Conclusions about test in "Viaduct over Tajo River" of Madrid-Seville high speed railway line. Considerations about design of railway bridges in high speed lines

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Conclusions about test in "Viaduct over Tajo River" of Madrid-Seville high speed railway line. Considerations about design of railway bridges in high speed lines

Author(s): Alvarez Cabal, R.; Díaz Lozano, J.; Moreno Blanes, C.; Santos Mesa, J.; Santos Olalla, F.

Publication: ACHE

Volume: 50

Issue: 214

Appears on pages(s): 131 - 140

Keywords: Pruebas de carga, coeficiente de impacto, efectos dinámicos, alta velocidad, puentes de ferrocarril.

DOI:

Date: 1/3/1999

Abstract:
A dynamic tests campaign has been carried out in the ?Viaducto sobre el Río Tajo?, by the ?Subdireccion General de Construccion de Infraestructira Ferroviaria del Ministerio de Fomento?. These tests consist on the passage of commercial trains at high speed (between 200 km/h and 300 km/h). In these tests, dynamic ampliffication coefficient near to 200% have been registered. In this article the variation of impact coefficient with trains speeds and the possible causes of the amplitude reached are analyzed. Likewise a design criterion for railways bridges in High Speed Lines is included.