Forecasting Durability of Reinforced Concrete Structures Under Weathering

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Forecasting Durability of Reinforced Concrete Structures Under Weathering

Author(s): Gusev Boris Vladimirovich and Fayvusovich Alexander Solomonovich

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 79.1-79.8

Keywords: concrete, corrosion, degradation, double porosity system, moving boundary, phase transitions

DOI: 10.14359/51711062

Date: 8/10/2018

Abstract:

The engineering method presented in this article is based on mathematical models and theoretical and practical research conducted by the authors, including the results of their quantitative modelling.

The increase in forecasting precision and the provision of application simplicity are achieved through the improvement of the model and through linearization of initial equations. It is recommended to determine the initial data for the calculations based on the distribution of corrosion products along the depth of used structures.

Related References:

1. Lykov A.V., Theory of Heat Conductivity. M.:High School. 1967.- 600 p.

2. Vagelis G., Papadakis, “Service life prediction of a reinforced concrete bridge exposed to chloride induced deterioration”, Advances in Concrete Construction, V. 1, No. 3, 2013.

3. Czarnecki L., Woyciechowski P., “Modelling of concrete carbonation: is it a process unlimited in time and restricted in space”, Bulletin of the Polisch, V. 63, No. 1, 2015, p.43-54.

4. Ekolu O.S., “Towards Practical Carbonation of Reinforced Concrete Structure”, IOP Conference Series Material Science and Engineering – IOP Publishing, V.96, No. 1, pp. 12-65.

5. Hack L.I., Koher I., “Modelling the special-temporal progression of corrosion with special emphatic on its influence on structural reliability”, ABSE Symposium Report-International Association for Bridge and Structural Engineering, V.103, No. 4, 2015, pp.152 – 159

6. Hokst Y.F., Wittman F.H., “Depth profiles of carbonates formed during natural carbonation”, Cement and concrete research, V. 32, No. 12, 2002, pp.1923 – 1930.

7. Woyciechowski P.P., Sokolowska I.I., “Self – Terminated Carbonation Model as Useful Support for Durable Concrete Designing”, The 2016. Structures Congress (Structures 16 August 28 – September 1, 2016).

8. Villain G., Thiery M., Platret G., “Measurement methods of carbonation profiles in concrete thermogravimetry, chemical analysis and gammadensimetry”, Cement and Concrete Research, V.37, No 8, 2007, pp. 1188 – 1192.

9. Muntean A.A., et.al., “A note on limitation of the use of accelerated concrete-carbonation test for service life predictions” – 2005

10. Wan – Hu Tsao, Miny – Te Liang and Ta – Peng Chang, “Chloride – binding isotherms in Concrete Submitted to non-steady – State Diffusion – Migration Model”, Journal of Marine Science and Technology, V. 24, No.4, 2016, pp 822 – 831.

11. Liang M.T., Huang P.S., Iheng H.I., “Reconsideration for a study of the effect of chloride binding on service life predictions”, Journal of Marine Science and Technology, V. 1, No. 3, 2011, p. 531 – 540.

12. Liang M.T. et.al. “Revisited to relationship between the free and total chloride diffusely in concrete”, Journal of Marine Science and Technology, V. 18, No. 3, 2010, pp. 442 – 448.

13. Liang M.T. et.al. “Studies of the Effect of Diffusion – Induced Chloride Binding on chlorination Life Predictions for Existing Reinforced Concrete Bridges”, Journal of Marine Science and Technology, V. 20, No.4, 2012, pp. 418 – 430.

14. Geng I. et.al. “Effect of carbonation on release of bound chlorides in chloride–contaminated concrete”, Magazine of Concrete Research, V. 63, No. 7, 2016, pp. 353 –363.

15. Zhou Y. et.al. “Carbonation–induced and chloride–induced corrosion in reinforced concrete structures”, Journal of Materials in Civil Engineering, V.27, No. 9, 2014, pp. 04014245.

16. Lin I. et.al. “Chloride transport and microstructure of chloride with cutout fly ash under atmospheric chloride condition”, Construction and Building Materials, V. 146, 2017, pp. 493 – 501.

17. Iones S. et.al. “Simulations Studies of methods to delay corrosion and increase service life for cracked concrete exposed to chlorides”, ?ement and Concrete Composites, V. 58, 2015, pp. 59-69.

18. Zhu K. et.al, “Combined of carbonation and chloride ingress in concrete”, Construction and Building Materials, V. 110, 2016, pp.369 – 380.

19. Barenblatt G.I. Zheltov Yu. P., Kochina I.N., “On basics of filtration theory for homogeneous liquids in fractured rocks’, PMM., V. 24, No.5, 1960, pp. 852 – 864.

20. Gusev B.V., Faivusovich A.S., “Mathematical model of concrete atmospheric corrosion with regard to phase transitions”, Volgograd University. Series: Construction and Architecture, 2013, No.31-3. pp. 308 – 325.

21. Gusev B.V., Faivusovich A.S., “Forecasting of concrete durability when leaching”, Nauchny Mir. M.: 2014–109p.