State of the Art of Steel Reinforced Grout Applications to Strengthen Masonry Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: State of the Art of Steel Reinforced Grout Applications to Strengthen Masonry Structures

Author(s): Gianmarco de Felice, Stefano De Santis, Roberto Realfonzo, Annalisa Napoli, Francesco Ascione, Elena Stievanin, Elvis Cescatti, Maria Rosa Valluzzi, Christian Carloni, Mattia Santandrea, Guido Camata

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 102.1-102.12

Keywords: arches; columns; confinement; field test; laboratory investigation; seismic retrofitting; out-of-plane

DOI: 10.14359/51711085

Date: 8/10/2018

Abstract:
Load-bearing unreinforced masonry structures represent a significant proportion of the building stock in several countries worldwide, and include historical constructions that belong to cultural heritage. Because of the limited tensile strength of unreinforced masonry, fiber-reinforced composites are an effective strengthening technique, which has already been widely used, especially in seismic prone areas, to delay the onset of collapse mechanisms of the entire structure or portions of it. Steel reinforced grout (SRG), which consists of steel textiles embedded in a cement or lime based mortar, is a particularly appealing alternative to fiber-reinforced polymer (FRP) composites, as well as to other mortar based composites (i.e., fabric reinforced cementitious matrix, FRCM), especially when applied to masonry structures. This paper sheds light into the retrofitting of masonry structures with SRG, providing an overview of the experimental investigations carried out in the laboratory and in the field on full-scale structural members. SRG proved effective for improving the out-of-plane flexural strength and deflection capacity of masonry walls (for which three or four-point bending tests and shake table tests were performed), the load-bearing and deflection capacity of vaults (tested both in the laboratory and in the field under quasi-static vertical loads), and the compressive strength of columns (subjected in the laboratory to centred axial load). Further research needs are identified, which are considered useful for the development of design guidelines.

Related References:

1. Valluzzi, M.R., Modena, C., de Felice, G., “Current practice and open issues in strengthening historical buildings with composites”, Materials and Structures, V. 47, No. 12, 2014, pp.1971-1985.

2. Papanicolaou C.G., Triantafillou T.C., Papathanasiou M., Karlos K., “Textile-reinforced mortar (TRM) versus FRP as strengthening material of URM walls: out-of-plane cyclic loading”, Materials and Structures, V. 41, No. 1, 2008, pp. 143-157.

3. De Santis S., de Felice G., Napoli A., Realfonzo R., “Strengthening of structures with Steel Reinforced Polymers: A state-of-the-art review”, Composites Part B: Engineering, V. 104, 2016, pp. 87-110.

4. Razavizadeh, A., Ghiassi, B., Oliveira, D.V., “Bond behavior of SRG-strengthened masonry units: Testing and numerical modeling”, Construction and Building Materials, V. 64, 2014, pp. 387-397.

5. Grande, E., Imbimbo, M., Sacco, E., “Investigation on the bond behavior of clay bricks reinforced with SRP and SRG strengthening systems”, Materials and Structures, V. 48, No. 11, 2015, pp. 3755-3770.

6. De Santis, S., “Bond behaviour of Steel Reinforced Grout for the extrados strengthening of masonry vaults”, Construction and Building Materials, V. 150, 2017, pp. 367-382.

7. De Santis S., Ceroni F., de Felice G., Fagone M., Ghiassi B., Kwiecien A., Lignola G.P., Morganti M., Santandrea M., Valluzzi M.R., Viskovic A., “Round Robin Test on tensile and bond behaviour of Steel Reinforced Grout systems”. Composites Part B: Engineering, V. 127, 2017, pp. 100-120.

8. de Felice G., De Santis S., Lourenço P.B., Mendes N., “Methods and challenges for the seismic assessment of historic masonry structures”. International Journal of Architectural Heritage, V. 11, No. 1, 2017, pp. 143-160.

9. ACI (American Concrete Institute). (2013). “ACI 549.4R-13 Guide to design and construction of externally bonded Fabric-Reinforced Cementitious Matrix (FRCM) systems for repair and strengthening concrete and masonry structures.” Farmington Hills, MI, US.

10. Kerakoll S.p.A. – web site: http://www.kerakoll.com/ accessed Nov 2017..

11. Valluzzi, M.R., Da Porto, F., Garbin, E., Panizza, M., “Out-of-plane behavior of infill masonry panels strengthened with composite materials”, Materials and Structures, V. 47, No. 12, 2014, pp. 2131-2145.

12. Bellini, A., Incerti, A., Bovo, M., Mazzotti, C., “Effectiveness of FRCM Reinforcement Applied to Masonry Walls Subject to Axial Force and Out-Of-Plane Loads Evaluated by Experimental and Numerical Studies”, International Journal of Architectural Heritage, 2017, In Press.

13. De Santis S., Casadei P., De Canio G., de Felice G., Malena M., Mongelli M., Roselli I., “Seismic performance of masonry walls retrofitted with steel reinforced grout”, Earthquake Engineering and Structural Dynamics, V. 45, No. 2, 2016, pp. 229-251.

14. De Canio G., de Felice G., De Santis S., Giocoli A., Mongelli M., Paolacci F., Roselli I., “Passive 3D motion optical data in shaking table tests of a SRG-reinforced masonry wall”, Earthquakes and Structures, V. 10, No. 1, 2016, pp. 53-71.

15. De Santis, S., De Canio, G., de Felice, G., Fantauzzi, D., Focaccetti, E., Roselli, I., “Seismic out-of-plane vertical bending behaviour of masonry walls reinforced with textile reinforced mortars”, International Masonry Conference, Milan, Italy, July 9-11, 2018.

16. Borri, A., Casadei, O., Castori, G., Hammond, J., “Strenghtening of Brick Masonry Arches with Externally Bonded Steel Reinforced Composites”, Journal of Composites for Construction, V. 13, No. 6, 2009, pp. 468-475.

17. Girardello, P., Pappas, A., Da Porto, F., Valluzzi, M.R., “Experimental testing and numerical modelling of masonry vaults”, International Conference on Rehabilitation and Restoration of Structures, Chennai, India, February 13-16, 2013.

18. Garmendia, L., Larrinaga, P., San-Mateos, R., San-José, J.T., “Strengthening masonry vaults with organic and inorganic composites: an experimental approach”, Materials & Design, V. 85, 2015, pp. 102-114.

19. De Santis, S., Roscini, F., de Felice, G., “Full-scale tests on masonry vaults strengthened with Steel Reinforced Grout”, Composites Part B: Engineering, 2017.

20. Cescatti, E. “Combined experimental and numerical approaches to the assessment of historical masonry structures”. PhD Thesis, University of Trento, 2016.

21. Cescatti, E., da Porto, F., Modena, C., “In-Situ Destructive Testing of Ancient Strengthened Masonry Vaults”, International Journal of Architectural Heritage, V. 12, No. 3, 2018, pp. 350-361. .

22. Sneed, L.H., Carloni, C., Baietti, G., Fraioli, G., “Confinement of clay masonry columns with SRG”, Key Engineering Materials, V. 747, 2017, pp. 350-357.

23. Santandrea, M., Quartarone, G., Carloni, C., Gu, X. “Confinement of masonry columns with steel and basalt FRCM composites”, Key Engineering Materials, V. 747, 2017, pp. 342-349.

24. Capozucca, R., “Double-leaf masonry walls under in-plane loading strengthened with GFRP/SRG strips”, Engineering Structures, V. 128, 2016, pp. 453-473.