Finishing the Sidewalk Scaling Situation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Finishing the Sidewalk Scaling Situation

Author(s): Henry B. Prenger

Publication: Concrete International

Volume: 40

Issue: 8

Appears on pages(s): 36-38

Keywords: finishing, curing, scaling, slag cement

DOI: 10.14359/51710890

Date: 8/1/2018

Abstract:
Extreme winter weather in Maryland in 1993 caused widespread sidewalk scaling. The damage prompted a long-term study of the causes of deterioration. Many of the problems witnessed are the result of premature finishing of extremely slow setting concrete in cold temperatures or using water as a finishing aid in hot temperatures.

Related References:

1. Sutter, L.L.; Van Dam, T.J.; Peterson, K.R.; and Johnston, D., “Long Term Effects of Magnesium Chloride and Other Concentrated Salt Solutions on Pavement and Structural Portland Cement Concrete – Phase I Results,” Journal of the Transportation Research Board, Transportation Research Board, V. 1979, 2006, pp. 54‐59.