Title: Methodology of Long-Term Concrete Tests for Bending

Author(s): Petr Arleninov, Sergey Krylov, and Dmitry Kuzevanov

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 78.1-78.6

Keywords: Calculation of structures, concrete, creep, deformations, reinforced concrete, non-liner calculation

DOI: 10.14359/51711061

Date: 8/10/2018

Abstract:
Two main novelties are proposed in this article: the first is an introduction that details deformation characteristics — long-term modulus of concrete elasticity during bending and its differentiation, and the second is the proposed simplified method for creep testing during the bending mode with the further matching of results with classic testing for compression in spring test rigs.