Title: Modification of Mineral Additives when Treating their Suspensions in Different Cavitators

Author(s): Gusev B.V, Bondarenko I.V., and Olenich D.I.

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 11.1-11.6

Keywords: cavitational apparatuses, fillers, hydrodynamic radiators, mineral additives, ultrasound oscillations

DOI: 10.14359/51710981

Date: 8/10/2018

Abstract:
Grinding, emulsion and suspension activation using ultrasound oscillations are widely used around the world. In the recent years, hydrodynamic radiators (rotor and pulse devices (RPD) and various cavitational apparatuses). The authors formulated the idea of and received the patent for using mineral additives - which all have a higher degree of dispersion in nano-sized terms- as fillers. The article presents activation and dispersion methods for mineral filler additives.

Related References:

1. Gusev B.V., Vasilyev V.G., Toyshibayev N.K. Activity of the cement stone treated by a hydrodynamic method. "Concrete and Reinforced Concrete". 1991, No. 6. P. 10-11.

2. Gusev B.V., Yudayev V.F. Mechanism for cement cavitation activation. "Construction Materials, Equipment. Technologies of the 21st century". 2003, No. 6, p.24-25.

3. Gusev B.V., Minsadrov I.N., Selivanov N.P. Nanobinders//Patent of the Russian Federation No. 2412919. - 2009.

4. Nanoscience and nanotechnologies. Encyclopedia of the life support systems. Moscow, UNESCO, EOLSS 2009, 992 p.