Strength analysis of masonry constructions. Application ta arch bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength analysis of masonry constructions. Application ta arch bridges

Author(s): Molins i Borrell, C.; Roca Fabregat, P.

Publication: ACHE

Volume: 49

Issue: 209

Appears on pages(s): Sep-32

Keywords:

DOI:

Date: 1/5/1998

Abstract:
A numerical model for the study of spatial structures consisting of linear curved members with variable cross sections is presented together with its application to the nonlinear geometric and material analysis of skeletal masonry constructions. Nonlinear material behaviour is included in the model by means of elastoplastic constitutive equations under shear and compressive stresses, while a linear-elastic prefectlybrittle behaviour is assumed in tension. Nonlinear geometric effects due to the imposition of the equilibrium condition upon the deformed configuration of the structure are considered. Two examples are presented. The first example deals with the analysis of a masonry arch up to failure including nonlinear material and geometric effects. The second example treats the application of the developed model to a four span medieval bridge.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »