watai, T.; Kominami, K.; Higashibata, Y.; and Kimura, H., “Cyclic Loading Test on RC Columns Using 80 MPa Concrete and High-Strength Longitudinal Bars (Grade SD490 and 685), Part 1: Test Program and Outline of Test Results (Fc 800高強度コンク リートと高強度主筋(SD490, 685)を用いたRC柱の曲げせん断実験, その1: 実験計画および実験結果の概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1996, pp. 167-168. (in Japanese)

20. Watai, T.; Murata, K.; Kominami, K.; Higashibata, Y.; and Kimura, H., “Cyclic Loading Test on RC Columns Using 80 MPa Concrete and High Strength Longitudinal Bars (Grade SD490 and 685), Part 2: Analysis of Test Results (Fc 800高強度コンクリートと高強 度主筋(SD490,685)を用いたRC柱の曲げせん断実験, その2: 実 験結果の検討),” Summaries of Technical Papers of Annual Meeting Architectural Institute of Japan, C-2, Structures IV, 1996, pp. 169-170. (in Japanese)

21. Nakae, A.; Kuramoto, H.; and Minami, K., “Experimental Studies on Reinforced Concrete Columns Using High-Strength Concrete, Part 1: Shear Behavior of Columns Using High-Strength Concrete of σB = 1200 kgf/cm2 (高強度コンクリートを用いた鉄筋コンクリート柱の実験 的研究, その1: σB = 1200 kgf/cm2 の場合のせん断破壊性状),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, Structures II, 1990, pp. 837-838. (in Japanese)

22. Nakazawa, A.; Yamashita, Y.; Kuwada, H.; and Minami, K., “Behavior in Shear Failure of RC Columns with High-Strength Shear Reinforcement and Concrete (高強度材料を用いたRC柱のせん断破壊 性状),” Proceedings of the Japan Concrete Institute, V. 21, No. 3, 1999, pp. 397-402. (in Japanese)

23. Okuda, J.; Nakai, S.; Funato, Y.; Tani, M.; Sun Y.; and Fujinaga, T., “Effects of Steel Ratio and Axial Load Level on the Seismic Properties of Concrete Columns with Extra-High-Strength Rebars, Part 1: Experimental Outline (超高強 度鉄筋を用いたRC柱の耐震性能に主筋比 等が及ぼす影響, その1: 実験概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 2011, pp. 119-120. (in Japanese)

24. Nakai, S.; Okuda, J.; Funato, Y.; Tani, M.; Sun, Y.; and Fujinaga, T., “Effects of Steel Ratio and Axial Load Level on the Seismic Properties of Concrete Columns with Extra- High-Strength Rebars, Part 2: Experimental Results and Discussion (超高強度鉄筋を用いたRC柱の耐震性能に主筋比等が及ぼす影 響, その2: 実験結果と考察),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 2011, pp. 121-120. (in Japanese)

25. Satoh, H.; Kaminosono, T.; Yagenji, A.; Takasaki, T.; Imanishi, T.; Kurihara, M.; and Murata, Y., “Behavior of High-Strength RC Columns under High Axial Load: Flexure Test on Columns (高強度鉄筋コンクリート造柱 の高軸力下の性状 : 柱の純曲げ実験),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C, Structures II, 1991, pp. 157-158. (in Japanese)

26. Sun, Y.P., and Sakino, K., “Ductility Improvement of Reinforced Concrete Columns with High-Strength Materials (高強度材料を 用いた鉄筋コンクリート柱の靭性改善に関 する実験的研究),” Proceedings of the Japan Concrete Institute, V. 15, No. 2, 1993, pp. 719-724. (in Japanese)

27. Takami, S., and Yoshioka, K., “RC Columns Under Bi-Axial Load Using High-Strength Concrete (超高強度コンクリートを用いた柱の2方向曲げせん断実験),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1996, pp. 177-178. (in Japanese)

28. Tanaka, H.; Sato, Y.; Park, R.; and Kani, N., “High-Strength Concrete Columns with Longitudinal Reinforcement of Mixed Steel Grades,” High-Performance Concrete,

Proceedings, International Conference, Singapore 1994, SP 149, V.M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1994, pp. 391-411.

