Ductility Index and Durability in Fiber-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductility Index and Durability in Fiber-Reinforced Concrete

Author(s): Andrea Gorino, Alessandro P. Fantilli, Bernardino Chiaia, Davide Zampini, Alexandre Guerini, and Giovanni Volpatti

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 59.1-59.10

Keywords: fiber-reinforced concrete; three-point bending tests; ductility index; water penetration tests; concrete durability

DOI: 10.14359/51711042

Date: 8/10/2018

Abstract:
To investigate the flexural behavior of fiber-reinforced concrete beams, even in the presence of traditional steel rebar, an experimental campaign has been carried out performing three-point bending tests. Conventional raw materials have been used to cast the concretes, which contain different amounts of steel fibers combined, in some cases, with a fixed amount of rebar. In addition, the use of a patented high performance self-compacting fiber-reinforced concrete mixture has been analyzed. In all these cases, the ductility index, measured on the experimental load-deflection curves and used to assess the brittle/ductile behavior of the beams, can also be correlated with some durability parameters. Specifically, better fresh properties of concrete and the increment of flexural ductility improve the resistance to water penetration. In other words, the higher the ductility index the longer the beam durability measured in accordance with major standards.

Related References:

1. Caratelli, A., Meda, A., Rinaldi, Z., “Design according to MC2010 of a fibre-reinforced concrete tunnel in Monte Lirio, Panama,” Structural Concrete, V. 13, 2012, pp. 166-173.

2. de la Fuente, A., Pujadas, P., Blanco, A., Aguado, A., “Experiences in Barcelona with the use of fibres in segmental linings,” Tunnelling and Underground Space Technology, V. 27, 2012, pp. 60-71.

3. Tiberti, G., Minelli, F., Plizzari, G.A., “Reinforcement optimization of fiber reinforced concrete linings for conventional tunnels,” Composites: Part B, V. 58, 2014, pp. 199-207.

4. Chiaia, B., Fantilli, A.P., Vallini, P., “Combining fiber-reinforced concrete with traditional reinforcement in tunnel linings,” Engineering Structures, V. 31, 2009, pp. 1600-1606.

5. fib, “Model Code 2010 - Final draft, Volume 1,” fib Bulletin 65, International Federation for Structural Concrete, Lausanne, 2012.

6. ACI “318-14: Building Code Requirements for Structural Concrete and Commentary,” American Concrete Institute, Farmington Hills, 2014.

7. Fantilli, A.P., Chiaia, B., Gorino, A., “Minimum reinforcement and ductility index of lightly reinforced concrete beams,” Computers and Concrete, V. 18, No. 6, pp. 1175-1194.

8. Fantilli, A.P., Chiaia, B., Gorino, A., “Fiber volume fraction and ductility index of concrete beams,” Cement and Concrete Composites, V. 65, 2016, pp. 139-149.

9. Fantilli, A.P., Chiaia, B., Gorino, A., “A unified approach for the minimum reinforcement of concrete beams,” ACI Structural Journal, V. 113, No. 05, 2016, pp. 1107-1116.

10. Gorino, A., Fantilli, A.P., Chiaia, B., Zampini, D., Guerini, A., Volpatti, G., “Brittle vs. ductile behavior of concrete beams reinforced with steel rebars and fibers.” Proc. 9th Rilem International Symposium on Fiber Reinforced Concrete (BEFIB 2016), Vancouver, 2016, pp. 1263-1274.

11. Bayasi, M.Z., Soroushian, P., “Effect of steel fiber reinforcement on fresh mix properties of concrete,” ACI Materials Journal, V. 89, 1992, pp. 369-374.

12. Kuder, K.G., Ozyurt, N., Mu, E.B., Shah, S.P., “Rheology of fiber-reinforced cementitious materials,” Cement and Concrete Research, V. 37, 2007, pp. 191-199.

13. Basheer, L., Kropp, J., Cleland, D.J., “Assessment of the durability of concrete from its permeation properties: a review,” Construction and Building Materials, V. 15, 2001, pp. 93-103.

14. Guerini, A., Volpatti, G., Zampini, D., “Patent PCT/EP2015/063045,” 2015 (Commercially available as Cemex® Resilia®).

15. CEN, “EN 12350-8: Testing fresh concrete - Part 8: Self-compacting concrete - Slump-flow test,” European Committee for Standardization, Brussels, 2010.

16. CEN, “EN 12350-7: Testing fresh concrete - Part 7: Air content - Pressure methods,” European Committee for Standardization, Brussels, 2000.

17. CEN, “EN 12390-8: Testing hardened concrete - Part 8: Depth of penetration of water under pressure,” European Committee for Standardization, Brussels, 2000.

18. CEN, “EN 12390-3: Testing hardened concrete - Part 3: Compressive strength of test specimens,” European Committee for Standardization, Brussels, 2001.

19. Maldague, J.C., “Établissement des Lois Moments-Courbures,” Annales de l'Institut Technique du Batiment et des Travaux Publics, V. 213, 1965, pp. 1170-1218.