Title: Prestressing looses due to creep and relaxation: Theory and experimental verification

Author(s): Sánchez Gálvez, V.; Elices Calafat, M.

Publication: ACHE

Volume: 36

Issue: 155

Appears on pages(s): 82 -

Keywords:

DOI:

Date: 1/3/1985

Abstract: