Numerical and experimental evaluation of the dynamic response of a fibre reinforced polymers (FRP) lighthouse

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical and experimental evaluation of the dynamic response of a fibre reinforced polymers (FRP) lighthouse

Author(s): José David Jiménez Vicaria, Pablo Sánchez Sierra, Eva Martínez Barrigüete, Carlo Paulotto

Publication: ACHE

Volume: 68

Issue: 282

Appears on pages(s): 121 - 128

Keywords: Fibre reinforced polymers, Lighthouse, Free vibrations, Dynamic response, Numerical simulation

DOI:

Date: 5/1/2017

Abstract:
A 32-metre high lighthouse, made entirely with fibre reinforced polymers (FRPs), was manufactured by ACCIONA Infrastructure in Madrid, and was installed in only two hours in the northern extension of the Port of Valencia in February 2015. Once the FRP lighthouse was installed, its wind induced vibrations were recorded by a set of accelerometers, strategically placed to determine its dynamic response. Previously, a numerical simulation of the structure was performed to assess its natural frequencies and mode shapes, and compare them with those determined experimentally.