Title: Flexural Behavior of Corroded RC Beams

Author(s): Giuseppe Campione, Francesco Cannella, Piero Colajanni, and Maurizio Papia

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 91.1-91.10

Keywords: shear-moment interaction; corrosion; bond; pitting; load-deflection response

DOI: 10.14359/51711074

Date: 8/10/2018

Abstract:
A handily model to evaluate the bending resistance and the ductility of corroded beams critical in flexure and shear is proposed and debated. Effects of diffused and pitting corrosion on steel bars, compressive concrete strength reduction and concrete bond strength reduction due to rust creation are modelled. Practical method derived on limit state theory was here used to calculate the flexural and shear strength and the available ductility. The effectiveness of the model was also corroborated against numerous results collected in the literature pertaining to bending and shear resistance.

Related References:

1. Saetta A V, Vitaliani R V., “Experimental investigation and numerical modeling of carbonation process in reinforced concrete structures Part I: Theoretical formulation”, Cement and Concrete Research, V. 34, 2004, pp. 571–579

2. Saetta A V, Vitaliani R V., “Experimental investigation and numerical modeling of carbonation process in reinforced concrete structures. Part II: Practical applications”, Cement and Concrete Research, V. 35, 2005, pp. 958–967

3. Coronelli D, Gambarova P., “Structural assessment of corroded reinforced concrete beams: modeling guidelines”, ASCE J. Struct. Eng., V. 130, No. 8, 2004, pp. 1214-1224.

4. Ting S, and Nowak A., “Effect of reinforcing steel area loss on flexural behavior of RC beams”, ACI J. Struct Eng., V. 88, No. 3, 1991, pp. 309–314.

5. Al-Sulaimani G J, Kaleemullah M, Basumbul I A, and Rasheeduzzafar, “Influence of corrosion and cracking on bond behavior and strength of reinforced concrete members”, ACI Struct. J., V. 87, 1991, pp. 220–231.

6. Rodriguez J, Ortega L, and Garcia A., “Corrosion of reinforcing bars and service life of R/C structures: Corrosion and bond deterioration”, Proc., Int. Conf. on Concrete across Borders, V. 2, 1994, pp. 315– 326.

7. Coronelli D., “Corrosion cracking and bond strength modeling for corroded bars in reinforced concrete”, ACI Struct. J., V. 99, No. 3, 2002, pp. 267–276.

8. Coronelli D, Kamyab Z H, Lundgren K., “Severely corroded RC with cover cracking”, J. Struct. Eng., V. 139, No. 2, 2013, pp. 221–232.

9. Rodriguez J, Ortega L, Casal J., “Load carrying capacity of concrete structures with corroded reinforcement”, 4th Int. Conf. on Structure Faults and Repair, M. Forde, ed., Engineering Tech. Press, Edinburgh U.K., 1995, pp. 189–199.

10. Rodriguez J, Ortega M, Casal J. “Load bearing capacity of concrete columns with corroded reinforcement”, Proc., 4th Int.Symp. on Corrosion of Reinforcement in Concrete Construction, C. L.Page, P. B. Bamforth, J. W. Figg, eds., The Royal Society of Chemistry, Cambridge, U.K., 1995.

11. Rodriguez J, Ortega L M, Casal J., “Load carrying capacity of concrete structures with corroded reinforcement”, Constr. Build. Mater., V. 11, No. 4, 1997, pp.239–248.

12. Campione G., Cannella F., Cavaleri L., “Shear and flexural strength prediction of corroded R.C. beams”, Construction and Building Materials, V. 149, 2017, pp. 395–405.

13. Khan I., Francois R., Castel A., “Experimental and analytical study of corroded shear-critical reinforced concrete beams” Materials and Structures , V. 47, 2014, pp 1467-1481.

14. Almusallam A.A., “Effect of degree of corrosion on the properties of reinforcing steel bars”, Construction and Building Materials, V.15, No. 8, 2001, pp. 361-368.

15. Val D V., “Deterioration of Strength of RC Beams due to Corrosion and Its Influence on Beam Reliability”, ASCE J. Struct. Eng., V. 133, No. 9, 2007, pp. 1297-1306.

16. Gonzalez J A, Andrade C, Alonso C, Feliu S. “Comparison of rates of general corrosion and maximum pitting penetration on concrete embedded steel reinforcement”, Cement and Concrete Research, V. 25, No. 2, 1995, pp. 257-264.

17. Molina F., J., Alonzo C. and Andrade C., “Cover cracking s a function of rebars corrosion: part II- numerical model”, Materials and structures, V.26, No. 163, 1993, pp.532-548.

18. MacGregor, J. G. (1997), “Reinforced concrete: Mechanics and design”, 3rd Ed., Prentice-Hall, Upper Saddle River, N.J.

19. Colajanni, P., La Mendola, L., Recupero, A., Spinella, N., “Stress field model for strengthening of shear-flexure critical RC beams”, Journal of Composites for Construction, 2017, V. 21, No. 5, art. no. 04017039.

20. Campione Colajanni Monaco, “Analytical evaluation of steel–concrete composite trussed beam shear capacity”, Materials and Structures, V. 49, No. 8, August 2016, pp. 3159-3176

21. Ou Y.C., Chen H.H. (2014), “Cyclic behaviour of reinforced concrete beams with corroded transverse steel reinforcement”, ASCE Structural Journal ISNN0733-9445/04014050(10).