Time-dependent stress redistribution in composite structures: a general approach based on the aging coeficient

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-dependent stress redistribution in composite structures: a general approach based on the aging coeficient

Author(s): Pérez Caldentey, A.; Corres Peiretti, H.

Publication: ACHE

Volume: 45

Issue: 192

Appears on pages(s): Sep-36

Keywords:

DOI:

Date: 1/5/1994

Abstract:
A general simplified procedure using an age adjusted effective modulus for the analysis of the time-dependent behaviour of the composite structures is presented. This simplified procedure is tested against a computer model using a step by step procedure for three different examples, including two real bridge projects. In all cases very close agreement is obtained between both computations.