Suitability of Recycled Aggregate as a Replacement for Natural Aggregate in Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Suitability of Recycled Aggregate as a Replacement for Natural Aggregate in Construction

Author(s): Deb Dulal Tripura, Shubham Raj, Sher Mohammad, and Rima Das

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 37.1-37.10

Keywords: recycled concrete aggregate; interfacial transition zone; unconfined compressive strength; splitting tensile strength; modulus of rigidity, bond strength

DOI: 10.14359/51711019

Date: 8/10/2018

Abstract:
This study investigates the effect of recycled coarse aggregate (RCA) as replacement of natural coarse aggregate on the strength properties of concrete. The investigation was carried out by conducting unconfined compressive strength (UCS) test, indirect tensile strength (ITS) test, flexural strength test and bond strength test on five concrete mixtures using 0%, 25%, 50%, 75% and 100% by weight of RCA as replacement of natural coarse aggregate. The test samples were prepared with a target strength of 40 MPa (6000 psi). Water-cement ratio (w/c) and slump was adopted as 0.40 and 100 mm (4.0 in.) respectively. It was observed that as the percentage of RCA in concrete mixtures increased, the strength properties of concrete decreased. There was a decrease of 1.92%, 5.43%, 10.46% and 27.13% in UCS for RCA 25%, 50%, 75% and 100% respectively. Tensile strength of concrete decreased considerably on addition of RCA. All samples achieved target strength except 100% replacement. Also, as the percentage of RCA increased in concrete mixtures, the rate of strength gain over time decreased. However, RCA can be efficiently used as a replacement of natural coarse aggregate up to 25% without any major laboratory testing and up to 50% with proper testing and care for concreting where high strength is not a priority.

Related References:

1. Ministry of Natural Resources, 2010, “State of the aggregate resource in Ontario study – consolidated report”, Ontario Ministry of Natural Resources, Ontario.

2. Centre for Science and Environment, 2014, “Construction and Demolition Waste”, New Delhi. http://www.cseindia.org/userfiles/Construction-and%20-demolition-waste.pdf (accessed on 6th May, 2017)

3. Faleschini, F., Zanini, M.A., and Pellegrino, C., 2016, “Environmental impacts of recycled aggregate concrete”, Evolution and Sustainability of the Concrete Structures, Italian Concrete Days Aicap CTE Congress, Rome.

4. Ismail, S., and Ramli, M., 2013, “Engineering properties of treated recycled concrete aggregate for structural applications”, Construction and Building Materials, 44(7), 464–476.

5. Zhang, J., Shi, C., Li, Y., Pan, X., Poon, C.S., and Xie, Z., 2015, “Performance Enhancement of Recycled Concrete Aggregates through Carbonation”, Journal of Materials in Civil Engineering, 27(11), 04015029.

6. Butler, L.J., West, J.S., and Tighe, S.L., 2014, “Towards the classification of recycled concrete aggregates: influence of fundamental aggregate properties on recycled concrete performance”, Journal of Sustainable Cement-Based Materials, 3(2), 140-163.

7. Neville, A.M., 2011, “Properties of concrete”, Pearson Education Limited, 5th edition, Essex CM20 2JE, England.

8. Ayob, A., Razali, M.E., Alias, S., Ahmad, A.G., and Ali, D.S.H., 2017, “Engineering Behavior of Concrete with Recycled Aggregate”, MATEC Web of Conferences, 87, 01002.

9. Jebli, M., Jamin, F., Malachanne, E., Garcia-Diaz, E., and Youssoufi, M.S. EI, 2018, “Experimental characterization of mechanical properties of the cement-aggregate interface in concrete”, Construction and Building Materials, 161, 16-25.

10. Liu, Q., Xiao, J., and Sun, Z., 2011, “Experimental study on the failure mechanism of recycled concrete”, Cement and Concrete Research, 41, 1050-1057.

11. Indian Standard, 2005, “Specification for 43 grade ordinary Portland cement”, IS 8112, New Delhi, India.

12. Indian Standard, 2009, “Concrete mix proportioning-guidelines”, IS 10262, New Delhi, India.

13. Indian Standard, 2006b, “Specification for determination of unconfined compressive strength of stabilized soils”, IS 4332 (Part 5), New Delhi, India.

14. Indian Standard, 1999, “Splitting tensile strength of concrete- Method of test”, IS 5816, New Delhi, India.

15. Indian Standard, 1967, “Methods of testing bond in reinforced concrete part 1 pull-out test”, IS 2770 (Part 1), New Delhi, India.

16. Indian Standard, 1959, “Methods of tests for strength of concrete”, IS 516, New Delhi, India.

17. Kwan, W.H., Ramli, M., Kam, K.J., and Sulieman, M.Z., 2012, “Influence of the amount of recycled coarse aggregate in concrete design and durability properties”, Construction and Building Materials, 26(1), 565-573.

18. Xiao, J., Li, J., and Zhang, C., 2005, “Mechanical properties of recycled aggregate concrete under uniaxial loading”, Cement and Concrete Research, 35(6), 1187–1194.

19. Lotfy, A., and Al-Fayez, M., 2015, “Performance evaluation of structural concrete using controlled quality coarse and fine recycled concrete aggregate”, Cement and Concrete Composites, 61, 36-43.

20. Sagoe-Crentsil, K.K., Brown, T., and Taylor A.H., 2001, “Performance of concrete made with commercially produced coarse recycled concrete aggregate”, Cement and. Concrete Research, 31, 707–712.

21. Ajdukiewicz, A., and Kliszczewicz, A., 2002, “Influence of recycled aggregates on mechanical properties of HS/HPC”, Cement and Concrete Composites, 24, 269–279.

22. Muscalu, M.T., and Andrei, R., “Use of recycled aggregates in rigid pavement construction”, Buletinul Institutului Politehnic din iasi, Tomul LVII (LXI), Fasc. 2.

23. Won, M.C., 1999, “Use of Crushed Concrete as Aggregate for Pavement Concrete”, Research Section, Construction Division, Texas Department of Transport, Texas, USA.

24. Shayan, A., and Xu, A., 2002, “Performance and properties of structural concrete made with recycled concrete aggregate”, ACI Material Journal, 100, 371–380.