Performance of Calcium Sulphoaluminate Cement for Fast Concrete Repair: Real-Scale Test Results

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance of Calcium Sulphoaluminate Cement for Fast Concrete Repair: Real-Scale Test Results

Author(s): Sergio Tortelli and Maurizio Marchi

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 35.1-35.10

Keywords: calcium sulfoaluminate cement; fast-hardening concrete; blended cement performance

DOI: 10.14359/51711017

Date: 8/10/2018

Abstract:

The recent years’ enhancement of traffic on roads and airport runways put under the spotlight some new emerging needs such as the necessity of fast and reliable materials for roads and infrastructure maintenance, so as to minimize the shutdown periods and the related issues. In the same ages, the enhanced environmental consciousness led to an increase search of the eco-friendly solutions, so as to minimize the effect of the climate changes caused by the human activities.

The use of an innovative type of binder such as the Calcium Sulphoaluminate Cement (CSA) could be the right answer to both the issues, since it couples the benefits of a rapid-hardening cement with an outstanding C02 emission reduction with respect to ordinary portland cement (OPC).

This paper presents the performance at laboratory and industrial scale of a CSA-based concrete mixture designed to meet extremely strict requirements in terms of mechanical resistance evolution and durability, such as the case of highways or airport runways repair, in order to minimize the closing time and the bother related to the infrastructure serviceability interruption, even at low temperatures.