Flexural Response of Reinforced Concrete Beams Strengthened with Near-Surface-Mounted Fe-Based Shape-Memory Alloy Strips

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Response of Reinforced Concrete Beams Strengthened with Near-Surface-Mounted Fe-Based Shape-Memory Alloy Strips

Author(s): Kinam Hong / Sugyu Lee / Yeongmo Yeon / Kyusan Jung

Publication: IJCSM

Volume: 12

Issue:

Appears on pages(s):

Keywords: NSM reinforcing method, prestressed strengthening material, Fe-SMA strip, pre-straining level,

DOI:

Date: 6/30/2018

Abstract:
This paper proposes an advanced near-surface-mounted (NSM) technique with an Fe-based shape-memory alloy (Fe-SMA) strip which can solve issues of low workability and reduced ductility of reinforced concrete (RC) beams strengthened with an NSM technique using prestressed fiber-reinforced polymer (FRP) strips in the concrete tension section. The flexural behavior of the RC beam strengthened by the NSM technique with the Fe-SMA strip was investigated. A total of seven RC beams were tested by four-point bending tests under displacement control. The type of reinforcements, the quantity of Fe-SMA strips, and the pre-straining level of the Fe-SMA strips were considered as experimental variables. Cracking load, yielding load, and ultimate load increased, respectively, with larger quantities of Fe-SMA strip. In addition, activation of embedded Fe-SMA in the concrete by electrical resistance heating effectively induces a prestressing force on the concrete beam, resulting in a cambering effect. The introduced prestressing force to the RC beam by activation of the Fe-SMA increased the crack and yielding loads, and did not decrease the ductility of the RC beam compared to the RC beam with non-activated Fe-SMA. It can be concluded from the test results that the strengthening technique using the recovery stress of the Fe-SMA strip as the prestressing force solves the various problems of the existing prestressing strengthening systems, meaning that Fe-SMA can be used as a substitute for conventional prestressing strengthening systems.