Fibre reinforced self-compacting concrete for precast

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fibre reinforced self-compacting concrete for precast

Author(s): Gemma Rodríguez de Sensale, Luis Segura-Castillo, Iliana Rodríguez Viacava, Rosana Rolfi Netto, Darío Miguez Passada, María Esther Fernández Iglesias

Publication: ACHE

Volume: 69

Issue: 284

Appears on pages(s): 69 - 75

Keywords: Self-compacting concrete, Structural fibres

DOI:

Date: 1/1/2018

Abstract:
A self-compacting concrete (SCC), which is usual in local precast, was used as reference. The variables analysed were the type of fibres and their amount. Properties of concretes in fresh and hardened state were studied. The use of fibres, compared to the SCC without fibres, significantly influences the rheology in the fresh state and improves mechanical resistance in the hardened state. As regards the air permeability and the resistance to chloride penetration, the results obtained do not differ significantly between the two states.