29. Komuro, T.; Sato, Y.; Tanaka, H.; and Park, R., “High-Strength Concrete Columns with Longitudinal Reinforcement of Mixed Steel Grades (強度の異なる軸鉄筋をもつ高 強度コンクリート柱),” Proceedings of the Japan Concrete Institute, V. 17, No. 2, 1995, pp. 441-446. (in Japanese)

30. Tano, K.; Yamanaka, H.; and Oda, M., “Flexural and Shear Behavior of High-Strength RC Columns, Part 3: Precast Members and Ultra-High Strength Member Experiments (高 強度RC造柱の曲げおよびせん断性状, その 3: プレキャスト部材および超高強度部材実 験),” Summaries of the Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1998, pp. 375-376. (in Japanese)

31. Yamauchi, S.; Ooi, T.; Chiba, O.; Ishikawa, K.; Kikuta, S.; Izumi, N.; and Takenaka, H., “Experimental Study on Behavior of Reinforced Concrete Columns Using High-Strength Materials, Part 3: Outline of Experiment (超高強度材料を用いた鉄筋コンクリート造の柱部材に関する実験 研究, その3: 実験概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 2000, pp. 191-192. (in Japanese)

32. Inanaga, E.; Oi, T.; Chiba, O.; Ishikawa, K., Yamauchi, M.; Izumi, N.; and Kikuta, S., “Experimental Study on Behavior of Reinforced Concrete Columns Using High-Strength Materials, Part 4: Outline of Experimental Results (超高強度材料を用いた鉄筋コンクリート造の 柱部材に関する実験研究, その4: 実験結果の概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 2000, pp. 193-194. (in Japanese)

33. Takenaka, H.; Okamoto, M.; Chiba, O.; Yamauti, S.; and Kikuta, S., “Experimental Study on Behavior of Reinforced Concrete Columns Using High-Strength Materials, Part 1: Outline of Experiment (超高強度 材料を用いた鉄筋コンクリート造の柱部材に関する実験研究, その 1: 実験概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1996, pp. 171-172. (in Japanese)

34. Kikuta, S.; Okamoto, M.; Chiba, O.; Takenaka, H.; and Yamauti, S., “Experimental Study on Behavior of Reinforced Concrete Columns Using High-Strength Materials, Part 2: Outline of Experimental Results (超高強度材料を用いた鉄筋コンクリート造の柱部材に関する実験 研究, その2: 実験結果の概要),” Summaries of Technical Papers of the Annual Meeting of the Architectural Institute of Japan, C-2, Structures IV, 1996, pp. 173-174. (in Japanese)

35. ACI Committee 369, “Standard Requirements for Seismic Evaluation and Retrofit of Existing Concrete Buildings (ACI 369.1-17) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2017, 110 pp.

36. Ghannoum, W.; Sivaramakrishnan, B.; Pujol, S.; Catlin, A.C.; Fernando, S.; Yoosuf, N.; and Wang, Y., “NEES: ACI 369 Rectangular Column Database,” 2015, https://datacenterhub.org/resources/255.

37. Matamoros, A.B., “Study of Drift Limits for High-Strength Concrete Columns,” PhD thesis, Department of Civil Engineering, University of Illinois at Urbana-Champaign, Urbana, IL, 1999, 484 pp.

38. Rautenberg, J., “Drift Capacity of Concrete Columns Reinforced with High-Strength Steel,” PhD thesis, Department of Civil Engineering, Purdue University, West Lafayette, IN, 2011, 289 pp.

39. Sokoli, D., and Ghannoum, W., “High-Strength Reinforcement in Columns Under High Shear Stresses,” ACI Structural Journal, V. 113, No. 3, May-June 2016, pp. 605-614.

40. ACI Committee 374, “Guide to Nonlinear Modeling Parameters for Earthquake-Resistant Structures (ACI 374.3R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 13 pp.

41. “Minimum Design Loads for Buildings and Other Structures (ASCE/SEI 7-16),” American Society of Civil Engineers, Reston, VA, 2017, 690 pp.

42. “Administrative Bulletin 83: Requirements and Guidelines for the Seismic Design of New Tall Buildings Using Non-Prescriptive Seismic- Design Procedures,” San Francisco Department of Building Inspection, San Francisco, CA, Mar. 25, 2008, 8 pp.

43. “An Alternative Procedure for the Analysis and Design of Tall Buildings Located in the Los Angeles Region: A Consensus Document,” Los Angeles Tall Buildings Structural Design Council, Los Angeles, CA 2014, 51 pp.

44. “Minimum Design Loads for Buildings and Other Structures (ASCE/SEI 7-10),” American Society of Civil Engineers, Reston, VA, 2010, 650 pp.

45. Macchi, G.; Pinto, P.E.; and Sanpaolesi, L., “Ductility Requirements for Reinforcement under Eurocodes,” Structural Engineering International, V. 6, No. 4, 1996, pp. 249-254.

46. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

47. Richter, B.P., “A New Perspective on the Tensile Strength of Lap Splices in Reinforced Concrete Members,” MS thesis, Purdue University, West Lafayette, IN, 2012.